公开(公告)号:US06284174B1
公开(公告)日:2001-09-04
申请号:US09424954
申请日:1999-12-06
申请人: Kunihiko Ueda , Toshio Nishitani , Hiroki Furuta , Teruaki Saijo , Kanji Saito , Hiroshi Kato , Hiroshi Ohtani , Shinji Shimizu , Koji Hashimoto
发明人: Kunihiko Ueda , Toshio Nishitani , Hiroki Furuta , Teruaki Saijo , Kanji Saito , Hiroshi Kato , Hiroshi Ohtani , Shinji Shimizu , Koji Hashimoto
IPC分类号: D01D110
摘要: A melt spinning pack, including a pack case, a spinneret having many spinning holes positioned at the bottom of the case, a pack cap having a polymer introducing hole at the center positioned at the top of the case, and a flow arranging plate having many flow arranging holes with restricted portions reduced in cross sectional area compared to the inlets of the holes positioned between the spinneret and the pack cap, satisfying the requirement that the contraction percentage R be 50% or less, respectively contained in the case.
摘要翻译: 一种熔融纺丝组件,包括一个包装盒,一个具有位于壳体底部的许多纺丝孔的喷丝头,一个在壳体顶部位于中心位置处具有聚合物引入孔的包装盖,以及具有许多 与位于喷丝头和包装盖之间的孔的入口相比,具有限制部分的横截面积减小的流动分配孔满足分别包含在壳体中的收缩百分比R为50%或更小的要求。
-
公开(公告)号:US06485662B1
公开(公告)日:2002-11-26
申请号:US08753931
申请日:1996-12-03
IPC分类号: D01D110
CPC分类号: B29C47/68 , B29C47/0021 , B29C47/0023 , C08L23/06 , C08L23/0815 , C08L2205/02 , C08L2666/04
摘要: A process comprising: (i) providing a first polyethylene, prepared independently, having a melt index in the range of about 5 to about 3000 grams per 10 minutes and a density in the range of about 0.900 to about 0.975 gram per cubic centimeter and a second polyethylene, prepared independently, having a flow index in the range of about 0.01 to about 30 grams per 10 minutes and a density in the range of about 0.860 to about 0.940 gram per cubic centimeter, the weight ratio of the first polyethylene to the second polyethylene being in the range of about 75:25 to about 25:75; (ii) blending the first polyethylene with the second polyethylene; (iii) melting the blend; and, prior to extrusion or pelletizing, (iv) passing the molten blend through one or more active screens, in the case of two or more active screens, positioned in series, each active screen having a micron retention size in the range of about 2 to about 70, at a mass flux of about 5 to about 100 pounds per hour per square inch.
摘要翻译: 一种方法,包括:(i)提供独立制备的具有约5至约3000克/ 10分钟范围内的熔体指数和约0.900至约0.975克/立方厘米范围内的密度的第一聚乙烯和 第二聚乙烯,其独立制备,流动指数在约0.01至约30克/ 10分钟的范围内,密度在约0.860至约0.940克/立方厘米的范围内,第一聚乙烯与第二聚乙烯的重量比 聚乙烯在约75:25至约25:75的范围内;(ii)将第一聚乙烯与第二聚乙烯混合;(iii)熔融共混物; 并且在挤出或造粒之前,(iv)使熔融共混物通过一个或多个活性筛网,在两个或更多个活性筛网的情况下,串联定位,每个活性筛网的微米保留尺寸在约2 至约70,以每平方英寸约5至约100磅的质量通量。
-
3.
公开(公告)号:US06171536B2
公开(公告)日:2001-01-09
申请号:US09058492
申请日:1998-04-10
IPC分类号: D01D110
CPC分类号: D01D1/106
摘要: A method and apparatus for melt spinning molten polymeric material into filaments, preferably embodied in the form of a spin pack assembly, utilizes an annular polymer filter formed of a screen mesh material to have a U-shaped axial cross-section defining an open end oriented to face upwardly for receiving polymer within the annular interior of the screen to flow outwardly therefrom to a downstream spinneret for extrusion. The filter eliminates any need to utilize sand or other filter material contained by the screen as a primary or auxiliary filtration medium and enables effective polymer flow substantially through the entire surface area of the screen without stagnation of material flow.
摘要翻译: 将熔融聚合物材料熔融纺丝成长丝的方法和装置,优选以纺丝组件的形式体现,利用由筛网材料形成的环形聚合物过滤器具有限定开口端定向的U形轴向横截面 面向上以在屏幕的环形内部中接收聚合物从其向外流动到用于挤出的下游喷丝头。 过滤器不需要使用筛网所含的砂或其他过滤材料作为主要或辅助过滤介质,并且使得有效聚合物基本上流过筛网的整个表面区域而不会停滞物料流。
-
4.
