Leadless glaze composition made with alkaline earth molybdenate
    1.
    发明授权
    Leadless glaze composition made with alkaline earth molybdenate 失效
    用碱土金钼酸盐制成的无铅釉料

    公开(公告)号:US4316963A

    公开(公告)日:1982-02-23

    申请号:US232162

    申请日:1981-02-06

    CPC分类号: C03C8/04 C03C8/02

    摘要: A leadless glaze composition having properties that make lead oxide containing glazes so widely used as ceramic glazes. The glazes according to this invention are prepared to analyze more than about 0.53 to about 1.5 weight percent molybdenum trioxide with the source of the molybdenum trioxide either in the frit or as a mill addition being alkaline earth molybdenate, for example, calcium molybdenate (CaMoO.sub.4).

    摘要翻译: 具有使含有釉料的氧化铅如陶瓷釉料广泛使用的性质的无铅釉料组合物。 根据本发明的釉料被制备成分析多于约0.53至约1.5重量%的三氧化钼,三氧化钼的来源在玻璃料中或作为研磨添加剂是碱土金属钼酸盐,例如钼酸钙(CaMoO 4) 。

    Method and system for quenching, drying, and elevating glass compositions
    2.
    发明授权
    Method and system for quenching, drying, and elevating glass compositions 失效
    淬火,干燥和提升玻璃组合物的方法和系统

    公开(公告)号:US4305743A

    公开(公告)日:1981-12-15

    申请号:US174622

    申请日:1980-08-01

    IPC分类号: C03B19/10 C03B1/00

    CPC分类号: C03B19/1045

    摘要: A method and system for quenching, drying, and elevating glass compositions comprising an incline reciprocating conveyor arranged to receive a stream of molten glass. The reciprocating conveyor has deep side and lower end walls in order to hold a pool of quenching liquid which is constantly replenished. The reciprocating action of the incline conveyor moves the quenched and shattered glass up out of the quenching pool to the higher end of the conveyor where it is drained and then delivered to a second conveyor. The second conveyor preferably comprises a helical vibrating conveyor surrounded by infrared heaters. The infrared heaters can be adjusted to supply just enough heat to the shattered glass on a helical vibrating conveyor surface to provide drying of the glass.

    摘要翻译: 一种用于淬火,干燥和升高玻璃组合物的方法和系统,其包括布置成接收熔融玻璃流的倾斜往复式输送机。 往复式输送机具有深的侧壁和下端壁,以便容纳不断补充的骤冷液池。 倾斜输送机的往复运动使淬火和破碎的玻璃从淬火池中移出到输送机的较高端,在那里排出,然后输送到第二输送机。 第二输送机优选地包括由红外加热器包围的螺旋振动输送机。 可以调节红外线加热器以向螺旋振动输送机表面上的破碎玻璃提供足够的热量,以提供玻璃的干燥。