Abstract:
Injection molded article for healthcare applications based on propylene homopolymer having a melt flow rate in the range of 40 to 120 g/10 min, a pentad isotacticity of more than 92.5%, and meso sequence length of 91.0 to 160.
Abstract:
A propylene copolymer composition which comprises —a random copolymer of propylene (A), —a random copolymer of propylene (B), and —optional additive(s), suitable for pressure pipe applications.
Abstract:
The invention relates to a polypropylene composition comprising a crystalline propylene random copolymer and an amorphous propylene copolymer having improved hot-tack force and adhesion properties, to a process for the manufacture thereof, to the use thereof in the manufacture of adhesives and hot tack films and to articles comprising the polypropylene composition, as well as to a process for producing such article.
Abstract:
Molded article comprising a propylene copolymer having a xylene cold soluble content (XCS) in the range of 35 to 60 wt.-% and a comonomer content in the range of 7.0 to 17.0 wt-%, wherein further the propylene copolymer fulfills inequation (I), wherein Co (total) is the comonomer content [wt.-%] of the propylene copolymer Co (XCS) is the comonomer content [wt.-%] of the xylene cold soluble fraction (XCS) of the propylene copolymer. Co ( total ) Co ( XCS ) ≥ 0.50 ( I )
Abstract:
Propylene homopolymer having a melt flow rate MFR2 (230° C.) at least 50 g/10 min, a Mw/Mn at least 12.0 and a xylene cold soluble content (XCS) of at least 2.8 wt.-%.
Abstract:
Process for the preparation of polypropylene in a polymerization process, said comprises a pre-polymerization reactor and at least one polymerization reactor, wherein said process leads to polypropylene with broad molecular weight distribution.
Abstract:
Propylene homopolymer having a melt flow rate MFR2 (230° C.) at least 50 g/10 min, a Mw/Mn at least 12.0 and a xylene cold soluble content (XCS) of at least 2.8 wt.-%.
Abstract:
Heterophasic polypropylene composition comprising a propylene homo- or random copolymer matrix phase (A), and an ethylene-propylene copolymer rubber phase (B) dispersed within the matrix phase, the heterophasic polypropylene composition including a fraction soluble in pxylene at 25° C. (XCS fraction) which is present in the resin in an amount of 4 to 14 wt.-%, and a fraction insoluble in p-xylene at 25° C. (XCU fraction) which is present in the resin in an amount of 86 to 96 wt.-%, wherein the heterophasic polypropylene composition has an MFR2, determined according to ISO 1133 at 230° C. and under a load of 2.16 kg, of 4.0 to 8.0 g/10 min; and wherein the heterophasic polypropylene composition has a flexural modulus higher than 1500 MPa measured on an injection moulded specimen with the dimension 80×10×4 mm3 according to ISO 178; and wherein the heterophasic polypropylene composition has a content of monomer units derived from ethylene of 2.0 to 7.0 wt.-%.