公开(公告)号:US20190112403A1
公开(公告)日:2019-04-18
申请号:US16200996
申请日:2018-11-27
Applicant: AGC Inc.
Inventor: Masatoshi ABE , Takashi SATO , Tomoya HOSODA , Takuya NAKAO
IPC: C08F214/26 , C08J5/18 , H01B13/14 , H01B3/44
Abstract: A process for producing a fluororesin in which a low-boiling component is reduced, by subjecting a melt-formable fluororesin to melt-kneading treatment by a twin screw extruder 10, wherein the twin screw extruder 10 has at least one melting zone, a set temperature of a most upstream first melting zone Z1 among melting zones is the melting point of the fluororesin +25 to 100° C., a vacuum degree at a vent port of the vacuum vent 14 is at most −0.07 MPa [gage], and a melt mass-flow rate α2 (g/10 min) of the fluororesin after the melt-kneading treatment at a specific temperature under a specific load, to a melt mass-flow rate α1 (g/10 min) of the fluororesin before the melt-kneading treatment at the same temperature under the same specific load satisfy α1
-
公开(公告)号:US20200157301A1
公开(公告)日:2020-05-21
申请号:US16751301
申请日:2020-01-24
Applicant: AGC Inc.
Inventor: Norio OZAWA , Tomoya HOSODA , Takashi SATO
Abstract: To provide a resin composition, wherein the resin composition is excellent in impregnation into a reinforcing fiber sheet as it contains a polyamide having a low viscosity number; wherein the resin composition can be molded into a film, a fiber, etc., even though it contains a polyamide having a low viscosity number; and wherein the resin composition can produce a fiber-reinforced molded product having excellent impact resistance; a molded product and a method for its production; and a fiber-reinforced molded product having excellent impact resistance and a method for its production.A resin composition comprising: a polyamide having a viscosity number of from 100 to 170 determined by a method specified in ISO 307: 2007; and a melt-processable fluororesin having at least one type of a functional group selected from the group consisting of a carbonyl group-containing group, a hydroxy group, an epoxy group and an isocyanate group, and having a melting point of from 100 to 325° C.
-
公开(公告)号:US20210028571A1
公开(公告)日:2021-01-28
申请号:US16931593
申请日:2020-07-17
Applicant: AGC Inc.
Inventor: Sotaro KITADE , Takashi SATO , Hidehiko WATANABE
Abstract: An electrical connection structure according to the present disclosure includes a glass plate, a power supply part formed on the glass plate, a connection terminal including a base part facing the glass plate, and a spring member disposed between the power supply part and the base part and configured to electrically connect the power supply part to the base part. The spring member includes a fixing part, a curved part, and contact parts. The curved part includes branch parts branched by a slit. The contact part is disposed at each of end parts of the branch parts. The contact parts are in contact with the base part independently of each other. The curved part is in contact with the power supply part at a part protruding toward the glass plate.
-
公开(公告)号:US20200338872A1
公开(公告)日:2020-10-29
申请号:US16924299
申请日:2020-07-09
Applicant: AGC Inc.
Inventor: Norio OZAWA , Tomoya HOSODA , Takashi SATO
Abstract: The purpose of the present invention is to provide a laminate being excellent in chemical resistance, wear resistance, vibration absorption properties and flame resistance, and having high mechanical strength; and a method for its production. A laminate 1 comprises a fiber-reinforced resin layer 20 which comprises a reinforcing fiber base material and a resin component containing at least 50 vol % of a specific fluororesin, wherein the ratio of the reinforcing fiber base material to the total volume of the reinforcing fiber base material and the resin component is from 0.30 to 0.70, and a specific substrate 10, wherein at least one outermost layer is the fiber-reinforced resin layer 20, and the ratio of the total thickness of the fiber-reinforced resin layer 20 to the total thickness of the substrate 10 is from 1/99 to 30/70.
-
-
-