Abstract:
Propylene-ethylene random copolymers with improved long-term mechanical properties, especially improved impact strength retention, their manufacture as well as their use, e.g. for the production of moulded articles, particularly injection moulded articles, such as thin-walled plastic containers for packaging.
Abstract:
Synergistic visbreaking composition of peroxide and a hydroxylamine ester for increasing the visbreaking efficiency for polypropylene polymers at melt extrusion temperatures below 250° C. and its use in visbreaking polypropylene. The present invention is furthermore related to the use of such visbroken polypropylene polymers for producing melt blown non-wovens with improved barrier properties.
Abstract:
Propylene copolymer having a comonomer content in the range of 2.0 to 11.0 mol.-% and a melt flow rate MFR2 (230° C.) in the range of 25.0 to 100 g/10 min, wherein said propylene copolymer is featured by good toughness.
Abstract:
The present invention is directed to a new polypropylene composition comprising a propylene homopolymer and a polymeric nucleating agent, to melt-blown fibers comprising the polypropylene composition, to a melt-blown web comprising the melt-blown fibers and/or the polypropylene composition, to an article comprising the melt-blown fibers and/or the melt-blown web as well as to the use of the polypropylene composition for improving the relation between pressure drop and hydrohead of a melt-blown web and for improving the thermo-mechanical properties of a melt-blown web in machine direction (MD) and transverse direction (TD).
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 1.0 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 16.0 to 28.0 wt.-% and an intrinsic viscosity (IV) in the range of more than 1.2 to below 2.5 dl/g.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 0.8 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 4.5 to 10.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 12.0 to 22.0 wt.-% and the xylene cold insoluble (XCI) fraction of the propylene copolymer has a Mw/Mn of more than 4.9 to 10.0.
Abstract:
Fiber reinforced composition comprising (a) a polypropylene random copolymer comprising ethylene and/or C4 to C8 α-olefin (PP-RACO), (b) fibers (F), and (c) a polar modified polypropylene as adhesion promoter (AP), wherein (i) the polypropylene random copolymer comprising ethylene and/or C4 to C8 α-olefin (PP-RACO) heaving a melt flow rate MFR2 (230° C.) measured according to ISO 1133 of at least 5 g/10 min, (ii) the fibers (F) are selected from the group consisting of glass fibers, metal fibers, ceramic fibers and graphite fibers, and (iii) the polymer contained in the reinforced composition forms a continuous phase being the matrix of the fiber reinforced composition.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 1.0 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 16.0 to 28.0 wt.-% and an intrinsic viscosity (IV) in the range of more than 1.2 to below 2.5 dl/g.
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 0.8 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 25.0 to 35.0 wt.-%, a comonomer content in the range of more than 4.5 to 10.0 wt.-%, wherein further the xylene cold soluble (XCS) fraction of the propylene copolymer has comonomer content in the range of 12.0 to 22.0 wt.-% and the xylene cold insoluble (XCI) fraction of the propylene copolymer has a Mw/Mn of more than 4.9 to 10.0.