公开(公告)号:US20060141133A1
公开(公告)日:2006-06-29
申请号:US11298730
申请日:2005-12-09
申请人: Jean-Pierre Tahon , Paul Leblans , Luc Struye , Johan Lamotte
发明人: Jean-Pierre Tahon , Paul Leblans , Luc Struye , Johan Lamotte
CPC分类号: G03B42/02
摘要: A method of preparing a stimulable phosphor layer comprising a phosphor composed of a host or matrix compound and a dopant or activator compound or element wherein a precipitate or inclusion having a size in the range from 10−3 μm up to 10 μm is present in said matrix compound, proceeds by the steps of (1) providing one or more crucibles containing precursor compounds for said host, said dopant and said precipitate, by increasing the temperature of said crucible(s) up to a temperature provoking evaporation of all of said precursor compounds as a vaporized latent phosphor cloud, (2) depositing said vaporized latent phosphor cloud in form of a layer onto a temperature controlled substrate, (3) followed by cooling said substrate, and (4) further annealing said phosphor layer at a temperature in the range from 35° C. up to 200° C., wherein said method is characterized by performing said annealing in an atmosphere having a water content of more than 10 g per m3 of dry air at the temperature at which annealing proceeds. In a further embodiment the temperature of the said substrate as presented in the annealing atmosphere when starting annealing, is lower than the dew point of water in said atmosphere.
摘要翻译: 一种制备可刺激的磷光体层的方法,其包括由主体或基体化合物和掺杂剂或活化剂化合物或元素组成的磷光体,其中尺寸在10 -3以上的沉淀物或夹杂物 通过以下步骤(1)提供一种或多种含有前体化合物的坩埚,所述主体,所述掺杂剂和所述沉淀物的坩埚通过将所述坩埚的温度升高至温度 引起所有前体化合物的蒸发作为蒸发的潜在荧光云,(2)将所述蒸发的潜在荧光云以层的形式沉积到温度受控的基底上,(3)然后冷却所述基底,和(4)进一步退火 所述荧光体层在35℃至200℃的温度范围内,其中所述方法的特征在于在含水量大于10g / m 3的气氛中进行所述退火, SUP>的 在退火的温度下干燥空气。 在进一步的实施方案中,当起始退火时在退火气氛中呈现的所述基材的温度低于所述气氛中的水的露点。
-
公开(公告)号:US20060076538A1
公开(公告)日:2006-04-13
申请号:US11242295
申请日:2005-10-03
申请人: Johan Lamotte , Jean-Pierre Tahon , Paul Leblans
发明人: Johan Lamotte , Jean-Pierre Tahon , Paul Leblans
IPC分类号: C09K11/08
CPC分类号: G21K4/00 , C09K11/7733
摘要: An image storage screen or panel, suitable for use in applications related with computed radiography comprises, on a support, a binderless needle-shaped stimulable CsBr:Eu phosphor layer, wherein, besides low amounts of a europium activator or dopant in favor of homogeneous distribution of said activator in the CsBr matrix, presence of well-defined amounts of rubidium halide and cesium chloride in said matrix, and, optionally, further presence of alkali metal, alkaline earth metal and/or metal earth salts, and/or, optionally, other metal salts or oxides, provides a remarkable speed increase, without loss in sharpness.
摘要翻译: 适用于与计算机X线照相术有关的应用的图像存储屏幕或面板包括在支撑体上的无粘合剂针状可刺激CsBr:Eu荧光体层,其中除了少量的铕激活剂或掺杂剂之外,还有利于均匀分布 的CsBr基质中的所述活化剂,在所述基质中存在明确量的卤化铷和氯化铯,以及任选地进一步存在碱金属,碱土金属和/或金属土盐,和/或任选地, 其他金属盐或氧化物提供显着的速度增加,而没有锐度损失。
-
公开(公告)号:US09326741B2
公开(公告)日:2016-05-03
申请号:US14117333
申请日:2012-05-23
申请人: Paul Leblans , Jean-Pierre Tahon
发明人: Paul Leblans , Jean-Pierre Tahon
CPC分类号: A61B6/4216 , G21K4/00
摘要: The present invention concerns a method for the treatment of stimulable phosphors and/or screens for use in diagnosis, in particular medical radiography. The method comprises subjecting the stimulable phosphors and/or screens to an epoxide containing gaseous compound, promptly following their manufacture. By applying the method according to the invention yellowing of the stimulable phosphors and/or screens is prevented in a safe and efficient manner; thereby the disadvantages known as such resulting from such yellowing will not occur.
