Abstract:
A rubber composition which can improve performance on icy and snowy road sufficiently and a tire using the same. The rubber composition comprises 2 to 30 parts by weight of staple fibers having an average fiber diameter of 10 to 100 μm and an average fiber length of 0.01 to 4 mm, and 1 to 10 parts by weight of particles having a Moh's hardness of at least 5 and an average particle size of at most 500 μm based on 100 parts by weight of a diene rubber. The tire of the present invention is prepared by using the rubber composition for tread. Examples of the particle are pumice, quarts, emery and the like.
Abstract:
The present invention provides a rubber composition for a tire, which improves in fuel economy, wet grip performance, and abrasion resistance; and a pneumatic tire using the same. The present invention relates to a rubber composition for a tire, including: a rubber component including a modified styrene butadiene rubber that contains a constitutional unit derived from a specific nitrogen-containing compound in a main chain; silica; and a specific silane coupling agent.
Abstract:
A rubber roller, for use in an image-forming apparatus, which is formed by molding a rubber composition into the shape of a roller. In the rubber roller, a complex elastic modulus E* of rubber and a surface roughness Rz of the rubber roller satisfy a relationship indicated by an equation (1) shown below; and a hardness change of the rubber is set to not more than five points when the rubber ages at 70° C. for eight days: 7×Ln E*−0.12×Rz+3.0≦10. Equation (1)
Abstract:
A rubber roller, for use in an image-forming apparatus, which is formed by molding a rubber composition into the shape of a roller. In the rubber roller, a complex elastic modulus E* of rubber and a surface roughness Rz of the rubber roller satisfy a relationship indicated by an equation (1) shown below; and a hardness change of the rubber is set to not more than five points when the rubber ages at 70° C. for eight days: 7×Ln E*−0.12×Rz+3.0≦10 . Equation (1)
Abstract:
An elastomer composition containing 2 to 150 parts by mass of a mixture of a thermoplastic elastomer and a thermoplastic resin, 50 to 250 parts by mass of a softener, and 0.2 to 3.0 parts by mass of an organic peroxide serving as a crosslinking agent, and 2 to 20 parts by mass of a resin crosslinking agent with respect to 100 parts by mass of a rubber component containing diene rubber and/or ethylene-propylene-diene rubber. The rubber component is dynamically crosslinked to disperse the rubber component in the mixture of the thermoplastic elastomer and the thermoplastic resin.