Methods of preparing positive electrode active material precursor for lithium secondary battery and positive electrode active material

    公开(公告)号:US10892471B2

    公开(公告)日:2021-01-12

    申请号:US16333378

    申请日:2018-02-06

    Applicant: LG Chem, Ltd.

    Abstract: A method of preparing a positive electrode active material precursor for a lithium secondary battery by using a batch-type reactor, which includes the steps of 1) forming positive electrode active material precursor particles while continuously adding a transition metal-containing solution including a transition metal cation, an aqueous alkaline solution, and an ammonium ion-containing solution to a batch-type reactor, 2) sedimenting the positive electrode active material precursor particles formed; 3) discharging a supernatant formed after the sedimentation of the positive electrode active material precursor particles to an outside; 4) adjusting a pH to 10 to 12 by adding the ammonium ion-containing solution; and 5) growing the positive electrode active material precursor particles while continuously again adding the transition metal-containing solution to the batch-type reactor, and a method of preparing a positive electrode active material using the same.

    Method for Preparing Positive Electrode Active Material

    公开(公告)号:US20200350554A1

    公开(公告)日:2020-11-05

    申请号:US16614233

    申请日:2018-11-23

    Applicant: LG Chem, Ltd.

    Abstract: A method for preparing a positive electrode active material includes: a step for adding a reaction mixture containing a lithium-raw material and a nickel-manganese-cobalt precursor into a first crucible and performing a first heat treatment at a temperature of 500-800° C. to form a pre-calcinated mixture; a step for extracting the pre-calcinated mixture from the first crucible and pulverizing or classifying the same; and a step for adding the pulverized or classified pre-calcinated mixture into a second crucible and performing a second heat treatment at a temperature of 700-1000° C. under an atmosphere in which an oxygen partial pressure is 20% or less to form a lithium nickel-manganese-cobalt-based positive electrode active material, wherein a volume of the pre-calcinated mixture formed after the first heat treatment is 20-50% with respect to a volume of the reaction mixture added into the first crucible.