公开(公告)号:US20140246128A1
公开(公告)日:2014-09-04
申请号:US14347277
申请日:2012-09-27
Applicant: JFE Steel Corporation
Inventor: Katsutoshi Takashima , Yuki Toji , Kohei Hasegawa
IPC: C22C38/26 , C22C38/16 , C22C38/14 , C22C38/08 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00 , C21D8/02 , C22C38/12
CPC classification number: C22C38/26 , B21B1/26 , B21B3/00 , B32B15/013 , C21D8/0226 , C21D8/0263 , C21D8/0426 , C21D8/0463 , C21D8/0473 , C21D9/46 , C21D9/48 , C21D2211/004 , C21D2211/005 , C21D2211/009 , C22C18/00 , C22C18/04 , C22C38/00 , C22C38/001 , C22C38/002 , C22C38/005 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/08 , C22C38/12 , C22C38/14 , C22C38/16 , C22C38/18 , C22C38/58 , C23C2/06
Abstract: Provided is a hot-rolled steel sheet that has a chemical composition including, by mass %: C: 0.060% to 0.150%; Si: 0.15% to 0.70%; Mn: 1.00% to 1.90%; P: 0.10% or less; S: 0.010% or less; Al: 0.01% to 0.10%; N: 0.010% or less; Nb: 0.010% to 0.100%; and the balance including Fe and incidental impurities. The hot-rolled steel sheet has a microstructure containing ferrite of 18 μm or less in average grain size by a volume fraction of at least 75% and pearlite of at least 2 μm in average grain size by a volume fraction of at least 5%, the balance being low-temperature-induced phases, the pearlite having a mean free path of at least 5.0 μm.
Abstract translation: 本发明提供一种热轧钢板,其特征在于,具有质量%:C:0.060〜0.150%的化学组成; Si:0.15〜0.70% Mn:1.00〜1.90% P:0.10%以下; S:0.010%以下; Al:0.01〜0.10% N:0.010%以下; Nb:0.010〜0.100% 余量包括铁和杂质。 该热轧钢板的平均粒径为18μm以下,铁素体的体积分数为75%以上,平均粒径为2μm以上的珠光体的体积分数为5%以上的微结构, 余量为低温诱导相,珠光体具有至少5.0μm的平均自由程。
-
42.
公开(公告)号:US20140234655A1
公开(公告)日:2014-08-21
申请号:US14346363
申请日:2012-09-27
Applicant: JFE Steel Corporation
Inventor: Katsutoshi Takashima , Yuki Toji , Nobusuke Kariya , Kohei Hasegawa
CPC classification number: C23C2/02 , B32B15/013 , C21D8/0226 , C21D8/0263 , C21D8/0426 , C21D8/0463 , C21D9/46 , C21D9/48 , C21D2211/005 , C22C18/04 , C22C38/001 , C22C38/002 , C22C38/005 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/08 , C22C38/12 , C22C38/14 , C22C38/16 , C22C38/26 , C23C2/06 , C23C2/28 , Y10T428/12799
Abstract: A high-strength hot-dip galvanized steel sheet has excellent workability, namely, excellent ductility and hole expansion formability, and high yield ratio. The steel sheet has a chemical composition containing by mass %: C: 0.05-0.15%; Si: 0.10-0.90%; Mn: 1.0-1.9%; P: 0.005-0.10%; S: 0.0050% or less; Al: 0.01-0.10%; N: 0.0050% or less; Nb: 0.010-0.100%; and the balance being Fe and incidental impurities, in which: the steel sheet has a complex phase that includes: ferrite having an average crystal grain size of 15 μm or less to at least 90% in volume fraction; martensite having an average crystal grain size of 3.0 μm or less to 0.5% or more and less than 5.0% in volume fraction; pearlite to 5.0% or less in volume fraction; and the balance being a phase generated at low temperature.
Abstract translation: 高强度热浸镀锌钢板具有优异的可加工性,即延展性和孔膨胀成形性优异,成品率高。 该钢板具有以质量%计含有的化学成分:C:0.05〜0.15% Si:0.10-0.90%; Mn:1.0-1.9% P:0.005-0.10%; S:0.0050%以下; Al:0.01-0.10%; N:0.0050%以下; Nb:0.010-0.100% 余量为Fe和偶然杂质,其中:钢板具有复相,其包含:平均晶粒尺寸为15μm以下的铁素体,体积分数为至少90%; 马氏体的平均结晶粒径为3.0μm以下,体积分率为0.5%以上且小于5.0% 珠光体至体积分数的5.0%以下; 余量为在低温下产生的相。
-