1.
公开(公告)号:US5250509A
公开(公告)日:1993-10-05
申请号:US839324
申请日:1992-02-20
IPC分类号: C01G1/00 , C01G29/00 , C04B35/00 , C04B35/45 , H01B12/00 , H01B13/00 , H01L39/12 , H01L39/24 , C01F11/02 , C01G3/02
CPC分类号: C04B35/4521 , H01L39/126 , Y10S505/782
摘要: The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of Bi.sub.y Ca.sub.2 Sr.sub.2 Cu.sub.3 O.sub.x, where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical temperature T above 105 K and has a proportion of the phase Bi.sub.2 Sr.sub.2 Ca.sub.2 Cu.sub.3 O.sub.x of at least 85% by volume. The invention also relates to a process for producing a bismuth-containing superconducting material which comprises holding the oxides or oxide precursors of bismuth, strontium, calcium and copper at a temperature in the range from 850.degree. to 890.degree. C. over a time span of a plurality of hours and adhering to the following atomic ratios:Bi:Cu>2:3Ca:Sr=0.9 to 1.50.SIGMA.(Sr+Ca):Cu=4.2:3 to 4:3.33Bi:.SIGMA.(Sr+Ca)=2.35:4 to 3.1:4
摘要翻译: 本发明涉及含有铋,锶,钙和铜的氧化物 - 陶瓷超导材料,其总体组成为BiyCa2Sr2Cu3Ox,其中y为2.35至2.6的整数,x为约10至12.材料具有临界温度 T高于105K,并且Bi2Sr2Ca2Cu3Ox相的比例至少为85体积%。 本发明还涉及一种生产含铋的超导材料的方法,其包括在850℃至890℃的温度范围内保持铋,锶,钙和铜的氧化物或氧化物前体,时间跨度为 Cu:Sr = 0.9〜1.50,SIGMA(Sr + Ca):Cu = 4.2:3〜4:3.33 Bi:SIGMA(Sr + Ca) = 2.35:4〜3.1:4