摘要:
A method for manufacturing a PZT-based low-sintering piezoelectric ceramic material, the ions to be added as starting compounds being added as powdered oxides and/or powdered carbonates, mixed together, and then calcined to form the piezoelectric ceramic material. After calcining the starting compounds, lithium in ionic form is added to the mixture in an amount of 0.01 to 0.1 wt. % in relation to the weight of the PZT ceramic.
摘要:
A piezoelectric ceramic material having the molar composition Pb(1+c)−x−(3/2a)−1/2(x·b)A1xA2a(Zry(1−x·b−x·z)Ti(1−y)(1−x·b−x·w))(B1bB2zB3w)xO3 where A1 is selected from the group Ca, Mg, Sr, Ba, or their mixtures, A2 is selected from the group of rare-earth elements or their mixtures, B1 is selected from the group Nb, Ta, or Sb or their mixtures, B2 is Cu or a mixture of Cu with at least one element selected from the group Zn, Ni, Co, or Fe, and B3 is Fe, and where the following applies: 0.001≦a≦0.05; 0.05≦b≦0.90; 0≦c≦0.04; 0.005≦x≦0.03; 0.5≦y≦0.55; 0.05≦z≦0.90; 0≦w≦0.5. Furthermore, an electroceramic multilayer component is described having insulating layers containing such a material. Two manufacturing methods are described for the ceramic material, metal ions being introduced as powdered oxides and/or carbonates, mixed together, and calcined to form the ceramic material, or powdered ZrO2 and TiO2 is calcined to form ZryTi1−yO2 where 0.50
摘要翻译:具有其中A 1的摩尔组成的压电陶瓷材料选自Ca,Mg,Sr,Ba或它们的混合物,A 2选自稀土元素或它们的混合物B 1 >选自Nb,Ta或Sb或它们的混合物,B 2是Cu或Cu与选自Zn,Ni,Co或Fe中的至少一种元素的混合物,以及B 3 是Fe,以下适用范围:0.001 <= a <= 0.05; 0.05 <= b <= 0.90; 0 <= c <= 0.04; 0.005 <= x <= 0.03; 0.5 <= y <= 0.55; 0.05 <= z <= 0.90; 0 <= w <= 0.5。 此外,描述了具有包含这种材料的绝缘层的电陶瓷多层组件。 对于陶瓷材料描述了两种制造方法,将金属离子作为粉末状氧化物和/或碳酸盐引入,混合在一起并煅烧形成陶瓷材料,或将粉末状的ZrO 2和TiO 2煅烧形成ZryTi1-yO2,其中0.50
摘要:
A method for manufacturing a PZT-based low-sintering piezoelectric ceramic material, the ions to be added as starting compounds being added as powdered oxides and/or powdered carbonates, mixed together, and then calcined to form the piezoelectric ceramic material. After calcining the starting compounds, lithium in ionic form is added to the mixture in an amount of 0.01 to 0.1 wt. % in relation to the weight of the PZT ceramic.