Positive electrode materials for lithium-ion batteries and method for preparing the same
    1.
    发明授权
    Positive electrode materials for lithium-ion batteries and method for preparing the same 有权
    锂离子电池正极材料及其制备方法

    公开(公告)号:US09379382B2

    公开(公告)日:2016-06-28

    申请号:US14133678

    申请日:2013-12-19

    摘要: A method for modifying a positive electrode material for a lithium-ion battery. The method includes: a) grinding a mixture of manganese dioxide and lithium carbonate, and calcining the mixture at no less than a temperature of 600° C. for no less than 20 hrs in the presence of air, to yield a powdery lithium manganese oxide (LiMn2O4); b) adding a precursor for forming a graphene-like structure to the powdery LiMn2O4, mixing, curing at a constant temperature of no less than 180° C. for between 2 and 4 hrs, grinding, and calcining at no less than a temperature of 500° C. for between 1 and 50 hrs in the presence of an inert gas, to yield a composite powder comprising a graphene-like structure and LiMn2O4; and c) collecting and sintering the composite powder at a temperature of between 300 and 500° C. for between 1 and 10 hrs in the presence of air.

    摘要翻译: 一种修改锂离子电池用正极材料的方法。 该方法包括:a)研磨二氧化锰和碳酸锂的混合物,并在600℃以下的温度下在空气存在下煅烧不少于20小时,得到粉末状的锂锰氧化物 (LiMn2O4); b)向粉末状LiMn 2 O 4中添加用于形成石墨烯结构的前体,在不低于180℃的恒定温度下混合固化2至4小时,研磨并在不低于 500℃,在惰性气体存在下1至50小时,得到包含石墨烯结构和LiMn 2 O 4的复合粉末; 和c)在空气存在下,在300-500℃的温度下收集和烧结复合粉末1至10小时。

    POSITIVE ELECTRODE MATERIALS FOR LITHIUM-ION BATTERIES AND METHOD FOR PREPARING THE SAME
    2.
    发明申请
    POSITIVE ELECTRODE MATERIALS FOR LITHIUM-ION BATTERIES AND METHOD FOR PREPARING THE SAME 有权
    用于锂离子电池的正极电极材料及其制备方法

    公开(公告)号:US20140103264A1

    公开(公告)日:2014-04-17

    申请号:US14133678

    申请日:2013-12-19

    IPC分类号: H01M4/505 H01M4/62

    摘要: A method for modifying a positive electrode material for a lithium-ion battery. The method includes: a) grinding a mixture of manganese dioxide and lithium carbonate, and calcining the mixture at no less than a temperature of 600° C. for no less than 20 hrs in the presence of air, to yield a powdery lithium manganese oxide (LiMn2O4); b) adding a precursor for forming a graphene-like structure to the powdery LiMn2O4, mixing, curing at a constant temperature of no less than 180° C. for between 2 and 4 hrs, grinding, and calcining at no less than a temperature of 500° C. for between 1 and 50 hrs in the presence of an inert gas, to yield a composite powder comprising a graphene-like structure and LiMn2O4; and c) collecting and sintering the composite powder at a temperature of between 300 and 500° C. for between 1 and 10 hrs in the presence of air.

    摘要翻译: 一种修改锂离子电池用正极材料的方法。 该方法包括:a)研磨二氧化锰和碳酸锂的混合物,并在600℃以下的温度下在空气存在下煅烧不少于20小时,得到粉末状的锂锰氧化物 (LiMn2O4); b)向粉末状LiMn 2 O 4中添加用于形成石墨烯结构的前体,在不低于180℃的恒定温度下混合固化2至4小时,研磨并在不低于 500℃,在惰性气体存在下1至50小时,得到包含石墨烯结构和LiMn 2 O 4的复合粉末; 和c)在空气存在下,在300-500℃的温度下收集和烧结复合粉末1至10小时。