摘要:
In a method of preparing a storage phosphor layer on a support by vapor deposition from a crucible unit by heating as phosphor precursor raw materials a matrix component and an activator component or a precursor component thereof, wherein said crucible unit comprises at least a bottom and surrounding side walls as a crucible for phosphor precursor raw materials present in said crucible in liquid form, wherein said crucible unit further comprises at least a chimney as part of the crucible unit and a slit allowing phosphor precursor raw materials to escape in vaporized form from said crucible unit in order to deposit it as a phosphor layer onto said support, the step of heating said precursor raw materials in the crucible in liquid form proceeds up to a temperature T1 and the step of heating said precursor raw materials in vaporized form in said chimney, proceeds up to a temperature T2, characterized in that a positive difference in temperature [T2−T1] is maintained.
摘要:
A photostimulable storage phosphor screen or panel suitable for use in mammographic applications comprises on a support, a storage phosphor layer and, adjacent thereto, an outermost top-coat layer, wherein said top-coat layer has a roughness profile such that an average spacing between peaks as measured by means of a stylus profiler over and along its scan-distance, is less than 250 μm.
摘要:
An image storage screen or panel, suitable for use in applications related with computed radiography comprises, on a support, a binderless needle-shaped stimulable CsBr:Eu phosphor layer, wherein, besides low amounts of a europium activator or dopant in favor of homogeneous distribution of said activator in the CsBr matrix, presence of well-defined amounts of rubidium halide and cesium chloride in said matrix, and, optionally, further presence of alkali metal, alkaline earth metal and/or metal earth salts, and/or, optionally, other metal salts or oxides, provides a remarkable speed increase, without loss in sharpness.
摘要:
Stimulable phosphor screens, sheets or panels having alkali metal halide storage phosphors have been disclosed, said phosphors showing emission of red light, after stimulation with an ultraviolet radiation source having a radiation emission maximum of 365 nm, wherein an intensity of red light is not higher than 10% of the blue light emission intensity, and wherein both emission intensities having been measured after stimulation of the said storage phosphors in the phosphor layer of the panel, having stored energy from radiation in the wavelength range shorter than 350 nm.
摘要:
A binderless storage phosphor screen comprises a vacuum deposited CsBr:Eu phosphor layer on a support, wherein the support includes a layer of amorphous carbon and optionally one or more auxilliary layers.
摘要:
An image storage screen or panel, suitable for use in applications related with computed radiography comprises, on a support, a binderless needle-shaped stimulable CsBr:Eu phosphor layer, wherein, besides low amounts of a europium activator or dopant in favor of homogeneous distribution of said activator in the CsBr matrix, presence of well-defined amounts of rubidium halide and cesium chloride in said matrix, and, optionally, further presence of alkali metal, alkaline earth metal and/or metal earth salts, and/or, optionally, other metal salts or oxides, provides a remarkable speed increase, without loss in sharpness.
摘要:
Needle-shaped CsBr:Eu2+ storage phosphor crystal particles in form of a cylinder suitable for use in flat storage phosphor panels have been provided, wherein said particles have an average cross-section in the range from 1 μm up to 30 μm and an average length, measured along the casing of said cylinder, in the range from 100 μm up to 1000 μm.
摘要:
A method for producing CsX:Eu stimulable phosphors and screens or panels provided with said phosphors as powder phosphors or vapor deposited needle-shaped phosphors suitable for use in image forming methods for recording and reproducing images of objects made by high energy radiation, wherein said CsX:Eu stimulable phosphors are essentially free from oxygen in their crystal structure, and wherein X represents a halide selected from the group consisting of Br, Cl and combinations thereof, and wherein the method further makes use of starting compounds (precursors) or combinations of precursors for the synthesis of said CsX:Eu stimulable phosphors, said precursors (starting compounds) having as a composition CsxEuyX′x+αy, wherein the ratio of x to y exceeds a value of 0.25, wherein α>2 and wherein X′ is a halide selected from the group consisting of Cl, Br and I and combinations thereof; heating said mixture at a temperature above 450° C.; cooling said mixture, and optionally annealing and recovering said CsX:Eu phosphor.
摘要翻译:一种生产CsX:Eu可激发的荧光体和屏幕或面板的方法,所述荧光体具有所述磷光体作为粉末磷光体或气相沉积的针状磷光体,适用于用于记录和再现由高能量辐射制成的物体的图像的图像形成方法,其中所述CsX :Eu可激发荧光体在其晶体结构中基本上不含氧,其中X表示选自Br,Cl及其组合的卤化物,并且其中该方法进一步利用起始化合物(前体)或前体的组合 为了合成所述CsX:Eu可激发的荧光体,所述前体(起始化合物)具有组成Cs x x Eu x Y x + alphay SUB 其中x与y的比值超过0.25,其中α> 2,其中X'是选自Cl,Br和I的卤化物及其组合; 在高于450℃的温度下加热所述混合物; 冷却所述混合物,并且任选地退火和回收所述CsX:Eu荧光体。
摘要:
Stimulable phosphor screens, sheets or panels having alkali metal halide storage phosphors have been disclosed, said phosphors showing emission of red light, after stimulation with an ultraviolet radiation source having a radiation emission maximum of 365 nm, wherein an intensity of red light is not higher than 10% of the blue light emission intensity, and wherein both emission intensities having been measured after stimulation of the said storage phosphors in the phosphor layer of the panel, having stored energy from radiation in the wavelength range shorter than 350 nm.
摘要:
A Eu-doped CsBr-type storage phosphor screen or panel has been disclosed, providing ratios of ultraviolet luminescence intensities of at least 10/9 after having been exposed to radiation having a wavelength in the range from 150 to 400 nm, measured at same sites without and with pretreatment exposure of said storage phosphor screen or panel with short ultraviolet radiation in the range from 150 to 300 nm and having an energy of 10 mJ/mm2, as well as a method of producing a stimulable phosphor screen or panel, characterized in that during or after at least one of the manufacturing steps a radiation exposure treatment is given with radiation sources emitting short ultraviolet radiation in the range from 150 to 300 nm with an energy of at least 10 mJ/mm2.
摘要翻译:已经公开了Eu掺杂的CsBr型存储荧光屏或面板,其在暴露于波长在150至400nm的辐射之后提供至少10/9的紫外发光强度的比率,在相同的位置 所述存储荧光屏或面板在150-300nm范围内具有短紫外线辐射并具有10mJ / mm 2的能量的预处理曝光以及产生可刺激荧光屏或面板的方法 其特征在于,在所述制造步骤中的至少一个之后或之后,以150-300纳米的能量至少为10mJ / mm 2的发射短的紫外线辐射的辐射源给予辐射曝光处理。