公开(公告)号:US11859032B2
公开(公告)日:2024-01-02
申请号:US17324326
申请日:2021-05-19
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Crisita Carmen H. Atienza , Rhutesh K. Shah , Ron Walker , John R. Hagadorn , Sudhin Datta
IPC: C08F210/16 , C08F210/02 , C08F210/06 , C08F236/04 , C08F236/20 , B01J31/18 , C08F4/64
CPC classification number: C08F210/16 , B01J31/183 , C08F4/64113 , C08F210/02 , C08F210/06 , C08F236/04 , C08F236/20 , B01J2231/12 , B01J2531/49 , C08F2800/20
Abstract: A process to produce a branched ethylene-α-olefin diene elastomer comprising combining a catalyst precursor and an activator with a feed comprising ethylene, C3 to C12 α-olefins, and a dual-polymerizable diene to obtain a branched ethylene-α-olefin diene elastomer; where the catalyst precursor is selected from pyridyldiamide and quinolinyldiamido transition metal complexes. The branched ethylene-α-olefin diene elastomer may comprise within a range from 40 to 80 wt % of ethylene-derived units by weight of the branched ethylene-α-olefin diene elastomer, and 0.1 to 2 wt % of singly-polymerizable diene derived units, 0.1 to 2 wt % of singly-polymerizable diene derived units, and the remainder comprising C3 to C12 α-olefin derived units, wherein the branched ethylene-α-olefin diene elastomer has a weight average molecular weight (Mw) within a range from 100 kg/mole to 300 kg/mole, an average branching index (g′avg) of 0.9 or more, and a branching index at very high Mw (g′1000) of less than 0.9.
-
公开(公告)号:US11174332B2
公开(公告)日:2021-11-16
申请号:US16356894
申请日:2019-03-18
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Sudhin Datta , Andy H. Tsou , Ron Walker , Krishnan Anantha Narayana Iyer , Hamidreza Khakdaman , Kimari T. M. Slaughter , Sebastian Vasquez , Antonios K. Doufas
IPC: C08F236/04 , C08F210/06 , C08F210/02 , C08L23/16 , C08L23/14 , C08J3/21 , C08J3/24 , C08F236/20 , C08F210/18
Abstract: This invention relates to a thermoplastic vulcanizate having excellent elongation comprising an isotactic polypropylene matrix phase in which a cross-linked ethylene-propylene-diene terpolymer (EPDM) is dispersed, the vulcanizate comprising the reaction product of: a) 35 to 55 wt % of an ethylene-propylene-diene terpolymer (EPDM); b) 10 to 40 wt % of isotactic polypropylene (iPP); c) 0.5 to 25 wt % of a propylene-ethylene-diene terpolymer (PEDM) compatibilizer, said compatibilizer having a heat of fusion of less than 2 J/g; and d) 0.015 to 0.03 wt % of curatives; wherein the percentages of components (a) to (d) are based on the total weight of the mixture.
-
公开(公告)号:US11041034B2
公开(公告)日:2021-06-22
申请号:US16250710
申请日:2019-01-17
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Crisita Carmen H. Atienza , Rhutesh K. Shah , Ron Walker , John R. Hagadorn , Sudhin Datta
IPC: C08F210/16 , C08F210/02 , C08F210/06 , C08F236/04 , C08F236/20 , C08F4/64 , B01J31/18
Abstract: A process to produce a branched ethylene-α-olefin diene elastomer comprising combining a catalyst precursor and an activator with a feed comprising ethylene, C3 to C12 α-olefins, and a dual-polymerizable diene to obtain a branched ethylene-α-olefin diene elastomer; where the catalyst precursor is selected from pyridyldiamide and quinolinyldiamido transition metal complexes. The branched ethylene-α-olefin diene elastomer may comprise within a range from 40 to 80 wt % of ethylene-derived units by weight of the branched ethylene-α-olefin diene elastomer, and 0.1 to 2 wt % of singly-polymerizable diene derived units, 0.1 to 2 wt % of singly-polymerizable diene derived units, and the remainder comprising C3 to C12 α-olefin derived units, wherein the branched ethylene-α-olefin diene elastomer has a weight average molecular weight (Mw) within a range from 100 kg/mole to 300 kg/mole, an average branching index (g′avg) of 0.9 or more, and a branching index at very high Mw (g′1000) of less than 0.9.
