公开(公告)号:US5336523A
公开(公告)日:1994-08-09
申请号:US602288
申请日:1990-12-27
申请人: Garry D. Chater , George Wilson
发明人: Garry D. Chater , George Wilson
CPC分类号: G01M3/3236 , B05D7/227 , C23D5/02 , B05D1/002
摘要: A method of applying a liquid coating material to the inside of a tank(10) and performing a hydrostatic pressure test on the tank at the same time. The method is useable for applying a liquid vitreous enamel coating material to a water heater tank, to be subsequently dried and furnace heated to form a glazed enamel internal coating. Preferably the hydrostatic pressure test is performed by displacing coating material from a portion(68) of an accumulator(51) by pumping liquid into a flexible bladder(66) housed in the accumulator. Pressure from pump(76) is transmitted to the tank(10 by the liquid coating material and held for a prescribed time interval to prove tank integrity. The method avoids excessive shear, hence viscosity changes in thixotropic coating materials.
摘要翻译: PCT No.PCT / AU89 / 00226 Sec。 371日期1990年12月27日第 102(e)日期1990年12月27日PCT提交1989年5月23日PCT公布。 公开号WO89 / 11344 日期:1989年11月30日。一种将液体涂料施加到罐(10)的内部并同时对罐进行静水压力试验的方法。 该方法可用于将液体玻璃质搪瓷涂料施加到热水器箱中,随后将其干燥并加热炉以形成釉面釉质内涂层。 优选地,通过将液体泵送到容纳在蓄能器中的柔性囊(66)中,通过从蓄液器(51)的部分(68)移位涂覆材料来进行静水压力测试。 来自泵(76)的压力通过液体涂料传输到罐(10)并保持规定的时间间隔以证明油箱完整性,该方法避免了过度的剪切,因此触变涂层材料的粘度变化。