摘要: The object of the present invention is to develop an innovative mud material which has the properties of a resin-type mud material for improving the working environment, which mud material is capable of increasing the depth of an iron tap hole and of improving the adhesion to mud material deposited in a furnace at high heat, such adhesion being a drawback of the conventional art.This invention provides a mud material used for an iron tap hole in a blast furnace, wherein 8 to 20 wt % of a solution of a novolak-type phenolic resin having a specific number-average molecular weight and serving as a binder is added to and blended with a refractory aggregate used as a conventional mud material.
摘要翻译: PCT No.PCT / JP92 / 00264 Sec。 371日期:1992年11月5日 102(e)日期1992年11月5日PCT 1991年3月5日PCT公布。 出版物WO92 / 15537 日本1992年9月17日。本发明的目的是开发具有改善工作环境的树脂型泥浆材料的特性的创新泥浆材料,该泥浆材料能够增加铁丝锥的深度 并且提高了在高温下沉积在炉中的泥浆材料的粘附性,这种粘合性是传统技术的缺点。 本发明提供了一种用于高炉中的铁离子孔的泥浆材料,其中加入8至20重量%的具有特定数均分子量和用作粘合剂的酚醛清漆型酚醛树脂溶液和 与用作常规泥浆材料的耐火骨料混合。