Surface Treatment Solution For Autodeposition Coating of Metallic Material and Autodeposition Coating Treatment Method
    11.
    发明申请
    Surface Treatment Solution For Autodeposition Coating of Metallic Material and Autodeposition Coating Treatment Method 失效
    表面处理溶液用于金属材料自动沉积涂层和自动沉积涂层处理方法

    公开(公告)号:US20110135913A1

    公开(公告)日:2011-06-09

    申请号:US12957750

    申请日:2010-12-01

    摘要: A surface treatment solution for autodeposition coating treatment of a metallic material, which is an aqueous solution comprising at least one tannin, at least one crosslinking agent having a crosslinking group capable of thermosetting reaction with a phenolic hydroxyl group and/or a phenolic nucleus, ferric ions, soluble type elemental fluorine, and an oxidizing agent, wherein the solids mass concentration ratio of the tannin to the crosslinking agent is in the range of from 1:1 to 1:10, the molar concentration of the soluble type elemental fluorine is at least 3-fold the molar concentration of the ferric ions, and the pH of the solution is from 2 to 6. The surface treatment solution allows shorter process length as compared with conventional coating processes, generates less environmentally harmful by-products such as sludge, has excellent throwing power at the interior of a pocket structure, does not use environmentally harmful components such as chromium compounds, has corrosion resistance, and allows overcoating of a baking finish on the obtained coating film.

    摘要翻译: 一种用于自动沉积涂覆处理金属材料的表面处理溶液,其是包含至少一种单宁的水溶液,至少一种具有能够与酚羟基和/或酚核心进行热固化反应的交联基团的交联剂,三价铁 离子,可溶型元素氟和氧化剂,其中单宁与交联剂的固体质量浓度比在1:1至1:10的范围内,可溶型元素氟的摩尔浓度为 三价铁离子的摩尔浓度至少为3倍,溶液的pH为2〜6。表面处理溶液与常规涂布方法相比,加工时间缩短,生成较少的环境有害副产物如污泥, 在口袋结构的内部具有优异的抛光力,不使用环境有害的成分,如铬化合物,具有腐蚀性 并且允许在所获得的涂膜上涂覆烤漆。

    Metal phthalocyanine dye mixture, curable composition, color filter, and method for producing color filter
    12.
    发明授权
    Metal phthalocyanine dye mixture, curable composition, color filter, and method for producing color filter 有权
    金属酞菁染料混合物,可固化组合物,滤色器和滤色器的制造方法

    公开(公告)号:US08445167B2

    公开(公告)日:2013-05-21

    申请号:US12934462

    申请日:2009-03-16

    IPC分类号: G02B5/20

    摘要: The invention aims to provide a metal phthalocyanine dye mixture having excellent solubility in an organic solvent, which can be formed into a thin film. Provided are a metal phthalocyanine dye mixture contains at least phthalonitrile, a compound represented by the following formula (I), a compound represented by the following formula (II), and a metal or a metal compound, and a curable composition containing the metal phthalocyanine dye mixture, a color filter containing the curable composition, and a method for producing the color filter: wherein, in formulae (I) and (II), R1 represents a substituent; n represents an integer of from 0 to 3; X represents —S—, —SO2—, or —SO2N(R4)—; R4 represents a hydrogen atom, an alkyl group, an alkenyl group, an aryl group, or a heterocyclic ring group; R2 represents an alkyl group, an alkenyl group, an aryl group, or a heterocyclic ring group; R3 represents a substituent; m represents an integer of from 0 to 3; and Z represents —SO3M or —(X1-A) group; wherein X1 has the same definition as X; A represents an optionally substituted group having at least one selected from —COOM, —SO3M, —SO2NH—R5, —SO2NHCOR6, —CONHSO2—R7, and —SO2NHSO2—R8; M represents a hydrogen atom, or an alkali metal or organic base group for neutralization of charges; and R5, R6, R7, and R8 each independently represents an alkyl group, an alkenyl group, an aryl group, or a heterocyclic ring group.

    摘要翻译: 本发明的目的在于提供一种在可形成薄膜的有机溶剂中具有优异的溶解性的金属酞菁染料混合物。 提供一种金属酞菁染料混合物,至少含有邻苯二甲腈,由下式(I)表示的化合物,下式(II)表示的化合物和金属或金属化合物,以及含有金属酞菁的固化性组合物 染料混合物,含有可固化组合物的滤色器和滤色器的制造方法,其中,在式(I)和(II)中,R 1表示取代基; n表示0〜3的整数, X表示-S - , - SO 2 - 或-SO 2 N(R 4) - ; R4表示氢原子,烷基,烯基,芳基或杂环基; R2表示烷基,烯基,芳基或杂环基; R3表示取代基; m表示0〜3的整数, Z表示-SO 3 M或 - (X 1 -A)基; 其中X1具有与X相同的定义; A表示具有选自-COOM,-SO3M,-SO2NH-R5,-SO2NHCOR6,-CONHSO2-R7和-SO2NHSO2-R8中至少一个的任选取代的基团; M表示氢原子,或用于中和电荷的碱金属或有机碱基; R 5,R 6,R 7和R 8各自独立地表示烷基,烯基,芳基或杂环基。

    Colored curable composition, color filter and production method thereof
    16.
    发明授权
    Colored curable composition, color filter and production method thereof 有权
    着色固化性组合物,滤色器及其制造方法

