    摘要: A building material product comprising a cementitious binder, an aggregate and cellulose reinforcing fibers wherein the cellulose reinforcing fibers have been treated with cationic or nonionic oil. The resulting fiber when included in a fiber cement composite results in improved deflection of the composite at peak loading as well as improved impact strength while maintaining overall board strength.

    摘要翻译: 一种建筑材料产品,包括水泥粘合剂,骨料和纤维素增强纤维,其中纤维素增强纤维已用阳离子或非离子油处理。 当包含在纤维水泥复合材料中时,所得的纤维导致复合材料在峰值载荷下的挠曲以及改善的冲击强度,同时保持整体板的强度。

    High temperature peroxide bleaching of mechanical pulps
    4.
    发明授权
    High temperature peroxide bleaching of mechanical pulps 有权
    高温过氧化氢漂白机械纸浆

    公开(公告)号:US06743332B2

    公开(公告)日:2004-06-01

    申请号:US09860025

    申请日:2001-05-16

    IPC分类号: D21C916

    CPC分类号: D21C9/163 D21C9/1042 D21D1/20

    摘要: A method of making bleached mechanical pulps is disclosed for pulping mills having a primary and a secondary refiner. A first step is to provide cellulosic materials, such as wood chips to refine into the pulp; the wood chips have an initial brightness level. A second step is to provide a bleaching liquor to the refining system of the pulp mill, wherein the liquor comprises an amount of hydrogen peroxide and an amount of alkali having greater than 0% to 100% magnesium hydroxide or soda ash or a combination thereof. A third step is to hold the pulp with the bleaching liquor at a temperature in the range of about 85° to about 160° C. and for about 2 to about 180 minutes. The components of the bleach liquor can be added at the first refiner or interstage between refiners.

    摘要翻译: 公开了一种具有初级和次级精磨机的制浆机的制造漂白机械纸浆的方法。 第一步是提供纤维素材料,例如木屑,以细化到纸浆中; 木片具有初始亮度水平。 第二步是向纸浆厂的精炼系统提供漂白液,其中所述液体包含一定量的过氧化氢和一定量的具有大于0%至100%的氢氧化镁或苏打灰或其组合的碱。 第三步是用漂白液将纸浆保持在约85℃至约160℃的温度和约2至约180分钟。 漂白液的组分可以在精炼机之间的第一精炼机或级间添加。

    Fiber cement board with modified fiber
    10.
    发明授权
    Fiber cement board with modified fiber 有权
    纤维水泥板改性纤维

    公开(公告)号:US08317914B2

    公开(公告)日:2012-11-27

    申请号:US12475206

    申请日:2009-05-29

    IPC分类号: C04B16/02

    摘要: A building material product comprising a cementitious binder, an aggregate and cellulose reinforcing fibers wherein the cellulose reinforcing fibers have been treated with cationic or nonionic oil. The resulting fiber when included in a fiber cement composite results in improved deflection of the composite at peak loading as well as improved impact strength while maintaining overall board strength.

    摘要翻译: 一种建筑材料产品,包括水泥粘合剂,骨料和纤维素增强纤维,其中纤维素增强纤维已用阳离子或非离子油处理。 当包含在纤维水泥复合材料中时,所得的纤维导致复合材料在峰值载荷下的挠曲以及改善的冲击强度,同时保持整体板的强度。