Rubber mixture and tire
    1.
    发明申请
    Rubber mixture and tire 有权
    橡胶混合物和轮胎

    公开(公告)号:US20070135564A1

    公开(公告)日:2007-06-14

    申请号:US10577307

    申请日:2004-11-01

    IPC分类号: C08L9/00

    摘要: The invention relates to a sulfur-vulcanizable rubber compound, in particular for treads of tires, which contains at least one diene rubber, liquid polybutadiene with a molecular weight of 1500-10000 g/mol and a vinyl content of 15-50%, at least one polar filler, at least one high-structure black with an iodine adsorption number of 115-200 g/kg and a DBP number of 125-160 mL/100 g and at least one glyceride and/or one factice for good abrasion characteristics, good wet traction and good traction on ice and snow with good dry braking at the same time.

    摘要翻译: 本发明涉及一种硫磺化橡胶化合物,特别是用于轮胎胎面的硫磺可硫化橡胶化合物,它含有至少一种二烯橡胶,分子量为1500-10000g / mol的液体聚丁二烯和15-50%的乙烯基含量, 至少一种极性填料,至少一种碘吸附数为115-200g / kg和DBP数为125-160mL / 100g的至少一种高结构黑色和至少一种甘油酯和/或一种具有良好耐磨特性的物质 良好的湿牵引力和良好的牵引力在冰雪上同时具有良好的干制动能力。

    Rubber mixture and tire
    2.
    发明授权
    Rubber mixture and tire 有权
    橡胶混合物和轮胎

    公开(公告)号:US07411018B2

    公开(公告)日:2008-08-12

    申请号:US10577307

    申请日:2004-11-01

    IPC分类号: C08L9/00

    摘要: The invention relates to a sulfur-vulcanizable rubber compound, in particular for treads of tires, which contains at least one diene rubber, liquid polybutadiene with a molecular weight of 1500-10000 g/mol and a vinyl content of 15-50%, at least one polar filler, at least one high-structure black with an iodine adsorption number of 115-200 g/kg and a DBP number of 125-160 mL/100 g and at least one glyceride and/or one factice for good abrasion characteristics, good wet traction and good traction on ice and snow with good dry braking at the same time.

    摘要翻译: 本发明涉及一种硫磺化橡胶化合物,特别是用于轮胎胎面的硫磺可硫化橡胶化合物,它含有至少一种二烯橡胶,分子量为1500-10000g / mol的液体聚丁二烯和15-50%的乙烯基含量, 至少一种极性填料,至少一种碘吸附数为115-200g / kg和DBP数为125-160mL / 100g的至少一种高结构黑色和至少一种甘油酯和/或一种具有良好耐磨特性的物质 良好的湿牵引力和良好的牵引力在冰雪上同时具有良好的干制动能力。