公开(公告)号:US5439712A
公开(公告)日:1995-08-08
申请号:US203406
申请日:1994-03-01
CPC分类号: F04C18/0246 , C25D11/18 , C25D11/20 , F04C2230/91 , F05B2230/90 , F05C2201/021 , F05C2225/04 , Y10T428/12146 , Y10T428/30
摘要: A method for making a composite aluminum article comprises the steps of electrochemically or chemically adsorbing fine particles of a polytetrafluoroethylene to the surface of a hard anodic oxide film of an aluminum material or an aluminum alloy material, and drying the aluminum material or the aluminum alloy material. Thereafter, the aluminum material or the aluminum alloy material and an opposite member which slides along the aluminum material or the aluminum alloy material are rubbed together, and a lubricating film is thereby formed.
-
公开(公告)号:US5419970A
公开(公告)日:1995-05-30
申请号:US922469
申请日:1992-07-30
CPC分类号: F04C18/0246 , C25D11/18 , C25D11/20 , F04C2230/91 , F05B2230/90 , F05C2201/021 , F05C2225/04 , Y10T428/12146 , Y10T428/30
摘要: A method for making a composite aluminum article comprises the steps of electrochemically or chemically adsorbing fine particles of a polytetrafluoroethylene to the surface of a hard anodic oxide film of an aluminum material or an aluminum alloy material, and drying the aluminum material or the aluminum alloy material. Thereafter, the aluminum material or the aluminum alloy material and an opposite member which slides along the aluminum material or the aluminum alloy material are rubbed together, and a lubricating film is thereby formed.
摘要翻译: 一种复合铝制品的制造方法,其特征在于,在铝材或铝合金材料的硬质阳极氧化膜的表面电化学或化学吸附聚四氟乙烯微粒子的步骤,干燥铝材或铝合金材料 。 此后,铝材或铝合金材料和沿着铝材料或铝合金材料滑动的相对构件被摩擦在一起,从而形成润滑膜。
-
公开(公告)号:US06692422B2
公开(公告)日:2004-02-17
申请号:US10091463
申请日:2002-03-07
申请人: Koji Yamaguchi , Yukio Ohyama , Tsutomu Saito , Naoaki Sasakibara
发明人: Koji Yamaguchi , Yukio Ohyama , Tsutomu Saito , Naoaki Sasakibara
IPC分类号: F16C1300
CPC分类号: G03G15/1685 , G03G15/0233 , G03G15/0818 , G03G2215/0861
摘要: A roll has a base material layer, a front surface layer, and stress relaxation layer. The base material layer is made of low hardness rubber material and provided on an outer circumference of a metal core. The stress relaxation layer is provided on the base material layer and made of material which is at least higher in hardness than the base material layer and larger in stretch than the front surface layer. The front surface layer is made of resin material and provided on the stress relaxation layer. The stress relaxation layer is made of rubber material containing self-crosslinking resin. The stress relaxation layer has a thickness in a range of from 5 to 50 &mgr;m, and stress not lower than 5 MPa at 10% stretch.
摘要翻译: 辊具有基材层,前表面层和应力松弛层。 基材层由低硬度橡胶材料制成,设置在金属芯的外周。 应力松弛层设置在基材层上并且由比基材层硬度至少高的材料制成,并且拉伸比前表面层大。 前表面层由树脂材料制成并设置在应力松弛层上。 应力松弛层由含有自交联树脂的橡胶材料制成。 应力松弛层的厚度在5〜50μm的范围内,10%拉伸时的应力不低于5MPa。
-
-