摘要:
Prepare polymeric foam articles having low yellowing using a styrene-acrylonitrile copolymer that contains less than 145 weight-parts acrylonitrile dimer and less than 8,500 weight-parts acrylonitrile trimer per million weight parts acrylonitrile copolymer.
摘要:
Prepare polymeric foam articles having low yellowing using a styrene-acrylonitrile copolymer that contains less than 145 weight-parts acrylonitrile dimer and less than 8,500 weight-parts acrylonitrile trimer per million weight parts acrylonitrile copolymer.
摘要:
Provide a foamable polymer composition containing: (i) a thermoplastic polymer matrix and a blowing agent, (a) the thermoplastic polymer matrix containing a styrene-acrylonitrile copolymer having a weight-averaged molecular weight in a range of 90,000 to 150,000 and polymerized acrylonitrile concentration in a range of five to twenty weight-percent relative to total polymer matrix weight; and (ii) a blowing agent containing water, 1,1,1,2-tetrafluouroethane and at least one of difluoromethane and 1,1-dilluoroethane; (b) cooling the foamable polymer composition to a foaming temperature; and (c) extruding the foamable polymer composition and allowing the blowing agent to expand the foamable polymer composition into a polymeric foam having an average vertical cell size in a range of 0.5 millimeters to 1.8 millimeters and a density in a range of 24 to 40 kilograms per cubic meter and a Normalized Roughness Quotient of 3.5 or less in a Milled Surface Test.
摘要:
The present invention is directed to a coaxial cable comprising (a) an inner conductor, (b) an outer conductor, and (c) a foamed insulation, surrounding the inner conductor. The foamed insulation is prepared from an insulation composition comprising a foamable polymer, a foaming agent, and a particulate, non-halogenated, nonheterocyclic polyolefinic nucleating agent. The invention is also related to methods and compositions for making the foamed insulation.
摘要:
An extruded polymeric foam comprising a styrenic polymer and an olefinic polymer, the olefinic polymer in an amount less than the amount of the styrenic polymer. The styrenic polymer and the olefinic polymer are present as a blend, preferably free of an interpolymer or compatiblizer. The foam has a density below about 36 kg/m3 (as measured by ASTM D1622-03), a vertical compressive strength greater than about 100 kPa (as measured by ASTM D1621-04) and a compressive strength ratio greater than about 0.35.
摘要翻译:包含苯乙烯聚合物和烯烃聚合物的挤出聚合物泡沫体,该烯烃聚合物的量小于苯乙烯聚合物的量。 苯乙烯聚合物和烯烃聚合物作为共混物存在,优选不含互聚物或增容剂。 泡沫的密度低于约36kg / m 3(通过ASTM D1622-03测量),大于约100kPa的垂直压缩强度(通过ASTM D1621-04测量),抗压强度比大于约0.35。