-
公开(公告)号:US10513601B2
公开(公告)日:2019-12-24
申请号:US15815815
申请日:2017-11-17
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Xin Chen , Sudhin Datta , Rohan A. Hule
Abstract: This invention relates to a polyolefin composition with (a) 80 to 90 wt % of an amorphous ethylene-propylene copolymer having either no crystallinity or crystallinity derived from ethylene, having about 30 wt % or more units derived from ethylene; (b) 5 to 15 wt % of a semi-crystalline ethylene-propylene copolymer having substantial crystallinity derived from ethylene and having 70 wt % or more units derived from ethylene; and (c) 1 to 5 wt % of a propylene-based elastomer having within the range from 5 to 25 wt % ethylene derived units and having a melting point temperature of less than 110° C. and a Mw/Mn within the range from 2.0 to 4.0.
-
公开(公告)号:US10364308B2
公开(公告)日:2019-07-30
申请号:US15786051
申请日:2017-10-17
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Xin Chen , Sudhin Datta
IPC: C08F210/06 , C08F210/02 , B32B27/32
Abstract: This invention relates to a thermoplastic polyolefin composition with (a) a polypropylene having a melting point of greater than 130° C. and a melt flow rate from 10 to 80 g/10 min; (b) an ethylene-propylene copolymer with 40 wt % to 80 wt % ethylene derived units and a Mooney Viscosity (1+4, 125° C.) of greater than 20 Mooney units, a Mw/Mn of from 1.8 to 4.0, and a weight average molecular weight of 50,000 to 300,000 g/mole; and (c) a propylene-based elastomer having 5 wt % to 25 wt % ethylene derived units and having a melting point of less than 110° C. and a Mw/Mn from 2.0 to 4.0; wherein the room temperature notch impact of the thermoplastic polyolefin composition is at least four times greater than the room temperature notch impact of a composition without the propylene-based elastomer.
-
公开(公告)号:US20180258203A1
公开(公告)日:2018-09-13
申请号:US15746965
申请日:2015-08-04
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Rohan A. Hule , Sudhin Datta , Yi Ping Ni
IPC: C08F110/06 , C08L23/12
CPC classification number: C08F110/06 , C08F2500/05 , C08F2500/12 , C08F2500/17 , C08L23/12 , C08L2203/30 , C08L2205/025 , C08L2205/035
Abstract: Bimodal polypropylene compositions and a process to form melt blended bimodal polypropylene compositions comprising combining at least two polypropylenes in at least a two-pass process, and forming a bimodal polypropylene composition having a Flexural Modulus (190° C., 1% secant) of at least 1700 MPa, as well as one or more other selected properties. These compositions are suitable for thermoformed articles and injection molded articles, any of which may be foamed.
-
公开(公告)号:US20170275443A1
公开(公告)日:2017-09-28
申请号:US15504233
申请日:2015-08-21
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Sudhin Datta , Xin Chen , Abdul M. Jangda , Rohan A. Hule , Jan Kalfus
IPC: C08L23/14
CPC classification number: C08L23/14 , C08L23/12 , C08L2205/02 , C08L2205/025 , C08L2205/03 , C08L2205/06 , C08L2207/04 , C08L2207/14 , C08L23/16 , C08L23/142
Abstract: Disclosed is a thermoplastic polyolefin composition useful in automotive components comprising at least a polypropylene having a melting point temperature (Tm) of greater than 130° C. and a melt flow rate (230° C./2.16 kg) within the range from 10 g/10 min to 80 g/10 min; an amorphous ethylene-propylene copolymer comprising within the range from 40 wt % to 80 wt % ethylene derived units and having a melt flow rate (230° C./2.16 kg) within the range from 0.1 g/10 min to 20 g/10 min; and a propylene-based elastomer having within the range from 5 to 25 wt % ethylene derived units and having a Tm of less than 110° C. The composition only partially breaks or there is no break at −29° C. (ASTM D256) with Notched Izod Force of between 10 to 40 ft-lb/in2 at 22° C. (533 to 2,132 J/m2), and between 1.0 to 12 ft-lb/in2 at −29° C. (53 to 636 J/m2).
