摘要:
Disclosed is a phosphor having enhanced luminance. Specifically disclosed is a phosphor characterized by being substantially composed of an oxide containing Sr, Ca, Eu, Mg, Si and a halogen element(s) at a molar ratio of a:b:c:d:e:f (wherein a is not less than 0.5 but less than l, b is not less than 0 but less than 0.5, c is more than 0 but less than 0.3, d is not less than 0.8 but not more than 1.2, e is not less than 1.9 but not more than 2.1 and f is not less than 0.0008 but not more than 0.3), which oxide further contains oxygen.
摘要:
Disclosed are a positive electrode active material and a method for producing an olivine-type phosphate. The positive electrode active material comprises an olivine-type phosphate represented by the following formula (I), wherein the maximum peak in an X-ray diffraction pattern obtained using a CuKα ray is the peak of the (031) plane of the olivine-type phosphate and the half-value width of the peak is 1.5° or less: AaMbPO4 (I), wherein A represents one or more elements selected from among alkali metals; M represents one or more elements selected from among transition metals; a is from 0.5 to 1.5; and b is from 0.5 to 1.5. The method for producing an olivine-type phosphate comprises preparing a raw material comprising element A, element M, and phosphorus (P) so that a A:M:P molar ratio may be a:b:1, preliminary calcining the raw material, and mainly calcining the preliminary calcined raw material.
摘要:
Disclosed are a positive electrode active material and a method for producing an olivine-type phosphate. The positive electrode active material comprises an olivine-type phosphate represented by the following formula (I), wherein the maximum peak in an X-ray diffraction pattern obtained using a CuKα ray is the peak of the (031) plane of the olivine-type phosphate and the half-value width of the peak is 1.5° or less: AaMbPO4 (I), wherein A represents one or more elements selected from among alkali metals; M represents one or more elements selected from among transition metals; a is from 0.5 to 1.5; and b is from 0.5 to 1.5. The method for producing an olivine-type phosphate comprises preparing a raw material comprising element A, element M, and phosphorus (P) so that a A:M:P molar ratio may be a:b:1, preliminary calcining the raw material, and mainly calcining the preliminary calcined raw material.
摘要:
Disclosed is a mixed metal oxide which is reduced in the amount of scarce metal used therein, while having excellent performance as a positive electrode active material for secondary batteries. Also disclosed are a positive electrode for sodium secondary batteries having excellent performance, and a sodium secondary battery. Specifically disclosed is a method for producing a sodium-manganese complex metal oxide which is characterized by comprising a step for calcining a material, which contains sodium carbonate (Na2CO3) and dimanganese trioxide (Mn2O3) in such amounts that the molar ratio of sodium to manganese (Na/Mn) is not less than 0.4 but not more than 0.7, at a temperature of not less than 850° C. Also specifically disclosed are a sodium-manganese complex metal oxide produced by the method, a positive electrode for sodium secondary batteries which contains such a sodium-manganese complex metal oxide, and a sodium secondary battery.
摘要翻译:公开了一种混合金属氧化物,其中使用的稀有金属的量减少,同时具有作为二次电池的正极活性物质的优异的性能。 还公开了具有优异性能的钠二次电池用正极和钠二次电池。 具体公开了一种钠锰复合金属氧化物的制造方法,其特征在于,包括使含有碳酸钠(Na 2 CO 3)和三氧化二锰(Mn 2 O 3)的物质煅烧的工序,使得钠与锰的摩尔比 (Na / Mn)在不低于850℃的温度下不小于0.4但不大于0.7。还具体公开了通过该方法生产的钠锰复合金属氧化物,钠二次电池用正极 其含有这样的钠锰复合金属氧化物和钠二次电池。
摘要:
Disclosed is a mixed metal oxide which is extremely useful as a positive electrode active material for secondary batteries, while being reduced in the amount of a scarce metal used therein. Also disclosed are a positive electrode for sodium secondary batteries, and a sodium secondary battery. Specifically disclosed is a mixed metal oxide having an α-NaFeO2 type (layered rocksalt-type) crystal structure and represented by the following formula: NaxFe1-yMyO2 (wherein M represents one or more elements selected from the group consisting of group 4 elements, group 5 elements, group 6 elements and group 14 elements of the IUPAC periodic table and Mn; x represents a value more than 0.5 but less than 1; and y represents a value more than 0 but less than 0.5). Also specifically disclosed are a positive electrode for sodium secondary batteries, which contains the mixed metal oxide, and a sodium secondary battery.