摘要翻译: 本发明涉及用于治疗用于诊断,特别是医学射线照相术的可刺激的荧光体和/或屏幕的方法。 该方法包括将可刺激的荧光体和/或筛网经过其制备后立即进行含环氧化物的气态化合物的处理。 通过应用根据本发明的方法,以安全和有效的方式防止可刺激的荧光体和/或筛网变黄; 从而不会发生由于这种变黄所导致的缺点。
-
公开(公告)号:US20080035857A1
公开(公告)日:2008-02-14
申请号:US11825499
申请日:2007-07-06
申请人: Luc Struye , Paul Leblans , Jean-Pierre Tahon
发明人: Luc Struye , Paul Leblans , Jean-Pierre Tahon
IPC分类号: G03C5/16
CPC分类号: G21K4/00 , C09K11/7733 , G21K2004/06
摘要: In a method of manufacturing a radiation image storage phosphor plate, comprising in its phosphor layer a storage phosphor of the type having an alkali metal halide salt as a main component and a lanthanide as a dopant, the plate after having been manufactured is uniformly exposed, i.e., exposed with a constant intensity and with a homogeneous energy distribution over its whole surface area, in order to absorb an X-ray dose in the range from 1 to 10 Gy.
摘要翻译: 在制造放射线图像存储磷光体板的方法中,在其荧光体层中包含具有碱金属卤化物盐作为主要成分和镧系元素作为掺杂剂的储存荧光体,制造后的板均匀地曝光, 即在其整个表面积上以恒定的强度和均匀的能量分布曝光,以便吸收1至10Gy范围内的X射线剂量。
-
公开(公告)号:US07297294B2
公开(公告)日:2007-11-20
申请号:US11601977
申请日:2006-11-20
申请人: Jean-Pierre Tahon , Johan Lamotte , Paul Leblans
发明人: Jean-Pierre Tahon , Johan Lamotte , Paul Leblans
CPC分类号: G21K4/00 , C09K11/7733 , G21K2004/06
摘要: A method for producing CsX:Eu stimulable phosphors and screens or panels provided with said phosphors as powder phosphors or vapor deposited needle-shaped phosphors suitable for use in image forming methods for recording and reproducing images of objects made by high energy radiation, wherein said CsX:Eu stimulable phosphors are essentially free from oxygen in their crystal structure, and wherein X represents a halide selected from the group consisting of Br, Cl and combinations thereof, and wherein the method further comprises the steps of mixing CsX with a compound or combinations of precursor compounds having as a composition CsxEuyX′x+αy, wherein the ratio of x to y exceeds a value of 0.25, wherein α≧2 and wherein X′ is a halide selected from the group consisting of Cl, Br and I and combinations thereof; heating said mixture at a temperature above 450° C.; cooling said mixture, and optionally annealing and recovering said CsX:Eu phosphor.
-
36.
公开(公告)号:US07288150B2
公开(公告)日:2007-10-30
申请号:US11015545
申请日:2004-12-17
申请人: Jean-Pierre Tahon , Johan Lamotte , Paul Leblans
发明人: Jean-Pierre Tahon , Johan Lamotte , Paul Leblans
CPC分类号: C09K11/7733 , G21K4/00
摘要: A method has been disclosed for manufacturing a storage phosphor for use in a photostimulable phosphor screen or panel comprising a support and a storage phosphor layer, wherein a dopant or activator is incorporated more homogeneously in amorphous and in crystalline phosphors as well, starting with a mixing step of said matrix component and activator component in stoechiometric ratios in order to provide a desired phosphor composition; and more particularly in order to prepare a CsBr:Eu2+ phosphor having an optimized sensitivity with respect to its particle size.
摘要翻译: 已经公开了用于制造用于可光激励荧光屏或面板的存储荧光体的方法,该荧光屏包括支撑体和存储磷光体层,其中掺杂剂或活化剂也更均匀地掺入无定形和结晶荧光体中,从混合开始 为了提供所需的荧光体组合物,所述基质组分和活化剂组分的组成比为步长; 并且更具体地是为了制备相对于其粒度具有优化的灵敏度的CsBr:Eu 2+ +磷光体。
-
公开(公告)号:US20070120093A1
公开(公告)日:2007-05-31
申请号:US11600494
申请日:2006-11-16
申请人: Jean-Pierre Tahon , Paul Leblans , Marcelle Escard
发明人: Jean-Pierre Tahon , Paul Leblans , Marcelle Escard
CPC分类号: G01T1/202 , C09K11/7733 , G21K4/00
摘要: In a method for producing precursor compounds suitable for use in the production of europium doped cesium halide photostimulable phosphors, at least one of the steps essentially makes use of an ammonium halide salt.
