Frame member used in friction stir welding
    1.
    发明授权
    Frame member used in friction stir welding 失效
    框架构件用于摩擦搅拌焊接

    公开(公告)号:US06640515B1

    公开(公告)日:2003-11-04

    申请号:US09547042

    申请日:2000-04-11

    IPC分类号: E04B208

    摘要: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in a joining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out. After the joining, the remaining parts of the thickened parts can be machined so as to form a smooth surface.

    摘要翻译: 公开了一种摩擦搅拌焊接技术,其避免了在接合区域中延伸到接合表面下方的凹陷处的凹陷。 在要连接的框架构件的端部处,在接合区域设置朝向旋转体接合工具突出的加厚部。 邻接的待连接件的两个相邻的加厚件可以形成梯形。 旋转体接合工具具有小直径末端部分和较大直径部分。 旋转体接合工具插入加厚部分。 在旋转体接合工具首先插入小直径尖端的状态下,到旋转体接合工具的较大直径部分与增厚部分重叠但不延伸到未加厚的上表面的水平 所述构件的表面接合,所述旋转体沿所述接合区旋转并移动。 即使在两个加厚部分之间存在间隙,也可以进行所需的接合。 在接合之后,加工部件的其余部分可以加工成形成光滑的表面。

    Structure joined by friction stir welding
    4.
    发明授权
    Structure joined by friction stir welding 失效
    结构通过摩擦搅拌焊接

    公开(公告)号:US06305866B1

    公开(公告)日:2001-10-23

    申请号:US09546564

    申请日:2000-04-11

    IPC分类号: B23K2012

    摘要: A friction stir welding technique which avoids occurrence of a dent, in a joining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out. After the joining, the remaining parts of the thickened parts can be machined so as to form a smooth surface.

    摘要翻译: 一种摩擦搅拌焊接技术,其避免在接合区域中发生凹陷,延伸到接合表面下方的水平面。 在要连接的框架构件的端部处,在接合区域设置朝向旋转体接合工具突出的加厚部。 邻接的待连接件的两个相邻的加厚件可以形成梯形。 旋转体接合工具具有小直径末端部分和较大直径部分。 旋转体接合工具插入加厚部分。 在旋转体接合工具首先插入小直径尖端的状态下,到旋转体接合工具的较大直径部分与增厚部分重叠但不延伸到未加厚的上表面的水平 所述构件的表面接合,所述旋转体沿所述接合区旋转并移动。 即使在两个加厚部分之间存在间隙,也可以进行所需的接合。 在接合之后,加工部件的其余部分可以加工成形成光滑的表面。

    Structure and railway car
    5.
    发明授权
    Structure and railway car 失效
    结构和铁路车

    公开(公告)号:US06722286B2

    公开(公告)日:2004-04-20

    申请号:US10188865

    申请日:2002-07-05

    IPC分类号: B61D1704

    摘要: In a railway car, extruded frame members of an aluminum base alloy containing Si of 0.4-0.9 wt % and Mg of 0.4-1.2 wt % are welded according to a friction stir welding method. In a structure, an aluminum base alloy plate containing Si of 0.4-0.9 wt % and Mg of 0.4-1.2 wt % is prepared, to one face of the aluminum base alloy plate a rib is formed, and the aluminum base alloy plate is an extruded frame member. Accordingly, a railway car having a low welding distortion and a structure having a low welding distortion can be obtained.

    摘要翻译: 在铁路车辆中,根据摩擦搅拌焊接方法焊接包含0.4-0.9重量%的Si和0.4-1.2重量%的Mg的铝基合金的挤压框架构件。 在一种结构中,制备含有0.4-0.9重量%的Si和0.4-1.2重量%的Mg的铝基合金板,在铝基合金板的一个面上形成肋,铝基合金板是 挤压框架构件。 因此,可以获得具有低焊接变形的轨道车辆和具有低焊接变形的结构。

    Structural body formed by friction stir welding
    6.
    发明授权
    Structural body formed by friction stir welding 失效
    结构体通过摩擦搅拌焊接形成

    公开(公告)号:US06716538B2

    公开(公告)日:2004-04-06

    申请号:US10095479

    申请日:2002-03-13

    IPC分类号: C25D510

    摘要: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out. After the joining, the remaining parts of the thickened parts can be machined so as to form a smooth surface.

