Continuous processing of asphalt formulations
    1.
    发明授权
    Continuous processing of asphalt formulations 有权
    连续加工沥青配方

    公开(公告)号:US09187644B2

    公开(公告)日:2015-11-17

    申请号:US14143074

    申请日:2013-12-30

    摘要: The subject invention provides a method for producing essentially homogeneous asphalt compositions which are comprised of the asphalt, a block copolymer (such as a linear block copolymer or a radial block copolymer), and one or more additional desired additives. This method offers the advantage of being capable of attaining the essentially homogeneous asphalt composition in one pass procedure with a short residence time in the mixing equipment. This greatly reduces the thermal history to which heat sensitive asphalt additives, such as asphalt modification polymers, are exposed. It also simplifies the mixing procedure and can reduce the overall amount of energy required to attain the desired blend. In some case, it allows for the production on a commercial basis of asphalt compositions which would otherwise not be feasible, for instance the production of asphalt compositions which contain high levels of asphalt modifications polymers which are otherwise difficult to process.

    摘要翻译: 本发明提供了一种用于生产由沥青,嵌段共聚物(例如线性嵌段共聚物或径向嵌段共聚物)和一种或多种另外的所需添加剂组成的基本上均匀的沥青组合物的方法。 该方法具有以下优点:能够在一次通过程序中获得基本上均匀的沥青组合物,并且在混合设备中具有短的停留时间。 这大大降低了热敏沥青添加剂如沥青改性聚合物暴露的热历史。 它还简化了混合过程,并且可以减少达到所需共混物所需的总能量。 在某些情况下,它允许在商业基础上生产沥青组合物,否则这是不可行的,例如生产含有高含量沥青改性聚合物的沥青组合物,否则难以加工。

    Preparation of industrial asphalt
    2.
    发明授权
    Preparation of industrial asphalt 有权
    工业沥青的制备

    公开(公告)号:US08901211B2

    公开(公告)日:2014-12-02

    申请号:US13478236

    申请日:2012-05-23

    摘要: The present invention relates to a method for preparing an industrial asphalt comprising sparging an oxygen containing gas through an asphalt flux in the presence of 0.25 weight percent to about 12 weight percent of a highly saturated rubbery polymer at a temperature within the range of about 400° F. to about 550° F. for a period of time which is sufficient to increase the softening point of the asphalt flux to a value which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm to produce the industrial asphalt. The highly saturated rubbery polymer can be a styrene-ethylene/butylene-styrene block copolymer rubber or a highly saturated styrene-ethylene/propylene-styrene block copolymer rubber.

    摘要翻译: 本发明涉及一种制备工业沥青的方法,其包括在约400℃的温度范围内,在0.25重量%至约12重量%的高度饱和的橡胶状聚合物的存在下,通过沥青助熔剂喷射含氧气体 F.至约550°F,持续一段时间,其足以将沥青助焊剂的软化点增加至185°F至250°F范围内的值,并且至少渗透值 15 dmm生产工业沥青。 高度饱和的橡胶状聚合物可以是苯乙烯 - 乙烯/丁烯 - 苯乙烯嵌段共聚物橡胶或高度饱和的苯乙烯 - 乙烯/丙烯 - 苯乙烯嵌段共聚物橡胶。

    PREPARATION OF INDUSTRIAL ASPHALT
    3.
    发明申请
    PREPARATION OF INDUSTRIAL ASPHALT 有权
    工业沥青的制备

    公开(公告)号:US20120302673A1

    公开(公告)日:2012-11-29

    申请号:US13478236

    申请日:2012-05-23

    IPC分类号: C08L95/00

    摘要: The present invention relates to a method for preparing an industrial asphalt comprising sparging an oxygen containing gas through an asphalt flux in the presence of 0.25 weight percent to about 12 weight percent of a highly saturated rubbery polymer at a temperature within the range of about 400° F. to about 550° F. for a period of time which is sufficient to increase the softening point of the asphalt flux to a value which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm to produce the industrial asphalt. The highly saturated rubbery polymer can be a styrene-ethylene/butylene-styrene block copolymer rubber or a highly saturated styrene-ethylene/propylene-styrene block copolymer rubber.

