公开(公告)号:US20120324950A1
公开(公告)日:2012-12-27
申请号:US13473130
申请日:2012-05-16
申请人: George O. Dale , Juergen Tinz
发明人: George O. Dale , Juergen Tinz
IPC分类号: C03B25/087
CPC分类号: C03B29/10
摘要: Disclosed is an apparatus and method for heat treating glass sheets, and in particular for heat treating very thing glass sheets arranged in closely spaced stacks. The glass sheets are positioned on a moving belt such that their major surfaces are substantially perpendicular to a direction of belt travel through the apparatus to aid in producing a uniform temperature profile within the glass sheets. The apparatus comprises air curtains positioned at the inlet and outlet of the apparatus to minimize the ingress of particulate into the apparatus. A reduced velocity of heated air flow within a lower portion of the apparatus relative to a velocity of the heated air in an upper portion of the apparatus causes particulate to drop out of the lower portion air flow. A rotating brush and vacuums positioned adjacent a lower portion of the belt assist in removing particulate from the moving belt.
摘要翻译: 公开了一种用于热处理玻璃板的设备和方法,特别是用于热处理布置成紧密堆叠的非常物品的玻璃板。 玻璃板定位在移动的带上,使得它们的主表面基本上垂直于穿过设备的带行进方向,以帮助在玻璃板内产生均匀的温度分布。 该装置包括设置在设备的入口和出口处的气帘,以最小化颗粒进入装置的进入。 相对于设备上部的加热空气的速度,设备下部内的加热空气流的减小的速度导致颗粒从下部气流中流出。 靠近皮带下部定位的旋转电刷和真空吸尘器有助于从运动皮带移除颗粒物。
-
公开(公告)号:US07198673B2
公开(公告)日:2007-04-03
申请号:US11059980
申请日:2005-02-16
申请人: John H. Brennan , Michael W. Price , Juergen Tinz , Liming Wang
发明人: John H. Brennan , Michael W. Price , Juergen Tinz , Liming Wang
IPC分类号: C30B11/00
CPC分类号: C30B33/00 , C30B29/12 , Y10T117/10 , Y10T117/1016 , Y10T117/1024
摘要: A method of making below 250-nm UV light transmitting optical fluoride lithography crystals includes applying heat along a shortest path of conduction of a selected optical fluoride crystal, heating the optical fluoride crystal to an annealing temperature, holding the temperature of the optical fluoride crystal at the annealing temperature, and gradually cooling the optical fluoride crystal to provide a low-birefringence optical fluoride crystal for transmitting below 250-nm UV light.
摘要翻译: 制造低于250nm的UV光透射光学氟化物光刻晶体的方法包括沿着所选择的氟化物晶体的最短导通路径施加热量,将氟化物晶体加热到退火温度,将氟化物晶体的温度保持在 退火温度,并逐渐冷却光氟化物晶体,以提供低于250nm紫外光的低双折射氟化物晶体。
-
公开(公告)号:US06997987B2
公开(公告)日:2006-02-14
申请号:US10611505
申请日:2003-06-30
申请人: John H. Brennan , Michael W. Price , Juergen Tinz , Liming Wang
发明人: John H. Brennan , Michael W. Price , Juergen Tinz , Liming Wang
IPC分类号: C30B11/04
CPC分类号: C30B33/00 , C30B29/12 , Y10T117/10 , Y10T117/1016 , Y10T117/1024
摘要: A method of making below 250-nm UV light transmitting optical fluoride lithography crystals includes applying heat along a shortest path of conduction of a selected optical fluoride crystal, heating the optical fluoride crystal to an annealing temperature, holding the temperature of the optical fluoride crystal at the annealing temperature, and gradually cooling the optical fluoride crystal to provide a low-birefringence optical fluoride crystal for transmitting below 250-nm UV light.
