Method for producing improved aluminum conductor from direct chill cast
ingot
    4.
    发明授权
    Method for producing improved aluminum conductor from direct chill cast ingot 失效
    从直接冷却铸锭生产改进的铝导体的方法

    公开(公告)号:US4397696A

    公开(公告)日:1983-08-09

    申请号:US334654

    申请日:1981-12-28

    IPC分类号: C22F1/04

    CPC分类号: C22F1/04

    摘要: Aluminum conductor is made from direct chill cast (DC) ingot with improved conductivity and creep resistance by heating an aluminum-base alloy ingot containing not more than 0.40 wt. % and preferably not more than 0.30 wt. % Fe or a mixture of Mg, Ni or Zr with Fe to a temperature of 400.degree. to 600.degree. C., hot rolling the ingot in this temperature range and then further hot rolling at a reduced temperature range of 175.degree. to 325.degree. C.

    摘要翻译: 铝导体由通过加热含有不大于0.40重量%的铝基合金锭的直接冷铸(DC)锭制成,具有改进的导电性和抗蠕变性。 %,优选不大于0.30重量%。 %Fe或Mg,Ni或Zr与Fe的混合物在400〜600℃的温度下,在该温度范围内热轧锭,然后在175〜325℃的降低的温度范围进一步热轧 。

    Aluminum alloy two-step aging method and article
    5.
    发明授权
    Aluminum alloy two-step aging method and article 失效
    铝合金两步老化方法及制品

    公开(公告)号:US4861391A

    公开(公告)日:1989-08-29

    申请号:US132889

    申请日:1987-12-14

    摘要: A method for thermally treating an article made from an aluminum alloy having a first temperature at which solute atoms cluster to yield nuclei for the formation and growth of strengthening precipitates, and a second higher temperature at which the strengthening precipitates dissolve. The method comprises: heating the article to allow substantially all soluble alloy components to enter into solution; rapidly cooling the article in a quenching medium; and precipitation hardening the article by aging at or below the first temperature for a few hours to several months; then aging above the first temperature and below the second temperature until desired strength is achieved. A method for imparting improved combinations of strength and fracture toughness to a solution heat treated-article which includes an aluminum-lithium alloy is also disclosed. This method comprises aging the article at one or more temperatures at or below a first temperature of about 93.degree. C. (200.degree. F.) for a few hours to several months; and further aging the article at one or more temperatures above the first temperature and below a second temperature of about 219.degree. C. (425.degree. F.) for at least about 30 minutes.

    Aluminum-lithium alloys
    7.
    发明授权
    Aluminum-lithium alloys 失效
    铝 - 锂合金

    公开(公告)号:US5137686A

    公开(公告)日:1992-08-11

    申请号:US149802

    申请日:1988-01-28

    摘要: Disclosed is an aluminum base alloy suitable for forming into a wrought product having improved combinations of strength, corrosion resistance and fracture toughness. The alloy is comprised of 0.2 to 5.0 wt. % Li, 0.05 to 6.0 wt. % Mg, at least 2.45 wt. % Cu, 0.01 to 0.16 wt. % Zr, 0.05 to 12 wt. % Zn, 0.5 wt. % max. Fe, 0.5 wt. % max. Si, the balance aluminum and incidental impurities.

    摘要翻译: 公开了一种适合于形成具有改进的强度,耐腐蚀性和断裂韧性组合的锻造产品的铝基合金。 该合金由0.2〜5.0重量% %Li,0.05〜6.0重量% %Mg,至少2.45wt。 %Cu,0.01〜0.16wt。 %Zr,0.05〜12wt。 %Zn,0.5wt。 最大% Fe,0.5wt。 最大% Si,余量为铝和杂质。