摘要:
The semiconductive roller according to the present invention includes a roller body having an outer peripheral surface made of a crosslinked substance of a semiconductive rubber composition and exhibiting Shore A hardness of not more than 60, the semiconductive rubber composition contains a base polymer made of a mixture of (1) mixed rubber N of liquid nitrile rubber and solid nitrile rubber, (2) chloroprene rubber C, and (3) epichlorohydrin rubber E in a mass ratio (C+E)/N of 10/90 to 80/20, the ratios of the chloroprene rubber and the epichlorohydrin rubber in the total quantity of the base polymer are not less than 5 mass % and not less than 5 mass % respectively, and roller resistance at an applied voltage of 5 V is not less than 104Ω and not more than 109Ω.
摘要:
A developing roller is provided, which is particularly used in an image forming apparatus of a highly durable design and is free from toner leakage even after formation of a predetermined number of images. Opposite end regions (5a) of an outer peripheral surface (5) of a roller body (2) of the developing roller (1) to be respectively kept in sliding contact with seal members each have a friction coefficient μ of not greater than 0.15.
摘要:
An inventive developing roller is adapted for use in an electrophotographic image forming apparatus. The developing roller includes a roller body. At least an outer peripheral surface of the roller body is formed from a rubber composition containing a base rubber. The base rubber contains a styrene butadiene rubber in a proportion of not less than 10 mass % and not greater than 70 mass % based on the overall amount of the base rubber. The outer peripheral surface of the rubber body has a surface roughness Ra of not less than 0.78 μm and not greater than 1.8 μm.
摘要:
An inventive developing roller is adapted for use in an electrophotographic image forming apparatus. The developing roller includes a roller body. At least an outer peripheral surface of the roller body is formed from a rubber composition containing a base rubber. The base rubber contains a styrene butadiene rubber in a proportion of not less than 10 mass % and not greater than 70 mass % based on the overall amount of the base rubber. The outer peripheral surface of the rubber body has a surface roughness Ra of not less than 0.78 μm and not greater than 1.8 μm.
摘要:
A developing roller is provided, which is particularly used in an image forming apparatus of a highly durable design and is free from toner leakage even after formation of a predetermined number of images. Opposite end regions (5a) of an outer peripheral surface (5) of a roller body (2) of the developing roller (1) to be respectively kept in sliding contact with seal members each have a friction coefficient μ of not greater than 0.15.
摘要:
The semiconductive roller according to the present invention includes a roller body having an outer peripheral surface made of a crosslinked substance of a semiconductive rubber composition and exhibiting Shore A hardness of not more than 60, the semiconductive rubber composition contains a base polymer made of a mixture of (1) mixed rubber N of liquid nitrile rubber and solid nitrile rubber, (2) chloroprene rubber C, and (3) epichlorohydrin rubber E in a mass ratio (C+E)/N of 10/90 to 80/20, the ratios of the chloroprene rubber and the epichlorohydrin rubber in the total quantity of the base polymer are not less than 5 mass % and not less than 5 mass % respectively, and roller resistance at an applied voltage of 5 V is not less than 104Ω and not more than 109Ω.