Method Of Colouring Tin And Tin-Containing Articles
    1.
    发明申请
    Method Of Colouring Tin And Tin-Containing Articles 有权
    着色锡和锡包含制品的方法

    公开(公告)号:US20120000412A1

    公开(公告)日:2012-01-05

    申请号:US13125510

    申请日:2009-10-22

    申请人: Trish Woods

    发明人: Trish Woods

    IPC分类号: G01D15/10 C09D7/12 C09D1/00

    CPC分类号: C23C22/58 C23C22/68 G01K11/14

    摘要: A method of colouring the surface of a tin-containing article is provided, the method comprising contacting at least a portion of the surface of the article with a solution comprising a thiosulphate, preferably under substantially neutral or acidic conditions. In one embodiment, the solution contains sodium thiosulphate and citric acid and further comprises a copper salt, together with acetone and/or glycerol. The method is preferably conducted at elevated temperatures, in particular by heating the solution to a temperature of from 45 to 85° C. The method is particularly suitable for the colouring of pewter articles, but may be applied to a wide range of tin-containing materials and tin alloys.

    摘要翻译: 提供了一种使含锡制品的表面着色的方法,该方法包括使制品的表面的至少一部分与包含硫代硫酸盐的溶液接触,优选在基本上中性或酸性条件下。 在一个实施方案中,溶液含有硫代硫酸钠和柠檬酸,并且还包含铜盐以及丙酮和/或甘油。 该方法优选在升高的温度下进行,特别是通过将溶液加热至45至85℃的温度。该方法特别适用于锡制品的着色,但可应用于宽范围的含锡 材料和锡合金。

    Method of colouring tin and tin-containing articles
    2.
    发明授权
    Method of colouring tin and tin-containing articles 有权
    锡和锡制品着色方法

    公开(公告)号:US09163312B2

    公开(公告)日:2015-10-20

    申请号:US13125510

    申请日:2009-10-22

    申请人: Trish Woods

    发明人: Trish Woods

    CPC分类号: C23C22/58 C23C22/68 G01K11/14

    摘要: A method of coloring the surface of a tin-containing article is provided, the method comprising contacting at least a portion of the surface of the article with a solution comprising a thiosulphate, preferably under substantially neutral or acidic conditions. In one embodiment, the solution contains sodium thiosulphate and citric acid and further comprises a copper salt, together with acetone and/or glycerol. The method is preferably conducted at elevated temperatures, in particular by heating the solution to a temperature of from 45 to 85° C. The method is particularly suitable for the coloring of pewter articles, but may be applied to a wide range of tin-containing materials and tin alloys.