    摘要翻译: 本发明涉及一种制备工业沥青的方法,其包括在约400℃的温度范围内,在0.25重量%至约12重量%的高度饱和的橡胶状聚合物的存在下,通过沥青助熔剂喷射含氧气体 F.至约550°F,持续一段时间,其足以将沥青助焊剂的软化点增加至185°F至250°F范围内的值,并且至少渗透值 15 dmm生产工业沥青。 高度饱和的橡胶状聚合物可以是苯乙烯 - 乙烯/丁烯 - 苯乙烯嵌段共聚物橡胶或高度饱和的苯乙烯 - 乙烯/丙烯 - 苯乙烯嵌段共聚物橡胶。

    PREPARATION OF INDUSTRIAL ASPHALT
    4.
    发明申请
    PREPARATION OF INDUSTRIAL ASPHALT 有权
    工业沥青的制备

    公开(公告)号:US20150087734A1

    公开(公告)日:2015-03-26

    申请号:US14554180

    申请日:2014-11-26

    IPC分类号: C08L95/00

    摘要: The present invention relates to a method for preparing an industrial asphalt comprising sparging an oxygen containing gas through an asphalt flux in the presence of 0.25 weight percent to about 12 weight percent of a highly saturated rubbery polymer at a temperature within the range of about 400° F. to about 550° F. for a period of time which is sufficient to increase the softening point of the asphalt flux to a value which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm to produce the industrial asphalt. The highly saturated rubbery polymer can be a styrene-ethylene/butylene-styrene block copolymer rubber or a highly saturated styrene-ethylene/propylene-styrene block copolymer rubber.

    摘要翻译: 本发明涉及一种制备工业沥青的方法,其包括在约400℃的温度范围内,在0.25重量%至约12重量%的高度饱和的橡胶状聚合物的存在下,通过沥青助熔剂喷射含氧气体 F.至约550°F,持续一段时间,其足以将沥青助焊剂的软化点增加至185°F至250°F范围内的值,并且至少渗透值 15 dmm生产工业沥青。 高度饱和的橡胶状聚合物可以是苯乙烯 - 乙烯/丁烯 - 苯乙烯嵌段共聚物橡胶或高度饱和的苯乙烯 - 乙烯/丙烯 - 苯乙烯嵌段共聚物橡胶。

    CONTINUOUS PROCESSING OF ASPHALT FORMULATIONS
    5.
    发明申请
    CONTINUOUS PROCESSING OF ASPHALT FORMULATIONS 有权
    沥青配方的连续加工

    公开(公告)号:US20140275337A1

    公开(公告)日:2014-09-18

    申请号:US14143074

    申请日:2013-12-30

    IPC分类号: C08L95/00

    摘要: The subject invention provides a method for producing essentially homogeneous asphalt compositions which are comprised of the asphalt, a block copolymer (such as a linear block copolymer or a radial block copolymer), and one or more additional desired additives. This method offers the advantage of being capable of attaining the essentially homogeneous asphalt composition in one pass procedure with a short residence time in the mixing equipment. This greatly reduces the thermal history to which heat sensitive asphalt additives, such as asphalt modification polymers, are exposed. It also simplifies the mixing procedure and can reduce the overall amount of energy required to attain the desired blend. In some case, it allows for the production on a commercial basis of asphalt compositions which would otherwise not be feasible, for instance the production of asphalt compositions which contain high levels of asphalt modifications polymers which are otherwise difficult to process.

    摘要翻译: 本发明提供了一种用于生产由沥青,嵌段共聚物(例如线性嵌段共聚物或径向嵌段共聚物)和一种或多种另外的所需添加剂组成的基本均匀的沥青组合物的方法。 该方法具有以下优点:能够在一次通过程序中获得基本上均匀的沥青组合物,并且在混合设备中具有短的停留时间。 这大大降低了热敏沥青添加剂如沥青改性聚合物暴露的热历史。 它还简化了混合过程,并且可以减少达到所需共混物所需的总能量。 在某些情况下,它允许在商业基础上生产沥青组合物,否则这是不可行的,例如生产含有高含量沥青改性聚合物的沥青组合物,否则难以加工。