Abstract:
The present disclosure provides a low density polyethylene (LDPE) having (A) a density from 0.910 to 0.924 g/cm3, determined according to ISO 1183 at 23° C.; (B) an elongational hardening of at least 4.2, at 150° C. at an elongational rate of 1 s−1; (C) a ratio Mw/Mn of at least 18, where (i) Mw is the weight average molar mass, measured by a MALLS detector coupled to a GPC, and (ii) Mn is the number average molar mass, measured by GPC (Gel Permeation Chromatography); and (D) a Mw of at least 230,000 g/mol. The present disclosure also provides an article of manufacture made from or containing (A) a substrate and (B) a coating layer made from or containing the disclosed LDPE. The present disclosure further provides a polymerization process occurring (A) in the presence of oxygen as the only radical initiating agent and (B) in the absence of solvents.
Abstract:
A process for polymerizing or copolymerizing ethylenically unsaturated monomers at pressures in the range of from 110 MPa to 500 MPa in a production line comprising a continuously operated polymerization reactor, wherein at least one of a pre-heater or pre-cooler, a polymerization reactor or a post reactor cooler is composed of tubes of a length from 5 m to 25 m which are flanged together, either directly or via bends, and the flanges are covered by a chimney construction, and wherein air is conveyed through the chimney construction and the air exiting the chimney construction is monitored with respect to the hydrocarbons concentration.
Abstract:
A process for polymerizing or copolymerizing ethylenically unsaturated monomers at pressures in the range of from 110 MPa to 500 MPa in a production line comprising a continuously operated polymerization reactor, wherein at least one of a pre-heater or pre-cooler, a polymerization reactor or a post reactor cooler is composed of tubes of a length from 5 m to 25 m which are flanged together, either directly or via bends, and the flanges are covered by a chimney construction, and wherein air is conveyed through the chimney construction and the air exiting the chimney construction is monitored with respect to the hydrocarbons concentration.
Abstract:
A process for polymerizing or copolymerizing ethylenically unsaturated monomers at pressures in the range of from 110 MPa to 500 MPa in a production line comprising a continuously operated polymerization reactor which is installed within a protective enclosure, wherein the production line is monitored with respect to an occurrence of a leakage of monomers or of reaction mixture and a water based deluge system, which provides droplets of a diameter in a range from 25 μm to 20 mm to the enclosed area, is automatically started with a minimum flow rate of 10 L/min per m2 of enclosed area when a leakage of monomers or of reaction mixture is detected.
Abstract:
Process for polymerizing or copolymerizing ethylenically unsaturated monomers in the presence of free-radical polymerization initiators at pressures in the range of from 110 MPa to 500 MPa and temperatures in the range of from 100° C. to 350° C. in a continuously operated polymerization apparatus, wherein the reaction gas composition is compressed to the polymerization pressure by at least two sequentially operating compressors in which a low-pressure compressor first compresses the reaction gas composition to a pressure of from 10 MPa to 50 MPa and a high-pressure compressor then further compresses the reaction gas composition to the polymerization pressure wherein the high-pressure compressor is operated with a polyalkylene glycol based synthetic lubricant and oxygen is introduced into the fresh gas feed or into the polymerization apparatus in an amount that the gas composition to be compressed in the high-pressure compressor has an oxygen content in the range of from 0.01 ppm to 0.9 ppm.
Abstract:
A process for polymerizing or copolymerizing ethylenically unsaturated monomers at pressures in the range of from 110 MPa to 500 MPa in a production line comprising a continuously operated polymerization reactor, wherein the process comprises monitoring the surrounding of the production line with respect to an occurrence of a leakage of monomers or of reaction mixture by an IR point detector arrangement of at least three groups of IR point detectors which are capable of detecting hydrocarbons and the groups of IR point detectors are operating according to a voting logic and starting automatically an emergency pressure release program when a group of IR point detectors of the IR point detector arrangement detects the presence of hydrocarbons.
Abstract:
A process for polymerizing or copolymerizing ethylenically unsaturated monomers at pressures in the range of from 110 MPa to 500 MPa in a production line comprising a continuously operated polymerization reactor, wherein the process comprises monitoring the surrounding of the production line with respect to an occurrence of a leakage of monomers or of reaction mixture by an IR point detector arrangement of at least three groups of IR point detectors which are capable of detecting hydrocarbons and the groups of IR point detectors are operating according to a voting logic and starting automatically an emergency pressure release program when a group of IR point detectors of the IR point detector arrangement detects the presence of hydrocarbons.
Abstract:
The present disclosure relates to a plant for performing polymerization, such as the polymerization of ethylene, having a recycle connection with two or more cooling channels arranged in parallel, a process for polymerization and downstream processes, and a plant for polymerization, comprising the following plant components in fluid communication: a) A reactor with an inlet side and an outlet side; b) A recycle connection positioned in fluid communication between the outlet side of the reactor and the inlet side of the reactor; wherein the recycle connection comprises two or more cooling channels arranged in parallel.
Abstract:
A process for polymerizing or copolymerizing ethylenically unsaturated monomers at pressures in the range of from 110 MPa to 500 MPa in a production line comprising a continuously operated polymerization reactor which is installed within a protective enclosure, wherein the production line is monitored with respect to an occurrence of a leakage of monomers or of reaction mixture and a water based deluge system, which provides droplets of a diameter in a range from 25 μm to 20 mm to the enclosed area, is automatically started with a minimum flow rate of 10 L/min per m2 of enclosed area when a leakage of monomers or of reaction mixture is detected.
Abstract:
The present disclosure relates to a plant for performing polymerization, such as the polymerization of ethylene, having a recycle connection with two or more cooling channels arranged in parallel, a process for polymerization and downstream processes, and a plant for polymerization, comprising the following plant components in fluid communication: a) A reactor with an inlet side and an outlet side; b) A recycle connection positioned in fluid communication between the outlet side of the reactor and the inlet side of the reactor; wherein the recycle connection comprises two or more cooling channels arranged in parallel.