摘要翻译: 在制备适用于生产铕掺杂铯卤化物可光激发荧光体的前体化合物的方法中,至少一个步骤基本上是使用卤化铵盐。
-
公开(公告)号:US20070075293A1
公开(公告)日:2007-04-05
申请号:US11601977
申请日:2006-11-20
申请人: Jean-Pierre Tahon , Johan Lamotte , Paul Leblans
发明人: Jean-Pierre Tahon , Johan Lamotte , Paul Leblans
IPC分类号: C09K11/61
CPC分类号: G21K4/00 , C09K11/7733 , G21K2004/06
摘要: A method for producing CsX:Eu stimulable phosphors and screens or panels provided with said phosphors as powder phosphors or vapor deposited needle-shaped phosphors suitable for use in image forming methods for recording and reproducing images of objects made by high energy radiation, wherein said CsX:Eu stimulable phosphors are essentially free from oxygen in their crystal structure, and wherein X represents a halide selected from the group consisting of Br, Cl and combinations thereof, and wherein the method further comprises the steps of mixing CsX with a compound or combinations of precursor compounds having as a composition CsxEuyX′x+αy, wherein the ratio of x to y exceeds a value of 0.25, wherein α≧2 and wherein X′ is a halide selected from the group consisting of Cl, Br and I and combinations thereof; heating said mixture at a temperature above 450° C.; cooling said mixture, and optionally annealing and recovering said CsX:Eu phosphor.
摘要翻译: 一种生产CsX:Eu可激发的荧光体和屏幕或面板的方法,所述荧光体具有所述磷光体作为粉末磷光体或气相沉积的针状磷光体,适用于用于记录和再现由高能量辐射制成的物体的图像的图像形成方法,其中所述CsX :Eu可激发的荧光体在其晶体结构中基本上不含氧,并且其中X表示选自Br,Cl及其组合的卤化物,并且其中所述方法还包括以下步骤:将CsX与化合物或 作为组合物的前体化合物,其中x与y的比例超过0.25,其中x,y,x,y,x, 其中α> = 2,并且其中X'是选自Cl,Br和I的卤化物及其组合; 在高于450℃的温度下加热所述混合物; 冷却所述混合物,并且任选地退火和回收所述CsX:Eu荧光体。
-
39.
公开(公告)号:US07183560B2
公开(公告)日:2007-02-27
申请号:US11049445
申请日:2005-02-02
申请人: Jean-Pierre Tahon , Paul Leblans
发明人: Jean-Pierre Tahon , Paul Leblans
IPC分类号: G03B42/08
CPC分类号: G21K4/00 , C09K11/7733
摘要: Storage phosphor particles suitable for use in coated layers of stimulable phosphor screens or panels, in favor of high relative sensitivity, advantageously contain at the surface of the phosphor particles and in their inner volume, as components composing the said phosphor, a matrix component and a dopant or activator element that is homogeneously incorporated, wherein preference is given to particles having an aspect ratio of more than 2:1 and less than 50:1, said aspect ratio being defined as a ratio of 2 largest sizes of said particles, said sizes being taken in 3 dimensions perpendicular to each other, provided that one of said 2 largest sizes is smaller than 10 μm.
摘要翻译: 适合用于可刺激荧光屏或涂层的涂层的存储荧光体颗粒有利于高相对灵敏度,有利地在荧光体颗粒的表面和其内部体积中包含作为构成所述磷光体的组分,基质组分和 均匀掺入的掺杂剂或活化剂元素,其中优选具有大于2:1且小于50:1的纵横比的颗粒,所述纵横比定义为所述颗粒的2个最大尺寸的比例,所述尺寸 其中所述2个最大尺寸中的一个小于10um。
-
公开(公告)号:US20060163538A1
公开(公告)日:2006-07-27
申请号:US11298722
申请日:2005-12-09
申请人: Gabi Schierning , Miroslaw Batentschuk , Andres Osvet , Albrecht Winnacker , Luc Struye , Johan Lamotte , Jean-Pierre Tahon , Paul Leblans
发明人: Gabi Schierning , Miroslaw Batentschuk , Andres Osvet , Albrecht Winnacker , Luc Struye , Johan Lamotte , Jean-Pierre Tahon , Paul Leblans
IPC分类号: C09K11/08
CPC分类号: G21K4/00 , G21K2004/06
摘要: In a storage phosphor sheet, plate or panel, comprising a needle-shaped storage or photostimulable phosphor, said needle-shaped phosphor comprising a host or matrix compound and a dopant or activator compound or element in an amount of less than 0.01 mole % versus said host or matrix compound, said needle-shaped phosphor further comprises, as inclusions or precipitates, particles having a size in the range from 10−3 μm up to 10 μm, wherein said particles are present as ferroelectric particles, providing said panel with ferro-electric properties.
摘要翻译: 在包含针状储存或可光刺激的荧光体的存储荧光体片,板或面板中,所述针状荧光体包含主体或基质化合物,并且掺杂剂或活化剂化合物或元素的量小于0.01摩尔% 主体或基质化合物,所述针状荧光体还包含作为夹杂物或沉淀物的粒径在10 -3μm至10μm以下的颗粒,其中所述颗粒以铁电粒子形式存在 ,为所述面板提供铁电性能。
-
-
-
-
-
-
-
-
-