Abstract:
New 6xxx aluminum alloy strips having an improved combination of properties are disclosed. The new 6xxx new aluminum alloy strips are rolled to a target thickness in-line via at least a first rolling stand and a second rolling stand. In one approach, the 6xxx new aluminum alloy strips may contain 0.8 to 1.25 wt. % Si, 0.2 to 0.6 wt. % Mg, 0.5 to 1.15 wt. % Cu, 0.01 to 0.2 wt. % manganese, 0.01 to 0.2 wt. % iron; up to 0.30 wt. % Ti; up to 0.25 wt. % Zn; up to 0.15 wt. % Cr; and up to 0.18 wt. % Zr.
Abstract:
A clip for assembling corners of hollow members such as the rails and stiles of an extruded aluminum door. The clip has a double L shape. A portion of the clip inserts into the hollow of a first member and is attached thereto. Another U-shaped portion defining the bottom of the double L extends into the other hollow member for attachment thereto to form a sturdy joint without welding. The first member may have a slot that receives the clip and the clip may be shaped to conform to the internal surfaces of one or both members. Clips may be used at each corner.
Abstract:
New 2xxx aluminum alloy bodies and methods of producing the same are disclosed. The new 2xxx aluminum alloy bodies may be produced by preparing the aluminum alloy body for post-solutionizing cold work, cold working by at least 25%, and then thermally treating. The new 2xxx aluminum alloy bodies may realize improved strength and other properties.
Abstract:
New heat treatable aluminum alloys having magnesium and zinc are disclosed. The new aluminum alloys generally contain 3.0-6.0 wt. % Mg, 2.5-5.0 wt. % Zn, where (wt. % Mg)/(wt. % Zn) is from 0.60 to 2.40.
Abstract:
A fastener including a pin member with an elongated shank having a first end, a second end opposite the first end, a cylindrical shank portion having an outer surface, a head located at the first end of the elongated shank, the head including a bearing surface located on the underside of the head, and a threaded portion located at the second end of the elongated shank. The fastener includes a washer installed on the pin member against the bearing surface of the head of the pin member. The washer includes an outer surface and at least one dielectric gasket layer located on the outer surface of the washer.
Abstract:
A locking member includes a body having a first end, a second end opposite the first end, a bore extending through the body from the first end to the second end, a bearing surface at the first end, fastening means for securing the locking member to a pin member, and a channel formed within the bearing surface and surrounding the bore. The locking member also includes a first insert located within the channel. The first insert is adapted such that, when the locking member is secured against a surface of a workpiece, the first insert prevents passage of a sparking material from within the bore of the locking member.
Abstract:
A fastener adapted to be installed in a hole of a composite structure includes a sleeve, a pin member, and a locking member. The sleeve has an outer surface having an outer diameter. The outer surface of the sleeve is textured. The outer diameter of the tubular portion is less than an inner diameter of the hole of the structure. The pin member has a shank portion. The sleeve is adapted to expand radially over the shank portion of the pin member to form an interference fit between the outer surface of the sleeve and the hole of the structure so as to provide an installed position of the fastener. When the fastener is in the installed position, the texture of the outer surface of the tubular portion deforms to engage with voids of the composite material present on the inner surface of the hole.
Abstract:
Methods for removing sulfur dioxide front a gas stream are disclosed. A method may include passing a gas stream comprising SO2 through a gas scrubbing apparatus. A scrubbing liquor comprising hydroxide ions and at least one oxidation catalyst may be flowed into the gas scrubbing apparatus, thereby contacting the gas stream with the scrubbing liquor. In response to the contacting, at least 90 wt. % of the sulfur dioxide may be removed from the gas stream. Concomitant to the contacting, at least some of the sulfur dioxide may react with at least some of the hydroxide ions, thereby forming sulfite ions in the scrubbing liquor. Some of the sulfite ions may be oxidized, via the oxidation catalyst, thereby forming sulfate ions in the scrubbing liquor. A used scrubbing liquor may be discharged from the scrubbing apparatus.
Abstract:
New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 330° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.
Abstract:
New 7xx aluminum casting alloys are disclosed. The aluminum casting alloys generally include from 3.0 to 8.0 wt. % Zn, from 1.0 to 3.0 wt. % Mg, where the wt. % Zn exceeds the wt. % Mg, from 0.35 to 1.0 wt. % Cu, where the wt. % Mg exceeds the wt. % Cu, from 0.05 to 0.30 wt. % V, from 0.01 to 1.0 wt. % of at least one secondary element (Mn, Cr, Zr, Ti, B, and combinations thereof), up to 0.50 wt. % Fe, and up to 0.25 wt. % Si, the balance being aluminum and other elements, wherein the aluminum casting alloy include not greater than 0.05 wt. % each of the other elements, and wherein the aluminum casting alloy includes not greater than 0.15 wt. % in total of the other elements.