摘要:
A process for metallizing substrates by activation of the substrate by deposition of palladium from a palladium complex, followed by electroless metallization. The palladium is deposited on the substrate by dipping the substrate into a solution of a palladium(O) complex and decomposing this complex at from 100.degree. to 300.degree. C.With this method it is possible to effectively activate substrates which are attacked by acid or alkali or swollen by organic solvents.
摘要:
A process for the manufacture of wear-resistant magnetic recording media comprising a dimensionally stable base, a thin ferromagnetic metal layer, containing cobalt and/or nickel, firmly bonded thereto and a thin protective layer applied thereon. The protective layer is produced by treating the recording medium in a liquid basic medium, containing gaseous oxygen, for from 1 to 60 minutes at from 5.degree. to 70.degree. C., washing and drying the treated recording medium and then heating it in air at from 170.degree. to 300.degree. C. This method offers a particularly simple way of providing the ferromagnetic layer of the recording medium with a thin but uniform, mechanically stable and wear-resistant protective layer.
摘要:
A process for the manufacture of rigid magnetic recording media by depositing a cobalt-containing ferromagnetic metal layer on a non-magnetic metallic base disc provided with a cured layer of binder which does not dissolve or swell in organic solvents and contains non-magnetic pigments, and which has been activated, before deposition of the ferromagnetic layer, by treatment with a solution of a palladium (O) complex in an organic solvent, followed by decomposition of this complex, to prepare it to receive the ferromagnetic metal layer which is produced by electroless deposition.
摘要:
Acicular ferrimagnetic iron oxides are prepared by a process in which iron (III) oxide hydroxide consisting essentially of lepidocrocite is reduced at from 350.degree. to 600.degree. C. by means of an organic compound which is a synthetic polymer with a molecular weight of from 3,000 to 40,000 to give magnetite, which, if desired, is subsequently partially or completely oxidized with an oxygen-containing gas at from 200.degree. to 450.degree. C.
摘要:
Disk-shaped nickel-plated aluminum substrates which are used as bases in the production of magnetic recording disks having a magnetizable metallic layer are surface treated by polishing and texturing.