Abstract:
To obtain a nonwoven fabric which is excellent in the heat resistance and the chemical resistance, of which the fiber diameter is small, and which is excellent in the mechanical strength at a temperature at which it is used; and an electrolyte membrane which is excellent in the dimensional stability when it is swollen by water, and of which an increase in the resistance by a reinforcing material is suppressed.A nonwoven fabric 28 containing fibers 26 of an ethylene/tetrafluoroethylene copolymer having a storage elastic modulus E′ at 25° C. of at least 8×108 Pa and a melt viscosity measured at 300° C. of higher than 60 Pa·s and at most 300 Pa·s, wherein the average fiber diameter of the fibers is from 0.01 to 3 μm; and an electrolyte membrane reinforced by the nonwoven fabric 28.
Abstract:
To obtain a nonwoven fabric which is excellent in the heat resistance and the chemical resistance, of which the fiber diameter is small, and which is excellent in the mechanical strength at a temperature at which it is used; and an electrolyte membrane which is excellent in the dimensional stability when it is swollen by water, and of which an increase in the resistance by a reinforcing material is suppressed.A nonwoven fabric 28 containing fibers 26 of an ethylene/tetrafluoroethylene copolymer having a storage elastic modulus E′ at 25° C. of at least 8×108 Pa and a melt viscosity measured at 300° C. of higher than 60 Pa·s and at most 300 Pa·s, wherein the average fiber diameter of the fibers is from 0.01 to 3 μm; and an electrolyte membrane reinforced by the nonwoven fabric 28.
Abstract:
It is an object of the present invention to provide a nonwoven fabric which is excellent in the heat resistance and the chemical resistance, of which the fiber diameter is small, which is excellent in the strength and of which the maximum pore diameter is small.A nonwoven fabric made of an ethylene/tetrafluoroethylene copolymer, characterized in that the nonwoven fabric is mutually fused continuous fibers of an ethylene/tetrafluoroethylene copolymer which has a melt viscosity of from higher than 100 to 1,500 Pa·s at 240° C.
Abstract:
It is an object of the present invention to provide a nonwoven fabric which is excellent in the heat resistance and the chemical resistance, of which the fiber diameter is small, which is excellent in the strength and of which the maximum pore diameter is small.A nonwoven fabric made of an ethylene/tetrafluoroethylene copolymer, characterized in that the nonwoven fabric is mutually fused continuous fibers of an ethylene/tetrafluoroethylene copolymer which has a melt viscosity of from higher than 100 to 1,500 Pa˜s at 240° C.
Abstract:
To provide a process for producing a fluorinated copolymer nanocomposite comprising a fluorinated copolymer and inorganic fine particles dispersed therein to a high degree, and a process for producing a molded fluororesin product. The process for producing a fluorinated copolymer nanocomposite comprising a fluorinated copolymer and inorganic fine particles, characterized in that a mixture (A) containing a fluorinated copolymer comprised of repeating units based on tetrafluoroethylene and repeating units based on ethylene, inorganic fine particles, and a solvent which can dissolve the fluorinated copolymer under ordinary or elevated pressure at a temperature of not higher than the melting point of the fluorinated copolymer, is heated to at least a temperature at which the fluorinated copolymer dissolves in the solvent, and the solvent is subsequently removed. The process for producing a molded fluororesin product by using the fluorinated copolymer nanocomposite to produce a molded product.
Abstract:
To provide a method for easily producing an ethylene/tetrafluoroethylene copolymer porous material having excellent chemical resistance and filtration performance and has a high heat resistance, within a wide range of the porosity, and an ethylene/tetrafluoroethylene copolymer porous material obtained by such a process.A process for producing an ethylene/tetrafluoroethylene copolymer porous material which comprises a step of dissolving an ethylene/tetrafluoroethylene copolymer having repeating units based on ethylene and repeating units based on tetrafluoroethylene at a temperature of at most 300° C. in a solvent which can dissolve the ethylene/tetrafluoroethylene copolymer at a temperature of at most 300° C., to achieve a predetermined concentration to obtain a solution, a step of forming the solution to obtain a formed product, and a step of cooling the formed product to a temperature of at most the phase separation temperature of the solution to solidify the ethylene/tetrafluoroethylene copolymer.