LOW-TEMPERATURE FIRED, LEAD-FREE GLASS FRIT, PASTE, AND VACUUM GLASS ASSEMBLY USING SAME

    公开(公告)号:US20230101150A1

    公开(公告)日:2023-03-30

    申请号:US16970073

    申请日:2018-04-20

    Abstract: A glass frit according to this application may include a composition of P2O5, V2O5, TeO2, CuO, ZnO, and BaO configured to replace a conventional lead glass composition and enable a low temperature calcination. A coefficient of thermal expansion (CTE) of the glass frit may be matched with that of a glass substrate. The composition may not include an inorganic filler or at least reduce a content of an inorganic filler to reduce or prevent separation and breakage and to improve durability. The glass frit may be used as a paste for a vacuum glass assembly.

    SEALANT GLASS COMPOSITION AND SOLID OXIDE FUEL CELL USING SAME

    公开(公告)号:US20220024809A1

    公开(公告)日:2022-01-27

    申请号:US17296495

    申请日:2019-11-28

    Abstract: The present invention relates to a glass composition capable of being used as a sealant, and a solid oxide fuel cell using same. The sealant glass composition according to the present invention comprises 10-45 wt % of SiO2, 0.1-20 wt % of B2O3, 40-65 wt % of BaO, 0.1-20 wt % of CaO, and 0.1-15 wt % of at least one of Al2O3 and ZrO2, and unlike existing sealant glass compositions, can be suitably used in solid oxide fuel cells operating at intermediate temperatures, and exhibits an advantageous effect in keeping a decrease in sealing adhesion strength to a minimum, even after prolonged use.

    ENAMEL COMPOSITION, METHOD FOR PREPARING ENAMEL COMPOSITION, AND COOKING APPLIANCE

    公开(公告)号:US20200270171A1

    公开(公告)日:2020-08-27

    申请号:US16796102

    申请日:2020-02-20

    Abstract: An enamel composition, a method for preparing an enamel composition, and a cooking appliance are provided. The enamel composition may include phosphorus pentoxide (P2O5) at 15 to 50 wt %; silicon dioxide (SiO2) at 10 to 20 wt %; boron oxide (B2O3) at 1 to 15 wt %; one or more of lithium superoxide (Li2O), sodium oxide (Na2O), or potassium oxide (K2O) at 5 to 20 wt %; one or more of sodium fluoride (NaF), calcium fluoride (CaF2), or aluminum fluoride (AlF3) at 1 to 5 wt %; one or more of magnesium oxide (MgO), barium oxide (BaO), or calcium oxide (CaO) at 1 to 35 wt %; and one or more of titanium dioxide (TiO2), cerium dioxide (CeO2), molybdenum trioxide (MoO3), bismuth oxide (Bi2O3), or copper oxide (CuO) at 10 to 25 wt %, such that a heating time required for cleaning may be shortened and oil contaminants may be completely removed.