Abstract:
In a method of enhancing the dry grinding efficiency of petcoke including adding additives to the petcoke and dry grinding the petcoke together with the additives. The additives may include a combination of at least one organic additive and at least one inorganic additive.
Abstract:
In a device for the solar-thermal gasification of carbon-containing charging material, comprising a solar reactor (1) including at least one, preferably a plurality of, light-transmissive window(s) (2) for introducing concentrated solar radiation, and a gasification chamber (9) having a preferably rectangular bottom and receiving means for the charging material (21), the receiving means are comprised of at least one, preferably elongated drawer (7,8,20,21,22,23) that is movable relative to the gasification chamber.
Abstract:
In a process for the production of cement clinker, in which raw meal is preheated in a preheater (3) using the hot exhaust gases from a clinker kiln, and the preheated raw meal, which is optionally calcined in a calciner (4), is burned to clinker in the clinker kiln (2), wherein the preheater (3) comprises at least one string of a plurality of cyclone suspension-type heat exchangers (8, 9, 10), through which the kiln exhaust gas successively flows and in which the raw meal is preheated in stages, a partial stream of the kiln exhaust gas is diverted such that only a remaining residual stream of the kiln exhaust gas is utilized for preheating the raw meal.
Abstract:
A hydraulic binder containing 25 to 85 wt % of cement clinker, 0 to 7 wt % of CaSO4, a mineral additive(s), and 1 to 10 wt % of a dual setting control system that includes an activator and a retarder, in a weight ratio of activator to retarder, based on the dry substance selected to be greater than 85:15, in particular greater than 90:10, more particularly greater than 95:5, and, in particular, greater than 98:2.