摘要:
The present invention provides a phosphor and an electron beam excited light-emitting device. The phosphor comprises a compound represented by the formula (I) ; and at least one selected from the group consisting of Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb and Mn as an activator, M1O.mM2O.nM3O2 (I) wherein M1 is at least two selected from the group consisting of Ca, Sr and Ba, Sr alone or Ba alone, M2 is at least one selected from the group consisting of Mg and Zn, M3 is at least one selected from the group consisting of Si, Ge and Zr, 0.8≦m≦1.2, and 1.6≦n≦2.4. The electron beam excited light-emitting device comprises the above phosphor.
摘要:
The present invention provides a sodium secondary battery capable of reducing the amount of lithium used, and ensuring a larger discharge capacity maintenance rate when having repeated a charge and discharge, as compared with conventional techniques; and a mixed metal oxide usable as the positive electrode active material therefor. A mixed metal oxide of the present invention comprises Na and M1 wherein M1 represents three or more elements selected from the group consisting of Mn, Fe, Co and Ni with an Na:M1 molar ratio being a:1 wherein a is a value falling within the range of more than 0.5 and less than 1. Also, a mixed metal oxide of the present invention is represented by the following formula (1): NaaM1O2 (1) wherein M1 and a each have the same meaning as above. The positive electrode active material for secondary batteries of the present invention comprises the mixed metal oxide above.
摘要:
A sodium secondary battery capable of reducing the amount used of a scarce metal element such as lithium and cobalt and moreover, ensuring a larger discharge capacity after repeating charge/discharge as compared with conventional techniques, and a mixed metal oxide usable as the positive electrode active material therefor. The mixed metal oxide comprises Na, Mn and M1 wherein M1 is Fe or Ni, with a Na:Mn:M1 molar ratio being a:(1−b):b wherein a is a value falling within the range of more than 0.5 and less than 1, and b is a value falling within the range of from 0.001 to 0.5. Another mixed metal oxide is a mixed metal oxide represented by the following formula (1): NaaMn1−bM1bO2 (1) wherein M1, a and b each have the same meaning as above. The positive electrode active material for sodium secondary batteries comprises the mixed metal oxide above.
摘要:
The present invention provides a sodium secondary battery. The sodium secondary battery includes a positive electrode, a negative electrode, a separator disposed between the positive electrode and the negative electrode, and a nonaqueous electrolytic solution, the separator is composed of a porous laminate film in which a heat resistant porous layer and a porous film are stacked each other, and the heat resistant porous layer is disposed on the positive electrode side.
摘要:
The present invention provides a sodium secondary battery capable of reducing the amount of lithium used, and ensuring a larger discharge capacity maintenance rate when having repeated a charge and discharge, as compared with conventional techniques; and a mixed metal oxide usable as the positive electrode active material therefor. A mixed metal oxide of the present invention comprises Na and M1 wherein M1 represents three or more elements selected from the group consisting of Mn, Fe, Co and Ni with an Na:M1 molar ratio being a:1 wherein a is a value falling within the range of more than 0.5 and less than 1. Also, a mixed metal oxide of the present invention is represented by the following formula (1): NaaM1O2 (1) wherein M1 and a each have the same meaning as above.The positive electrode active material for secondary batteries of the present invention comprises the mixed metal oxide above.