摘要: A liquid unsaturated resin composition for coating material which comprises (A) 60 to 95 parts by weight of liquid resin and (B) 5 to 40 parts by weight of polyvinyl monomer, having high boiling point, in which said liquid resin is produced by adding a compound having both epoxy group and polymerizable unsaturated group to a linear polyester having terminal carboxyl groups and said linear polyester is produced by condensation of (a) aromatic dibasic acid or its acid anhydride and (b) aliphatic saturated compounds consisting of saturated aliphatic dibasic acid and saturated aliphatic glycol.
摘要翻译: 一种用于涂料的液体不饱和树脂组合物,其包含(A)60至95重量份的液体树脂和(B)5至40重量份的具有高沸点的聚乙烯基单体,其中所述液体树脂通过添加 通过(a)芳族二元酸或其酸酐和(b)由饱和脂族二元酸组成的脂族饱和化合物的缩合制备具有末端羧基的直链聚酯和所述线性聚酯具有环氧基和可聚合不饱和基团的化合物 和饱和脂肪族二醇。
-
公开(公告)号:US3974303A
公开(公告)日:1976-08-10
申请号:US490753
申请日:1974-07-22
申请人: Seigo Iwase , Osamu Isozaki , Naozumi Iwasawa , Tadashi Watanabe
发明人: Seigo Iwase , Osamu Isozaki , Naozumi Iwasawa , Tadashi Watanabe
IPC分类号: C09D5/00 , B05D3/06 , C08G18/32 , C08G18/67 , C08J3/28 , C09D4/00 , C09D5/03 , C09D175/16 , B05B5/02
CPC分类号: C08G18/3206 , B05D3/067 , B05D3/068 , C08G18/672 , C08J3/28 , C09D175/16 , B05D2401/32 , C08G2150/20
摘要: A method for forming coating films which can provide coating films having good surface appearance and being excellent in such properties as impact resistance, adhesion to the substrate article, flexibility and chemical resistance, said method comprising coating a powdery composition of a thermoplastic resin having 0.5 to 3.5 polymerizable unsaturated bonds per 1000 of the molecular weight on an article to be coated, heat-melting the powdery resinous composition, and curing the molten film under application of ionizing radiation or ultraviolet radiation.
摘要翻译: 一种形成涂膜的方法,其可以提供具有良好的表面外观并且具有优异的耐冲击性,对基材制品的粘附性,柔韧性和耐化学性的性能的涂膜,所述方法包括将具有0.5的热塑性树脂的粉末组合物涂覆至 3.5可聚合的不饱和键,每1000个待涂覆的物品上的分子量,对粉末状树脂组合物进行加热熔融,并在施加电离辐射或紫外线辐射下固化熔融膜。
-