公开(公告)号:US20110005493A1
公开(公告)日:2011-01-13
申请号:US12736247
申请日:2010-03-05
CPC分类号: F02M55/025 , B23K20/227 , B23P19/042 , C21D1/09 , C21D9/08 , C21D9/14 , C21D10/005 , C21D2261/00 , C22C38/001 , C22C38/002 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/14 , F02M63/0225 , F02M2200/8084 , Y10T29/49229 , Y10T29/49231 , Y10T29/49728
摘要: The present invention provides a method of producing a common rail having a common rail body and a holder which include chemical components of 0.01-0.3 mass % of C, 0.01-0.5 mass % of Si, 0.01-3.0 mass % of Mn, 0.0003-0.01 mass % of B, 0.001-0.01 mass % of N, over 0.01-0.5 mass % of Al, 0.01-0.05 mass % of Ti, P limited to 0.03 mass % or less, S limited to 0.01 mass % or less, O limited to 0.01 mass % or less, a total content of As, Sn, Sb, Pb, and Zn limited to 0.015 mass % or less, the balance including Fe and inevitable impurities, in which the TLB value is 0.001% or more, the method including: inserting an insert metal; performing liquid phase diffusion bonding; performing laser-peening; and removing a surface layer.
摘要翻译: 本发明提供一种具有共轨体和保持器的共轨的制造方法,其包括C:0.01〜0.3质量%,Si:0.01-0.5质量%,Mn:0.01-3.0质量%,0.0003〜 B的0.01质量%,N的0.01〜0.01质量%,Al:0.01〜0.5质量%,Ti:0.01〜0.05质量%,P:0.03质量%以下,限制为0.01质量%以下的S 限于0.01质量%以下,将As,Sn,Sb,Pb,Zn的总含量限定为0.015质量%以下,余量包含Fe和不可避免的杂质,其中TLB值为0.001%以上, 方法包括:插入插入金属; 进行液相扩散接合; 进行激光喷丸处理; 并去除表面层。
-
公开(公告)号:US20100055490A1
公开(公告)日:2010-03-04
申请号:US12448581
申请日:2008-11-12
申请人: Atsushi Sugihashi , Koji Hirano , Yasushi Hasegawa
发明人: Atsushi Sugihashi , Koji Hirano , Yasushi Hasegawa
CPC分类号: F02M55/025 , C21D7/00 , C21D7/06 , C22C38/001 , C22C38/02 , C22C38/04 , C22C38/22 , C22C38/24 , C22C38/28 , C22C38/32 , F02M61/168 , F02M63/0225 , F02M2200/8069 , F02M2200/9061 , Y10T428/12361
摘要: This invention relates to a method producing a common rail excellent in fatigue strength from an inexpensive steel which uses as the material of the common rail a steel for high-strength liquid phase diffusion bonding having good toughness and fatigue strength, which steel contains, in mass %, C: 0.01 to 0.3%, Si: 0.01 to 0.5%, Mn: 0.01 to 3.0%, Cr: 1.0 to 12.0% and Mo: 0.1 to 2.0%, further contains, in mass %, V: 0.01 to 1.0%, B: 0.0003 to 0.01%, Ti: 0.01 to 0.05% and N: 0.001 to 0.01%, has P content limited to 0.03% or less, S content to 0.01% or less and O content to 0.01% or less, further has total content of grain boundary segregated embrittling elements As, Sn, Sb, Pb and Zn limited to 0.015% or less, and a balance of unavoidable impurities and Fe. The steel is used for liquid phase diffusion bonding. The production method uses a pulsed laser beam to perform laser-peening in the presence of a transparent liquid with respect to the vicinity of the boundary between the inner surface 21 of each branch hole 6 and the inner surface 22 of the rail hole 5, located at an opening peripheral zone of the branch hole 6. The surface layer of steel of the opening peripheral zone is thereafter removed.
摘要翻译: 本发明涉及一种制造廉价钢的共轨的方法,该廉价钢用作共轨材料,具有良好的韧性和疲劳强度的高强度液相扩散接合用钢,该钢含有质量 %,C:0.01〜0.3%,Si:0.01〜0.5%,Mn:0.01〜3.0%,Cr:1.0〜12.0%,Mo:0.1〜2.0%,V:0.01〜1.0% ,B:0.0003〜0.01%,Ti:0.01〜0.05%,N:0.001〜0.01%,P含量限制在0.03%以下,S含量为0.01%以下,O含量为0.01%以下,进一步具有 晶界分离脆化元素As,Sn,Sb,Pb和Zn的总含量限制在0.015%以下,余量为不可避免的杂质和Fe。 钢用于液相扩散接合。 该制造方法使用脉冲激光束,在透明液体的存在下,相对于分支孔6的内表面21与轨道孔5的内表面22之间的边界附近进行激光喷丸处理,位于 在分支孔6的开口周边区域。然后除去开口周边区域的钢的表面层。
-