公开(公告)号:US5961902A
公开(公告)日:1999-10-05
申请号:US750124
申请日:1997-03-27
申请人: Katsunori Ishitoya , Minoru Takaishi , Michihiro Okochi , Hideyuki Iwamoto , Sakuyoshi Nakagami , Kazufumi Tanaka
发明人: Katsunori Ishitoya , Minoru Takaishi , Michihiro Okochi , Hideyuki Iwamoto , Sakuyoshi Nakagami , Kazufumi Tanaka
IPC分类号: B29C31/04 , B29C43/18 , B29C43/20 , B29C43/34 , B29C44/00 , B29C47/00 , B29C70/78 , B60R13/02 , B29C43/04 , B29C44/06 , B29C44/12 , B29C47/06
CPC分类号: B60R13/02 , B29C31/044 , B29C43/18 , B29C43/203 , B29C43/34 , B29C47/0019 , B29C47/0021 , B29C70/78 , B29C2043/3433 , B29C2043/3438 , B29C44/00 , B29C47/00 , B29K2105/04 , B29K2105/256 , B29K2311/14 , B29K2711/14 , B29L2009/00 , B29L2031/3014 , B29L2031/3041 , B60R13/0243
摘要: A multilayer article such as a door trim board is fabricated by the steps of extruding melted resin layers (13m), (12m) and (11m) respectively forming a soft skin material (13), a foamed soft intermediate layer (12) and a base member (11) in the form of a multilayer resin sheet from a die-head (40) of an extruding machine, supply the extruded multilayer resin sheet to a molding machine in such a manner that the resin layer for the skin material is placed on a lower molding die of the molding machine and molding the resin layers in the form of the multilayer article. The resin layer for the skin material consists of thermoplastic elastomer, the resin layer for the intermediate layer consists of ethylenic copolymer copolymerized with ethylene and at least radical copolymerizable acid anhydride, and the resin layer for the base member consists of olefinic resin. The thermoplastic elastomer for the skin material is prepared in the form of olefinic thermoplastic elastomer and/or styrenic thermoplastic elastomer The melting flow rate of the thermoplastic elastomer is determined to be 0.1-200 g/10 min at 230.degree. C. under load of 2.16, and the shore A hardness of the elastomer is determined to be in a range of 50-96.
摘要翻译: PCT No.PCT / JP96 / 00592 Sec。 371日期1997年3月27日 102(e)1997年3月27日PCT 1996年3月7日PCT PCT。 出版物WO96 / 30185 日期1996年10月3日通过挤出分别形成软皮材料(13)的熔融树脂层(13m),(12m)和(11m),发泡软中间层 (12)和来自挤出机的模头(40)的多层树脂片形式的基底构件(11),将挤出的多层树脂片材提供给成型机,使得用于 将表皮材料放置在成型机的下模塑模具上并以多层制品的形式模制树脂层。 用于表皮材料的树脂层由热塑性弹性体构成,中间层的树脂层由与乙烯和至少自由基可共聚的酸酐共聚的乙烯类共聚物构成,基体的树脂层由烯烃树脂构成。 用于表皮材料的热塑性弹性体以烯烃类热塑性弹性体和/或苯乙烯类热塑性弹性体的形式制备。热塑性弹性体的熔融流动速率在230℃,负荷2.16下测定为0.1-200g / 10min ,弹性体的肖氏A硬度确定在50-96的范围内。