Thermoplastic polyolefin containing amorphous ethylene elastomer

    公开(公告)号:US10647841B2

    公开(公告)日:2020-05-12

    申请号:US15504233

    申请日:2015-08-21

    Abstract: Disclosed is a thermoplastic polyolefin composition useful in automotive components comprising at least a polypropylene having a melting point temperature (Tm) of greater than 130° C. and a melt flow rate (230° C./2.16 kg) within the range from 10 g/10 min to 80 g/10 min; an amorphous ethylene-propylene copolymer comprising within the range from 40 wt % to 80 wt % ethylene derived units and having a melt flow rate (230° C./2.16 kg) within the range from 0.1 g/10 min to 20 g/10 min; and a propylene-based elastomer having within the range from 5 to 25 wt % ethylene derived units and having a Tm of less than 110° C. The composition only partially breaks or there is no break at −29° C. (ASTM D256) with Notched Izod Force of between 10 to 40 ft-lb/in2 at 22° C. (533 to 2,132 J/m2), and between 1.0 to 12 ft-lb/in2 at −29° C. (53 to 636 J/m2).

    Thermoplastic Polyolefin Compositions with Ethylene-Propylene Copolymers

    公开(公告)号:US20180186982A1

    公开(公告)日:2018-07-05

    申请号:US15724401

    申请日:2017-10-04

    Abstract: This invention relates to a thermoplastic polyolefin composition with (a) 45 wt % to 70 wt % of a polypropylene having 70 wt % or more units derived from propylene, having a melting point temperature of greater than 130° C. and a melt flow rate from 2 to 80 g/10 min; (b) 20 wt % to 30 wt % of a bimodal ethylene-propylene copolymer comprising: (i) 80 wt % to 90 wt % of an amorphous ethylene-propylene copolymer having about 30 wt % or more units derived from ethylene; (ii) 5 wt % to 15 wt % of a semi-crystalline ethylene-propylene copolymer having 70 wt % or more units derived from ethylene; and (iii) 1 wt % to 5 wt % of a propylene-based elastomer having within the range from 5 wt % to 25 wt % ethylene derived units and having a melting point temperature of less than 110° C. and a Mw/Mn within the range from 2.0 to 4.0.

    Propylene-Based Polymer Compositions for Grip Applications

    公开(公告)号:US20180030257A1

    公开(公告)日:2018-02-01

    申请号:US15551819

    申请日:2015-03-27

    Inventor: Jie Hui Xu Xin Chen

    Abstract: The present invention is related to a grip composition comprising 5 to 10 wt % of a polymer blend modifier, having a weight average molecular weight of 10,000 to 100,000 g/mole, 65 to 75 wt % of a propylene-based elastomer, having a weight average molecular weight of 100,000 to 300,000 g/mole, and a mineral powder. The polymer blend modifier comprises a first propylene-based polymer and a second propylene-based polymer, where the first and second propylene-based polymers are different and are individually selected from a homopolymer of propylene or a copolymer of propylene and ethylene or a C4 to C10 alpha-olefin. The composition further comprises 5 to 10 wt % of a propylene polymer, which is a homopolymer of propylene or a copolymer of propylene units with from 0.5 to 4 wt % ethylene or C4 to C10 alpha-olefin comonomer derived units.

    Thermoplastic Polyolefin Containing Amorphous Ethylene Elastomer

    公开(公告)号:US20200239677A1

    公开(公告)日:2020-07-30

    申请号:US16793075

    申请日:2020-02-18

    Abstract: Disclosed is a thermoplastic polyolefin composition useful in automotive components comprising at least a polypropylene having a melting point temperature (Tm) of greater than 130° C. and a melt flow rate (230° C./2.16 kg) within the range from 10 g/10 min to 80 g/10 min; an amorphous ethylene-propylene copolymer comprising within the range from 40 wt % to 80 wt % ethylene derived units and having a melt flow rate (230° C./2.16 kg) within the range from 0.1 g/10 min to 20 g/10 min; and a propylene-based elastomer having within the range from 5 to 25 wt % ethylene derived units and having a Tm of less than 110° C. The composition only partially breaks or there is no break at −29° C. (ASTM D256) with Notched Izod Force of between 10 to 40 ft-lb/in2 at 22° C. (533 to 2,132 J/m2), and between 1.0 to 12 ft-lb/in2 at −29° C. (53 to 636 J/m2).

    Thermoplastic polyolefin containing amorphous ethylene elastomer

    公开(公告)号:US11104784B2

    公开(公告)日:2021-08-31

    申请号:US16793075

    申请日:2020-02-18

    Abstract: Disclosed is a thermoplastic polyolefin composition useful in automotive components comprising at least a polypropylene having a melting point temperature (Tm) of greater than 130° C. and a melt flow rate (230° C./2.16 kg) within the range from 10 g/10 min to 80 g/10 min; an amorphous ethylene-propylene copolymer comprising within the range from 40 wt % to 80 wt % ethylene derived units and having a melt flow rate (230° C./2.16 kg) within the range from 0.1 g/10 min to 20 g/10 min; and a propylene-based elastomer having within the range from 5 to 25 wt % ethylene derived units and having a Tm of less than 110° C. The composition only partially breaks or there is no break at −29° C. (ASTM D256) with Notched Izod Force of between 10 to 40 ft-lb/in2 at 22° C. (533 to 2,132 J/m2), and between 1.0 to 12 ft-lb/in2 at −29° C. (53 to 636 J/m2).