Method for priming wet or dry road surfaces
    2.
    发明授权
    Method for priming wet or dry road surfaces 失效
    灌注湿路面或干路面的方法

    公开(公告)号:US5468795A

    公开(公告)日:1995-11-21

    申请号:US079158

    申请日:1993-06-17

    申请人: Harald Guder

    发明人: Harald Guder

    CPC分类号: C09D5/00 E01F9/512

    摘要: Priming composition containing a homogeneous liquid solution containing a polymeric material and at least one water-miscible solvent in an amount sufficient to provide adhesion between wet or dry road surface materials and adhesive coated articles. The priming composition allows the marking of roadways with pressure sensitive adhesive articles even on wet or damp roadway surfaces. Also a method for priming roadway surfaces.

    摘要翻译: 含有含有聚合物材料的均匀液体溶液和至少一种水混溶性溶剂的引发组合物,其量足以提供湿路面或干路面材料与粘合剂涂覆制品之间的粘合。 起动组合物允许在湿路面或潮湿的道路表面上用压敏粘合剂制品标记道路。 也是一种用于起动道路表面的方法。

    Electrophoretically overcoatable coatings applied by electrocoating
    4.
    发明授权
    Electrophoretically overcoatable coatings applied by electrocoating 失效
    通过电泳涂覆电泳过涂覆涂层

    公开(公告)号:US4882090A

    公开(公告)日:1989-11-21

    申请号:US72269

    申请日:1987-08-17

    摘要: The invention relates to cathodically depositable aqueous electropaints which contain cationic amine-modified epoxy resins and are pigmented with electroconductive carbon black and which, on deposition and crosslinking, provide electrophoretically overcoatable coatings and contain as electroconductive carbon black a carbon black having an iodine absorption of 870-930 mg/g, a specific surface area (BET/N.sub.2) of 850-1,000 m.sup.2 /g, a pore volume (DBP) of 330-390 ml/100 g and an average particle size of 25-35 nm in an amount of 1.5 to 5.1% by weight - based on total solids.

    摘要翻译: PCT No.PCT / EP86 / 00585 Sec。 371日期1987年8月17日 102(e)日期1987年8月17日PCT提交1986年10月13日PCT公布。 出版物WO87 / 02717 日本1987年5月7日。本发明涉及含有阳离子胺改性环氧树脂并用导电炭黑着色的阴极可沉积的含水电极,并且在沉积和交联时,提供电泳可过涂层的涂层并且包含作为导电炭黑的炭黑 碘吸收量为870-930mg / g,比表面积(BET / N 2)为850-1,000m 2 / g,孔体积(DBP)为330-390ml / 100g,平均粒径为25 -35nm,其量为基于总固体的1.5至5.1重量%。