Abstract:
The present invention provides a cold-rolled and annealed Dual-Phase steel sheet having strength from 980 to 1100 MPa and a breaking elongation greater than 9%. The composition includes the contents being expressed by weight: 0.055%≦C≦0.095%, 2%≦Mn≦2.6%, 0.005%≦Si≦0.35%, S≦0.005%, P≦0.050%, 0.1≦Al≦0.3%, 0.05%≦Mo≦0.25%, 0.2%≦Cr≦0.5%, Cr+2Mo≦0.6%, Ni≦0.1%, 0.010≦Nb≦0.040%, 0.010≦Ti≦0.050%, 0.0005≦B≦0.0025%, and 0.002%≦N≦0.007%. The remainder of the composition includes iron and inevitable impurities resulting from the smelting. A manufacturing method is also provided.
Abstract:
The present invention provides a cold-rolled and annealed Dual-Phase steel sheet having a tensile strength from 980 to 1100 MPa. The composition includes the contents being expressed by weight: 0.055%≤C≤0.095%, 2%≤Mn≤2.6%, 0.005%≤Si≤0.35%, S≤0.005%, P≤0.050%, 0.1≤Al≤0.3%, 0.05%≤Mo≤0.25%, 0.2%≤Cr≤0.5%, Cr+2 Mo≤0.6%, Ni≤0.1%, 0.010≤Nb≤0.040%, 0.010≤Ti≤0.050%, 0.0005≤B≤0.0025%, and 0.002%≤N≤0.007%. The remainder of the composition includes iron and inevitable impurities resulting from the smelting. A microstructure of the steel sheet is 40 to 65% ferrite, 35 to 50% martensite and 0 to 10% bainite. A non-recrystallized ferrite fraction is less than or equal to 15%.
Abstract:
The present invention provides a cold-rolled and annealed Dual-Phase steel sheet having strength from 980 to 1100 MPa and a breaking elongation greater than 9%. The composition includes the contents being expressed by weight: 0.055%≤C≤0.095%, 2%≤Mn≤2.6%, 0.005%≤Si≤0.35%, S≤0.005%, P≤0.050%, 0.1≤Al≤0.3%, 0.05%≤Mo≤0.25%, 0.2%≤Cr≤0.5%, Cr+2Mo≤0.6%, Ni≤0.1%, 0.010≤Nb≤0.040%, 0.010≤Ti≤0.050%, 0.0005≤B≤0.0025%, and 0.002%≤N≤0.007%. The remainder of the composition includes iron and inevitable impurities resulting from the smelting. A manufacturing method is also provided.