    摘要翻译: 公开了一种摩擦搅拌焊接技术,其避免在邻接区域中发生凹陷,延伸到接合表面下方的水平。 在要连接的框架构件的端部处,在接合区域设置朝向旋转体接合工具突出的加厚部。 邻接的待连接件的两个相邻的加厚件可以形成梯形。 旋转体接合工具具有小直径末端部分和较大直径部分。 旋转体接合工具插入加厚部分。 在旋转体接合工具已经插入小直径尖端并且首先到达旋转体接合工具的较大直径部分与增厚部分重叠但不延伸到未加厚的上表面的水平的水平 所述构件的表面接合,所述旋转体沿所述接合区旋转并移动。 即使在两个加厚部分之间存在间隙,也可以进行所需的接合。 在接合之后,加工部件的其余部分可以加工成形成光滑的表面。

    Friction stir welding method including positioning of rotary tool, and structural body formed thereby
    8.
    发明授权
    Friction stir welding method including positioning of rotary tool, and structural body formed thereby 失效
    摩擦搅拌焊接方法,包括旋转工具的定位和由此形成的结构体

    公开(公告)号:US06382498B2

    公开(公告)日:2002-05-07

    申请号:US09828835

    申请日:2001-04-10

    IPC分类号: B23K2012

    摘要: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out. After the joining, the remaining parts of the thickened parts can be machined so as to form a smooth surface.

    摘要翻译: 公开了一种摩擦搅拌焊接技术,其避免在邻接区域中发生凹陷,延伸到接合表面下方的水平。 在要连接的框架构件的端部处,在接合区域设置朝向旋转体接合工具突出的加厚部。 邻接的待连接件的两个相邻的加厚件可以形成梯形。 旋转体接合工具具有小直径末端部分和较大直径部分。 旋转体接合工具插入加厚部分。 在旋转体接合工具已经插入小直径尖端并且首先到达旋转体接合工具的较大直径部分与增厚部分重叠但不延伸到未加厚的上表面的水平的水平 所述构件的表面接合,所述旋转体沿所述接合区旋转并移动。 即使在两个加厚部分之间存在间隙,也可以进行所需的接合。 在接合之后,加工部件的其余部分可以加工成形成光滑的表面。

    Structural body formed by friction stir welding two members, one of which has a protruding portion
    10.
    发明授权
    Structural body formed by friction stir welding two members, one of which has a protruding portion 失效
    结构体通过摩擦搅拌形成两个构件,其中一个具有突出部分

    公开(公告)号:US06585443B2

    公开(公告)日:2003-07-01

    申请号:US09828833

    申请日:2001-04-10

    IPC分类号: B23K2012

    摘要: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out. After the joining, the remaining parts of the thickened parts can be machined so as to form a smooth surface.

    摘要翻译: 公开了一种摩擦搅拌焊接技术,其避免在邻接区域中发生凹陷,延伸到接合表面下方的水平。 在要连接的框架构件的端部处,在接合区域设置朝向旋转体接合工具突出的加厚部。 邻接的待连接件的两个相邻的加厚件可以形成梯形。 旋转体接合工具具有小直径末端部分和较大直径部分。 旋转体接合工具插入加厚部分。 在旋转体接合工具已经插入小直径尖端并且首先到达旋转体接合工具的较大直径部分与增厚部分重叠但不延伸到未加厚的上表面的水平的水平 所述构件的表面接合,所述旋转体沿所述接合区旋转并移动。 即使在两个加厚部分之间存在间隙,也可以进行所需的接合。 在接合之后,加工部件的其余部分可以加工成形成光滑的表面。