Display device
    81.
    发明申请
    Display device 有权
    显示设备

    公开(公告)号:US20070085778A1

    公开(公告)日:2007-04-19

    申请号:US11545536

    申请日:2006-10-11

    申请人: Yasunori Yoshida

    发明人: Yasunori Yoshida

    IPC分类号: G09G3/22

    摘要: To provide a highly reliable display device whose electrical element is applied with a low voltage. The display device is an active matrix FED display device whose pixel has an individual extraction gate electrode, an emitter array, a driving transistor which is connected to the emitter array in series, a potential control circuit which controls the potential of the extraction gate electrode, and a circuit which includes a switching element and a voltage holding element. By varying the potential of the extraction gate electrode in accordance with Vgs of the driving transistor, the active matrix driving method is performed by connecting a driving transistor to the emitter array in series and voltage which is applied to the driving transistor can be reduced.

    摘要翻译: 提供一种高可靠性的显示装置,其电元件被施加低电压。 显示装置是有源矩阵FED显示装置,其像素具有单独的提取栅电极,发射极阵列,串联连接到发射极阵列的驱动晶体管,控制提取栅电极的电位的电位控制电路, 以及包括开关元件和电压保持元件的电路。 通过根据驱动晶体管的Vgs改变提取栅电极的电位,通过将驱动晶体管串联连接到发射极阵列来执行有源矩阵驱动方法,并且可以减小施加到驱动晶体管的电压。

    Crystalline polyimide for melt molding with satisfactory thermal stability
    84.
    发明授权
    Crystalline polyimide for melt molding with satisfactory thermal stability 有权
    用于熔体模塑的结晶聚酰亚胺,具有令人满意的热稳定性

    公开(公告)号:US06458912B1

    公开(公告)日:2002-10-01

    申请号:US09674916

    申请日:2001-02-05

    IPC分类号: C08G7300

    摘要: A thermoplastic polyimide having good thermal stability, comprising a repeating unit represented by the chemical formula (1), a molecular terminal being composed of the chemical formula (2) and/or chemical formula (3), characterized in that: a melt viscosity ratio calculated by the numerical formula (1) and/or the numerical formula (3) is within a numerical range shown in the numerical formula (2) and/or the numerical formula (4) and 1,3-bis(4-aminophenoxy)benzene represented by the chemical formula (3) for production of the above polyimide, characterized in that the content of an azo compound is from 0.0 to 0.2%. The thermoplastic polyimide of the present invention has excellent characteristics {circle around (1)} to {circle around (4)} described below. {circle around (1)} It is superior in thermal stability on melting. That is, the degree of lowering of the fluidity on melting with a lapse of time is small and it is possible to apply to conventional melt molding. {circle around (2)} It has high heat resistance. {circle around (3)} It is superior in productivity. {circle around (4)} It is superior in dimensional accuracy.

    摘要翻译: 一种具有良好热稳定性的热塑性聚酰亚胺,其包含由化学式(1)表示的重复单元,由化学式(2)和/或化学式(3)组成的分子末端,其特征在于:熔体粘度比 由式(1)和/或数值式(3)计算的数值在数值式(2)和/或数值式(4)和1,3-双(4-氨基苯氧基) 由化学式(3)表示的用于制备上述聚酰亚胺的苯,其特征在于偶氮化合物的含量为0.0-0.2%。 本发明的热塑性聚酰亚胺具有以下所述的{圆周(1)}〜{圆周(4)}的特性。 {circle around(1)}熔融时的热稳定性优异。 也就是说,随着时间的流逝,熔融流动性的降低程度小,可以适用于常规的熔融成型。 {circle around(2)}它具有很高的耐热性。 {circle around(3)}它的生产力优越。 {circle around(4)}尺寸精度优越。

    Preparation process of polyhydroxycarboxylic acid
    86.
    发明授权
    Preparation process of polyhydroxycarboxylic acid 失效
    聚羟基羧酸的制备方法

    公开(公告)号:US5770683A

    公开(公告)日:1998-06-23

    申请号:US546311

    申请日:1995-10-20

    IPC分类号: C08G63/06 C08G63/91

    CPC分类号: C08G63/912 C08G63/06

    摘要: A preparation process of polyhydroxycarboxylic acid comprising conducting dehydration polycondensation of hydroxycarboxylic acid or an oligomer of the same in a reaction mixture containing said hydroxycarboxylic acid or the oligomer of the same and an organic solvent substantially in the absence of water to give polyhydroxycarboxylic acid having an weight average molecular weight of 50,000 or more, successively mixing the reaction mixture containing said polyhydroxycarboxylic acid with at least one binder selected from the group consisting of (1) polyisocyanate compound, (2) polybasic acid anhydride, (3) cyclic imino ester, (4) cyclic imino ether, (5) aromatic hydroxycarboxylic acid, (6) polyamino compound, (7) polyhydric alcohol, (8) epoxy compound, (9) polyfunctional aziridine compound, (10) lactam, (11) lactone, and (12) diethylene glycol bischloroforate, and reacting to obtain polyhydroxycarboxylic acid having a weight average molecular weight of 100,000 or more the polyhydroxycarboxylic acid which is obtained by the process has a weight average molecular weight of 100,000 or more, has satisfactory mechanical strength in the form of molded articles and is useful as a degradable polymer for substituting medical materials and general purpose resins.

    摘要翻译: 一种聚羟基羧酸的制备方法,其包括在含有羟基羧酸或其低聚物的反应混合物中进行羟基羧酸或其低聚物的脱水缩聚,基本上不存在水,得到具有重量的多羟基羧酸 将(1)多异氰酸酯化合物,(2)多元酸酐,(3)环状亚氨基酯,(4)的多元酸酐,(4) )环状亚氨基醚,(5)芳族羟基羧酸,(6)聚氨基化合物,(7)多元醇,(8)环氧化合物,(9)多官能氮丙啶化合物,(10)内酰胺,(11)内酯和(12 )二甘醇双氯氟酸盐,并且反应得到重均分子量为100,000以上的聚羟基
    羧酸 通过该方法获得的氧酸的重均分子量为100,000以上,成型品的机械强度良好,作为用于代替医用材料和通用树脂的可降解聚合物是有用的。