公开(公告)号:US20170190989A1
公开(公告)日:2017-07-06
申请号:US15313608
申请日:2015-05-26
Applicant: SHELL OIL COMPANY
Inventor: Johannes Bernardus Wilhelmus MORSINK , Johannes TURFBOER , Rendert Jan WIERSMA , Ferry WINTER
CPC classification number: C10G45/58 , C10G2300/1022 , C10G2300/301 , C10G2300/302 , C10G2400/06 , C10L1/04
Abstract: The present invention provides a Fischer-Tropsch gasoil fraction having an initial boiling point of at least 175° C. and a final boiling point of at most 285° C. In another aspect the present invention provides a fuel composition and the use of a Fischer-Tropsch gasoil fraction according to the invention.
-
公开(公告)号:US20170190924A1
公开(公告)日:2017-07-06
申请号:US15313685
申请日:2015-05-26
Applicant: SHELL OIL COMPANY
Inventor: Johannes Bernardus Wilhelmus MORSINK , Johannes TURFBOER , Rendert Jan WIERSMA , Ferry WINTER
IPC: C09D7/00 , C10G47/00 , C09D11/033 , C10G2/00
CPC classification number: C09D7/20 , C09D5/00 , C09D11/033 , C10G2/332 , C10G47/00 , C10G2300/1022 , C10G2300/1055 , C10G2300/301 , C10G2300/302 , C10G2400/06
Abstract: The present invention provides a Fischer-Tropsch gasoil fraction having an initial boiling point of at least 210° C. and a final boiling point of at most 320° C. In another aspect the present invention provides a composition and the use of a Fisc-her-Tropsch gasoil fraction according to the invention.
-
13.
公开(公告)号:US20160045910A1
公开(公告)日:2016-02-18
申请号:US14779673
申请日:2014-03-28
Applicant: SHELL OIL COMPANY
Inventor: Ali AZGHAY , Patricia Johanna Anne Maria GILTAY , Marcello Stefano RIGUTTO , Arend Jan VAN WELSENES , Ferry WINTER
CPC classification number: B01J38/62 , B01J23/882 , B01J23/94 , B01J27/0515 , B01J37/20 , B01J38/12 , B01J38/48 , C10G45/08 , C10G65/00 , C10G2300/70
Abstract: The invention provides a process for rejuvenation of a used hydrotreating catalyst comprising at least 8% wt of coke and one or more non-noble Group VIII and/or Group VIb metals, which process comprises the steps of: (i) removing coke from the used hydrotreating catalyst; and (ii) treating the catalyst obtained in step (i) with of from 2 to 60% wt of gluconic acid, based on weight of dry catalyst.
Abstract translation: 本发明提供了一种使用的加氢处理催化剂的再生方法,其包含至少8重量%的焦炭和一种或多种非贵金属VIII族和/或VIb族金属,该方法包括以下步骤:(i) 使用加氢处理催化剂; 和(ii)以干燥催化剂的重量,用2-60重量%的葡萄糖酸处理步骤(ⅰ)中获得的催化剂。
-
-