-
公开(公告)号:US09771444B2
公开(公告)日:2017-09-26
申请号:US15295154
申请日:2016-10-17
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Danny Van Hoyweghen , Cynthia A. Mitchell , Achiel J. M. Van Loon , Narayanaswami Dharmarajan , Sudhin Datta
IPC: C08F210/06 , C08F210/02 , C08J5/18 , C08F210/16 , C08F110/02 , C08F10/02 , B32B27/32 , C08F2/06
CPC classification number: C08F210/02 , B32B1/02 , B32B27/08 , B32B27/24 , B32B27/32 , B32B27/327 , B32B2250/242 , B32B2307/40 , B32B2307/558 , B32B2307/5825 , B32B2307/732 , B32B2323/04 , B32B2439/00 , B32B2553/00 , C08F2/06 , C08F4/65908 , C08F10/02 , C08F110/02 , C08F210/06 , C08F210/16 , C08F2500/26 , C08J5/18 , C08J2323/08 , C08F4/65927 , C08F2500/03 , C08F2500/12 , C08F2500/09
Abstract: Provided herein is a polymer comprising greater than or equal to about 70 wt % units derived from ethylene, less than or equal to about 30 wt % units derived from propylene, and less than about 5 wt % of units derived from C4-C20 alpha-olefins, and having the following properties: crystallinity derived from ethylene; a heat of fusion of about 20 to about 85 J/g; a polydispersity index (Mw/Mn) of less than about 2.5; a reactivity ratio of about 0.5 to about 1.5; a proportion of inversely inserted propylene units based on 2, 1 insertion of propylene monomer in all propylene insertions, as measured by 13C NMR of less than 0.5 wt %; and a branching index greater than about 0.5
-
公开(公告)号:US20170174799A1
公开(公告)日:2017-06-22
申请号:US15295154
申请日:2016-10-17
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Danny Van Hoyweghen , Cynthia A. Mitchell , Achiel J.M. Van Loon , Narayanaswami Dharmarajan , Sudhin Datta
IPC: C08F210/02 , C08J5/18
CPC classification number: C08F210/02 , B32B1/02 , B32B27/08 , B32B27/24 , B32B27/32 , B32B27/327 , B32B2250/242 , B32B2307/40 , B32B2307/558 , B32B2307/5825 , B32B2307/732 , B32B2323/04 , B32B2439/00 , B32B2553/00 , C08F2/06 , C08F4/65908 , C08F10/02 , C08F110/02 , C08F210/06 , C08F210/16 , C08F2500/26 , C08J5/18 , C08J2323/08 , C08F4/65927 , C08F2500/03 , C08F2500/12 , C08F2500/09
Abstract: Provided herein is a polymer comprising greater than or equal to about 70 wt % units derived from ethylene, less than or equal to about 30 wt % units derived from propylene, and less than about 5 wt % of units derived from C4-C20 alpha-olefins, and having the following properties: crystallinity derived from ethylene; a heat of fusion of about 20 to about 85 J/g; a polydispersity index (Mw/Mn) of less than about 2.5; a reactivity ratio of about 0.5 to about 1.5; a proportion of inversely inserted propylene units based on 2, 1 insertion of propylene monomer in all propylene insertions, as measured by 13C NMR of less than 0.5 wt %; and a branching index greater than about 0.5
-
公开(公告)号:US09303341B2
公开(公告)日:2016-04-05
申请号:US14484376
申请日:2014-09-12
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Sudhin Datta , Derek W. Thurman , Chia Y. Cheng , Kuangyao B. Peng
IPC: C08F10/06 , C08L23/14 , D01D5/08 , D01D10/02 , D04H3/009 , D01D5/098 , D04H3/007 , C08L23/10 , D01F6/46 , D04H1/4291 , C08F210/06
CPC classification number: D04H3/009 , C08F210/06 , C08L23/10 , C08L23/142 , C08L2314/06 , D01D5/0985 , D01F6/46 , D04H1/4291 , D04H3/007 , Y10T442/696 , C08L2666/06
Abstract: Disclosed herein is a nonwoven fabric comprising within the range of from 1 to 49 wt %, by weight of the fabric, of a reactor grade propylene-α-olefin copolymer possessing; within the range of from 5 to 35 wt %, by weight of the copolymer, of units derived from one or more of ethylene and/or C4 to C12 α-olefins; a melt flow rate (230° C./2.16 kg) within the range of from 600 to 7500 g/10 min; and a weight average molecular weight of less than 200,000; and a second polypropylene having a melting point, Tm, of greater than 110° C. and a melt flow rate (230° C./2.16 kg) within the range of from 20 to 7500 g/10 min; wherein the fabric has a Handle value of less than 60% (measuring the fabric of 35 g/m2 basis weight). The fabric can be used in structures comprising one or more layers of the fabric described herein, and can include any number of other fabric layers made from other materials.
Abstract translation: 本文公开了一种非织造织物,其包含在织物重量的1至49重量%的范围内,该反应器级丙烯-α-烯烃共聚物具有; 在5至35重量%的共聚物的范围内,衍生自一种或多种乙烯和/或C 4 -C 12α-烯烃的单元; 熔体流动速率(230℃/ 2.16kg)在600至7500g / 10min的范围内; 重均分子量小于20万; 和熔点Tm(Tm)大于110℃,熔体流动速率(230℃/ 2.16kg)在20至7500g / 10min范围内的第二聚丙烯; 其中织物具有小于60%的手柄值(测量织物为35g / m 2基重)。 织物可以用于包括本文所述的一层或多层织物的结构中,并且可以包括由其它材料制成的任何数量的其它织物层。
-
-
-
-
-
-
-
-
-