METHOD TO INCREASE THE EFFICIENCY OF POLYMER DRAG REDUCTION FOR MARINE AND INDUSTRIAL APPLICATIONS
    3.
    发明申请
    METHOD TO INCREASE THE EFFICIENCY OF POLYMER DRAG REDUCTION FOR MARINE AND INDUSTRIAL APPLICATIONS 有权
    提高海洋和工业应用聚合物减少效率的方法

    公开(公告)号:US20080254226A1

    公开(公告)日:2008-10-16

    申请号:US11968573

    申请日:2008-01-02

    IPC分类号: B05D1/18

    摘要: A method for increasing the efficiency of additive drag reduction by establishing a drag-reducing viscoelastic coating on a surface. The method includes mixing a polymer into a concentrated solution that has approximately the same density as a fluid flowing over the surface, ejecting the mixture/solution into the flowing fluid in a manner such that a coating of polymer, which initially grows thicker with time, is adsorbed onto the surface, and reducing the ejection rate of the first fluid such that the coating of polymer then grows thinner with time. These steps may be repeated so that a desired minimum coating thickness is maintained over an extended period of time. The method reduces the polymer expenditure rate for a given drag reduction. Moreover, the produced viscoelastic coating impedes the attachment and growth of drag-producing natural organisms and may be applied without “down-time” (e.g., while underway).

    摘要翻译: 通过在表面上建立减阻粘弹性涂层来提高添加剂减阻效率的方法。 该方法包括将聚合物混合成浓缩溶液,该浓缩溶液具有与流过表面的流体大致相同的密度,将混合物/溶液以这样的方式喷射到流动的流体中,使得最初随时间变厚的聚合物涂层, 被吸附到表面上,并且降低第一流体的喷射速率,使得聚合物的涂层随着时间变得越来越薄。 可以重复这些步骤,使得在延长的时间段内保持期望的最小涂层厚度。 该方法降低了给定减阻的聚合物支出率。 此外,生产的粘弹性涂层阻止产生生产天然生物体的附着和生长,并且可以在没有“停机时间”(例如在进行中)的情况下施用。

    Method to increase the efficiency of polymer drag reduction for marine and industrial applications
    5.
    发明授权
    Method to increase the efficiency of polymer drag reduction for marine and industrial applications 有权
    提高海洋和工业应用聚合物减阻效率的方法

    公开(公告)号:US08039055B2

    公开(公告)日:2011-10-18

    申请号:US11968573

    申请日:2008-01-02

    IPC分类号: B05D5/00 B63B1/34

    摘要: A method for increasing the efficiency of additive drag reduction by establishing a drag-reducing viscoelastic coating on a surface. The method includes mixing a polymer into a concentrated solution that has approximately the same density as a fluid flowing over the surface, ejecting the mixture/solution into the flowing fluid in a manner such that a coating of polymer, which initially grows thicker with time, is adsorbed onto the surface, and reducing the ejection rate of the first fluid such that the coating of polymer then grows thinner with time. These steps may be repeated so that a desired minimum coating thickness is maintained over an extended period of time. The method reduces the polymer expenditure rate for a given drag reduction. Moreover, the produced viscoelastic coating impedes the attachment and growth of drag-producing natural organisms and may be applied without “down-time” (e.g., while underway).