公开(公告)号:US06565786B2
公开(公告)日:2003-05-20
申请号:US09734046
申请日:2000-12-12
IPC分类号: D01D110
CPC分类号: B29D7/01 , B29K2105/0073 , B29K2105/0079
摘要: The present invention provides a method for producing a formed article from a dope comprising a polyphosphoric acid solvent and a polymer soluble in polyphosphoric acid, which includes using a production apparatus containing an apparatus for stirring and uniformly dispersing or homogenizing a dope and a pump apparatus for delivering the uniformly dispersed or homogeneous dope, wherein at least one of the apparatus and the pump apparatus has a part that comes into contact with the dope. According to the present invention, maintenance frequency of production facility due to the corrosion and elution of metal in a recovered solvent can be reduced, which in turn decreases the production cost.
摘要翻译: 本发明提供一种由包含多磷酸溶剂和可溶于多磷酸的聚合物的涂料制备成型制品的方法,该方法包括使用含有搅拌装置和均匀分散或均化涂料的制备装置和用于 输送均匀分散或均匀的涂料,其中装置和泵装置中的至少一个具有与涂料接触的部分。 根据本发明,可以减少由于回收溶剂中的金属的腐蚀和洗脱引起的生产设备的维护频率,这又降低了生产成本。
-
公开(公告)号:US06312634B1
公开(公告)日:2001-11-06
申请号:US09517600
申请日:2000-03-02
申请人: Eun Lai Cho , Duk Ho Oh , Hyek Se Lee
发明人: Eun Lai Cho , Duk Ho Oh , Hyek Se Lee
IPC分类号: D01D110
CPC分类号: D01F6/62
摘要: A method for preparing industrial polyester fibers involving melt-spinning polyester chips through a nozzle, oiling the resultant filaments with an aqueous emulsion oiling agent, and producing, from the filaments, multifilament yarn at a speed of 2000-3300 m/min.
摘要翻译: 一种制备工业聚酯纤维的方法,其包括通过喷嘴熔融纺丝聚酯切片,用水性乳液上油剂对所得长丝进行加油,并以长度为2000-3300米/分钟的长丝生产复丝纱线。
-
6.
公开(公告)号:US06830715B1
公开(公告)日:2004-12-14
申请号:US09913947
申请日:2001-08-20
申请人: Ulrich Reinehr , Tilo Sehm , Wolfgang Anderheggen , Toni Herbertz , Helmut Judat
发明人: Ulrich Reinehr , Tilo Sehm , Wolfgang Anderheggen , Toni Herbertz , Helmut Judat
IPC分类号: D01D110
CPC分类号: D01F13/04 , D01F6/70 , Y02P70/629
摘要: Method and device for producing elastane threads from spinning solutions using recycled elastane material.
摘要翻译: 使用再生弹性材料从纺丝溶液生产弹性纤维的方法和装置。
-
公开(公告)号:US06764623B2
公开(公告)日:2004-07-20
申请号:US09983261
申请日:2001-10-23
申请人: Sung Joong Kim , Gi Woong Kim , Seung Oh Lee
发明人: Sung Joong Kim , Gi Woong Kim , Seung Oh Lee
IPC分类号: D01D110
CPC分类号: B60C9/0042 , D02G3/02 , D02G3/48 , Y10T428/2913 , Y10T428/2933 , Y10T428/2969
摘要: Polyester multi-filamentary yarn, useful as tire reinforcement, is produced by melting polyester resin at 290° C. or below including at least 90 mol % of polyethylene terephthalate with intrinsic viscosity of 0.7-1.2; filtering the molten resin for filtering retention time of ten minutes or below; spinning the filtered, molten resin by extrusion through a nozzle which has 250-500 holes, each ranging in diameter from 0.5 mm to 1.2 mm with a length/diameter ratio from 2 to 5; primarily quenching the extruded yarn at a temperature of 100-195° C. in a zone of 50 mm or more distance directly below the nozzle; secondarily quenching the yarn with air at its glass transition temperature (Tg) or below; taking off the yarn at spinning stress of 0.3 g/d or greater; drawing taken-off yarn at total draw ratio of 1.3 or greater; and thermally treating the yarn at temperature 150-230° C.
摘要翻译: 可用作轮胎加固的聚酯多丝纱是通过在290℃或更低的聚酯树脂下熔化而制得的,包括至少90摩尔%的特性粘度为0.7-1.2的聚对苯二甲酸乙二醇酯; 过滤熔融树脂,过滤保留时间为十分钟以下; 通过具有250-500个孔的喷嘴通过挤出纺丝过滤的熔融树脂,每个孔的直径为0.5mm至1.2mm,长度/直径比为2至5; 主要在100-195℃的温度下在直接在喷嘴下方的50mm或更多的距离的区域中淬火挤出的纱线; 二次以玻璃化转变温度(Tg)以下的空气淬火纱线; 在纺丝应力为0.3g / d以上时脱纱; 拉丝纱线总拉伸比为1.3以上; 并在150-230℃温度下对纱线进行热处理
-
-
-
-
-
-