摘要:
A poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst has a monomodal molecular weight distribution with a reduced content of very high molecular weight species. It also exhibits increased morpholine incorporation in the high molecular weight fraction. Compared to commercially available poly(2,6-dimethyl-1,4-phenylene ether) prepared using a di-n-butylamine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits reduced odor. Compared to other poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits improved molecular weight build during compounding and improved compatibilization with polyamides.
摘要:
A poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst has a monomodal molecular weight distribution with a reduced content of very high molecular weight species. It also exhibits increased morpholine incorporation in the high molecular weight fraction. Compared to commercially available poly(2,6-dimethyl-1,4-phenylene ether) prepared using a di-n-butylamine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits reduced odor. Compared to other poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits improved molecular weight build during compounding and improved compatibilization with polyamides.
摘要:
A poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst has a monomodal molecular weight distribution with a reduced content of very high molecular weight species. It also exhibits increased morpholine incorporation in the high molecular weight fraction. Compared to commercially available poly(2,6-dimethyl-1,4-phenylene ether) prepared using a di-n-butylamine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits reduced odor. Compared to other poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits improved molecular weight build during compounding and improved compatibilization with polyamides.
摘要:
A poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst has a monomodal molecular weight distribution with a reduced content of very high molecular weight species. It also exhibits increased morpholine incorporation in the high molecular weight fraction. Compared to commercially available poly(2,6-dimethyl-1,4-phenylene ether) prepared using a di-n-butylamine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits reduced odor. Compared to other poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits improved molecular weight build during compounding and improved compatibilization with polyamides.
摘要:
A composition is prepared by oxidative copolymerization of specific amounts of 2,6-dimethylphenol, 2,3,6-trimethylphenol, and a hydroxyaryl-terminated polysiloxane. The composition exhibits an increased heat resistance relative to a corresponding composition prepared by copolymerizing 2,6-dimethylphenol and hydroxyaryl-terminated polysiloxane, without 2,3,6-trimethylphenol. The composition is useful as a flame-retardant additive in polymer compositions that require high heat resistance.
摘要:
A thermoplastic composition that includes a poly(arylene ether)-polysiloxane block copolymer is prepared by a method that includes oxidatively copolymerizing a monohydric phenol and a hydroxyaryl-terminated polysiloxane. The oxidative polymerization includes a monohydric phenol addition period characterized by a first temperature, a build period following the addition period and characterized by a second temperature greater than the first temperature, and a temperature ramp period between the addition period and the build period. During the temperature ramp period, the temperature is increased at an average rate of about 0.01 to about 0.35° C. per minute, which improves the efficiency with which the hydroxyaryl-terminated polysiloxane is incorporated into the poly(arylene ether)-polysiloxane block copolymer.
摘要:
A thermoplastic composition that includes a poly(arylene ether)-polysiloxane block copolymer is prepared by a method that includes oxidatively copolymerizing a monohydric phenol and a hydroxyaryl-terminated polysiloxane. The oxidative polymerization includes a monohydric phenol addition period characterized by a first temperature, a build period following the addition period and characterized by a second temperature greater than the first temperature, and a temperature ramp period between the addition period and the build period. During the temperature ramp period, the temperature is increased at an average rate of about 0.01 to about 0.35° C. per minute, which improves the efficiency with which the hydroxyaryl-terminated polysiloxane is incorporated into the poly(arylene ether)-polysiloxane block copolymer.
摘要:
A thermoplastic composition includes a poly(arylene ether) and a poly(arylene ether)-polysiloxane block copolymer. The thermoplastic composition is prepared by a method that includes oxidatively copolymerizing a monohydric phenol and a hydroxyaryl-terminated polysiloxane. The method is simpler than prior methods of preparing poly(arylene ether)-polysiloxane block copolymers by linking pre-formed poly(arylene ether) and polysiloxane blocks. The method is also produces greater incorporation of polysiloxane into the poly(arylene ether)-polysiloxane block copolymer than prior methods of copolymerizing monohydric phenols and hydroxyaryl-terminated polysiloxane.
摘要:
A thermoplastic composition includes a poly(arylene ether) and a poly(arylene ether)-polysiloxane block copolymer. The thermoplastic composition is prepared by a method that includes oxidatively copolymerizing a monohydric phenol and a hydroxyaryl-terminated polysiloxane. The method is simpler than prior methods of preparing poly(arylene ether)-polysiloxane block copolymers by linking pre-formed poly(arylene ether) and polysiloxane blocks. The method is also produces greater incorporation of polysiloxane into the poly(arylene ether)-polysiloxane block copolymer than prior methods of copolymerizing monohydric phenols and hydroxyaryl-terminated polysiloxane.
摘要:
A poly(arylene ether) copolymer is the product of oxidative copolymerization of monomers including a monohydric phenol and a dihydric phenol. It has an intrinsic viscosity of about 0.04 to about 0.15 deciliter per gram and, on average, about 1.8 to about 2 hydroxyl groups per molecule. The poly(arylene ether) copolymer is enriched in low molecular weight copolymer chains and copolymer chains that include a terminal unit derived from the dihydric phenol.