摘要:
This invention provides, as a means of securing magnetic shield properties for a semi-tension mask and precluding color irregularity or mislanding on the phosphor due to beam drift, a Fe—Ni alloy for semi-tension mask comprising, in mass percentage (%), from 34 to 45% Ni, from 0.01 to 0.5% Mn, and the balance Fe and unavoidable impurities, said alloy being such that a sheet obtained after final cold rolling has an &agr;(111)+(220), said sum of the X-ray intensity ratio of (111) plane and (220) plane in the rolled surface represented by Formula 1 α ( 111 ) + ( 220 ) = I ( 111 ) + I ( 220 ) I ( 111 ) + I ( 200 ) + I ( 220 ) + I ( 311 ) × 100 ( % ) of no less than 15%. The invention also provides a semi-tension mask of the alloy, and a color picture tube using the semi-tension mask.
摘要:
An Fe--Ni alloy for use as a part 10 of an electron-gun 4 is press-blanked by a punch to form minute apertures 10a, 10b, 10c for passing an electron beam 3. The burrs 10 formed around the minute apertures 10a, 10b, 10c are detrimental to such part 4. The Fe--Ni alloy according to the present invention essentially consists of from 30 to 55 wt % of Ni, not more than 0.5 wt % of Si, not more than 1.5 wt % of Mn, and the balance being Fe and unavoidable impurities. The alloy includes from 10 to 1,000 of A type or B type non-metallic inclusions of 10 .mu.m or more in length per 1 mm.sup.2 of longitudinal cross section, and from 100 to 50,000 of C type non-metallic inclusions having a diameter of 5 .mu.m or less.
摘要:
A punched part consists of an Fe--Cr--Ni alloy essentially consisting of from 15 to 20% of Cr, from 9 to 15% of Ni, from 0.001 to 0.0050% of S, the balance being Fe and unavoidable impurities. The burrs formed during punching are suppressed due to addition of S to the Fe--Cr--Ni alloy.