    公开(公告)号:US08029951B2

    公开(公告)日:2011-10-04

    申请号:US11845148

    申请日:2007-08-27

    IPC分类号: G02B5/20 G03F7/00

    摘要: Provided is a colored curable composition, comprising at least one tetraazaporphyrin dye represented by the following Formula (C1), a color filter prepared by using the same, and a production method thereof. wherein, R1 represents a substituent group; L represents an aliphatic or aromatic connecting group; Z1 represents a non-metal atom group needed for forming a six-membered ring with carbon atoms; at least one of the multiple groups R1 has —OY, —COOY, —SO3Y, —CON(Y)CO—, —CON(Y)SO2— or —SO2N(Y)CO—; Y represents a hydrogen atom, a metal atom or a conjugate acid; and M represents two hydrogen atoms, a bivalent metal atom, a bivalent metal oxide, a bivalent metal hydroxide or a bivalent metal chloride.

    摘要翻译: 提供一种着色固化性组合物,其包含至少一种由下式(C1)表示的四氮杂卟啉染料,使用其制备的滤色剂及其制备方法。 其中,R1表示取代基; L表示脂族或芳族连接基团; Z1表示形成具有碳原子的六元环所需的非金属原子团; 多个基团R 1中的至少一个具有-OY,-COOY,-SO 3 Y,-CON(Y)CO-,-CON(Y)SO 2 - 或-SO 2 N(Y)CO-; Y表示氢原子,金属原子或共轭酸; M表示2个氢原子,2价金属原子,2价金属氧化物,2价金属氢氧化物或2价金属氯化物。

    Solution for treating metal surface, surface treating method, and surface treated material
    18.
    发明授权
    Solution for treating metal surface, surface treating method, and surface treated material 有权
    处理金属表面,表面处理方法和表面处理材料的方法

    公开(公告)号:US07575644B2

    公开(公告)日:2009-08-18

    申请号:US11810949

    申请日:2007-06-07

    IPC分类号: C23F11/00 B05D1/00 B32B15/18

    摘要: A solution for treating a surface of an iron material includes (a) zirconium fluoride; (b) ion of a rare earth element and/or a compound containing a rare earth element; (c) a polyallylamine; (d) aluminum ion; and (e) free fluorine ion. Zirconium in the component (a) is at a weight concentration A of 10 to 1000 ppm. The ratio K of the weight concentration B of the rare earth element in the component (b) to the weight concentration A (B/A) is 0.1 to 30. The component (d) is at a weight concentration D of 50 to 250 ppm. The component (e) is at a weight concentration E of 0.5 to 30 ppm. A coating having excellent corrosion resistance before and after the subsequent coating can be deposited on the surface of an iron material by using the surface treating solution which does not contain environmentally harmful ingredients.

    摘要翻译: 用于处理铁材料表面的溶液包括(a)氟化锆; (b)稀土元素和/或含有稀土元素的化合物的离子; (c)聚烯丙胺; (d)铝离子; 和(e)游离氟离子。 组分(a)中的锆的重量浓度A为10〜1000ppm。 组分(b)中稀土元素的重量浓度B与重量浓度A(B / A)之比K为0.1至30.组份(d)的重量浓度D为50至250ppm 。 成分(e)的重量浓度E为0.5〜30ppm。 通过使用不含环境有害成分的表面处理溶液,可以在铁材料的表面上沉积在后续涂布之前和之后具有优异耐腐蚀性的涂层。

    Solution for treating metal surface, surface treating method, and surface treated material
    20.
    发明申请
    Solution for treating metal surface, surface treating method, and surface treated material 有权
    处理金属表面,表面处理方法和表面处理材料的方法

    公开(公告)号:US20080008902A1

    公开(公告)日:2008-01-10

    申请号:US11810949

    申请日:2007-06-07

    IPC分类号: C23F11/00 B05D1/00 B32B15/18

    摘要: A solution for treating a surface of an iron material includes (a) zirconium fluoride; (b) ion of a rare earth element and/or a compound containing a rare earth element; (c) a polyallylamine; (d) aluminum ion; and (e) free fluorine ion. Zirconium in the component (a) is at a weight concentration A of 10 to 1000 ppm. The ratio K of the weight concentration B of the rare earth element in the component (b) to the weight concentration A (B/A) is 0.1 to 30. The component (d) is at a weight concentration D of 50 to 250 ppm. The component (e) is at a weight concentration E of 0.5 to 30 ppm. A coating having excellent corrosion resistance before and after the subsequent coating can be deposited on the surface of an iron material by using the surface treating solution which does not contain environmentally harmful ingredients.

    摘要翻译: 用于处理铁材料表面的溶液包括(a)氟化锆; (b)稀土元素和/或含有稀土元素的化合物的离子; (c)聚烯丙胺; (d)铝离子; 和(e)游离氟离子。 组分(a)中的锆的重量浓度A为10〜1000ppm。 组分(b)中稀土元素的重量浓度B与重量浓度A(B / A)之比K为0.1至30.组份(d)的重量浓度D为50至250ppm 。 成分(e)的重量浓度E为0.5〜30ppm。 通过使用不含环境有害成分的表面处理溶液,可以在铁材料的表面上沉积在后续涂布之前和之后具有优异耐腐蚀性的涂层。