摘要翻译: 制造低于250nm的UV光透射光学氟化物光刻晶体的方法包括沿着所选择的氟化物晶体的最短导通路径施加热量,将氟化物晶体加热到退火温度,将氟化物晶体的温度保持在 退火温度,并逐渐冷却光氟化物晶体,以提供低于250nm紫外光的低双折射氟化物晶体。
-
公开(公告)号:US08857215B2
公开(公告)日:2014-10-14
申请号:US13473130
申请日:2012-05-16
申请人: George O. Dale , Juergen Tinz
发明人: George O. Dale , Juergen Tinz
IPC分类号: C03B29/10
CPC分类号: C03B29/10
摘要: Disclosed is an apparatus and method for heat treating glass sheets, and in particular for heat treating very thing glass sheets arranged in closely spaced stacks. The glass sheets are positioned on a moving belt such that their major surfaces are substantially perpendicular to a direction of belt travel through the apparatus to aid in producing a uniform temperature profile within the glass sheets. The apparatus comprises air curtains positioned at the inlet and outlet of the apparatus to minimize the ingress of particulate into the apparatus. A reduced velocity of heated air flow within a lower portion of the apparatus relative to a velocity of the heated air in an upper portion of the apparatus causes particulate to drop out of the lower portion air flow. A rotating brush and vacuums positioned adjacent a lower portion of the belt assist in removing particulate from the moving belt.
摘要翻译: 公开了一种用于热处理玻璃板的设备和方法,特别是用于热处理布置成紧密堆叠的非常物品的玻璃板。 玻璃板定位在移动的带上,使得它们的主表面基本上垂直于穿过设备的带行进方向,以帮助在玻璃板内产生均匀的温度分布。 该装置包括设置在设备的入口和出口处的气帘,以最小化颗粒进入装置的进入。 相对于设备上部的加热空气的速度,设备下部内的加热空气流的减小的速度导致颗粒从下部空气流中流出。 靠近皮带下部定位的旋转电刷和真空吸尘器有助于从运动皮带移除颗粒物。
-
公开(公告)号:US20050139152A1
公开(公告)日:2005-06-30
申请号:US11059980
申请日:2005-02-16
申请人: John Brennan , Michael Price , Juergen Tinz , Liming Wang
发明人: John Brennan , Michael Price , Juergen Tinz , Liming Wang
IPC分类号: C30B29/12 , C30B1/00 , C30B9/00 , C30B11/00 , C30B17/00 , C30B21/02 , C30B28/06 , C30B33/00 , C30B33/02
CPC分类号: C30B33/00 , C30B29/12 , Y10T117/10 , Y10T117/1016 , Y10T117/1024
摘要: A method of making below 250-nm UV light transmitting optical fluoride lithography crystals includes applying heat along a shortest path of conduction of a selected optical fluoride crystal, heating the optical fluoride crystal to an annealing temperature, holding the temperature of the optical fluoride crystal at the annealing temperature, and gradually cooling the optical fluoride crystal to provide a low-birefringence optical fluoride crystal for transmitting below 250-nm UV light.
摘要翻译: 制造低于250nm的UV光透射光学氟化物光刻晶体的方法包括沿着所选择的氟化物晶体的最短导通路径施加热量,将氟化物晶体加热到退火温度,将氟化物晶体的温度保持在 退火温度,并逐渐冷却光氟化物晶体,以提供低于250nm紫外光的低双折射氟化物晶体。
-
公开(公告)号:US20050109270A1
公开(公告)日:2005-05-26
申请号:US10611505
申请日:2003-06-30
申请人: John Brennan , Michael Price , Juergen Tinz , Liming Wang
发明人: John Brennan , Michael Price , Juergen Tinz , Liming Wang
IPC分类号: C30B29/12 , C30B1/00 , C30B9/00 , C30B11/00 , C30B17/00 , C30B21/02 , C30B28/06 , C30B33/00 , C30B33/02
CPC分类号: C30B33/00 , C30B29/12 , Y10T117/10 , Y10T117/1016 , Y10T117/1024
摘要: A method of making below 250-nm UV light transmitting optical fluoride lithography crystals includes applying heat along a shortest path of conduction of a selected optical fluoride crystal, heating the optical fluoride crystal to an annealing temperature, holding the temperature of the optical fluoride crystal at the annealing temperature, and gradually cooling the optical fluoride crystal to provide a low-birefringence optical fluoride crystal for transmitting below 250-nm UV light.
-
-
-
-
-