Abstract:
A propylene copolymer composition which comprises —a random copolymer of propylene (A), —a random copolymer of propylene (B), and —optional additive(s), suitable for pressure pipe applications.
Abstract:
The present invention is directed to a polypropylene composition (C) comprising a heterophasic propylene copolymer (RAHECO) and a plastomer (PL) as well as a process for the preparation of said polypropylene composition and a film obtained from said polypropylene composition (C).
Abstract:
Propylene homopolymer having a melt flow rate MFR2 (230° C.) at least 50 g/10 min, a Mw/Mn at least 12.0 and a xylene cold soluble content (XCS) of at least 2.8 wt.-%.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 0.5 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 30.0 to 40.0 wt-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the comonomer content of xylene cold soluble (XCS) fraction of the propylene copolymer is in the range of 16.0 to 28.0 wt.-%.
Abstract:
The present invention is directed to a layer of an electrical device a photovoltaic module comprising at least one photovoltaic element and at least one layer comprising a polypropylene composition and to the use of a polypropylene composition for producing at least one layer of an element of a photovoltaic module.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 1.0 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 16.0 to 28.0 wt.-% and an intrinsic viscosity (IV) in the range of more than 1.2 to below 2.5 dl/g.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 0.8 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 4.5 to 10.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 12.0 to 22.0 wt.-% and the xylene cold insoluble (XCI) fraction of the propylene copolymer has a Mw/Mn of more than 4.9 to 10.0.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 1.0 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 16.0 to 28.0 wt.-% and an intrinsic viscosity (IV) in the range of more than 1.2 to below 2.5 dl/g.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 0.8 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 4.5 to 10.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 12.0 to 22.0 wt.-% and the xylene cold insoluble (XCI) fraction of the propylene copolymer has a Mw/Mn of more than 4.9 to 10.0.
Abstract:
Polyolefin composition comprising a heterophasic propylene copolymer and glass material, wherein said heterophasic propylene copolymer has • a xylene cold soluble fraction in the range of 25 to 50 wt.-%, and • a comonomer content in the range of 10.0 to 15.0 wt.-%, wherein further the xylene cold soluble fraction of the heterophasic propylene copolymer has a comonomer content in the range of 20 to 30 wt.-% and the polyolefin composition has a melt flow rate MFR2 (230° C.) of 2.0 to 15.0 g/10 min.