Abstract:
A thermoplastic polyurethane having a glass transition temperature of the soft phase of not more than −25° C. measured using DMA and a heating rate of 2K/min at 1 Hz under torsion based on DIN EN ISO 6721: 2016; maximum G″ can be obtained by a process at least including the reaction of a polyol composition including a polypropylene glycol, wherein the proportion of the secondary terminal OH groups based on the total number of terminal OH groups of the polypropylene glycol is in the range of more than 90%, with a polyisocyanate to obtain a polyol composition including a prepolymer and the reaction of the polyol composition including the prepolymer with a polyisocyanate composition including at least one polyisocyanate and at least one chain extender having a molecular weight
Abstract:
A composition comprises polyalkylene terephthalate and terpolymer of alkylene diol, isophthalic acid and terephthalic acid, and polyalkylene terephthalate reinforcing fiber. The composition may be used to form an article, alone or with other thermoplastic material, at lower processing temperature, with higher melt flowability. The article formed is characterized with lower warpage and improved mechanical properties. The article may be useful for automotive, electrical, household, construction, and industrial applications. A method of preparing such thermoplastic polyester is also disclosed.
Abstract:
A composition comprises polyalkylene terephthalate and terpolymer of alkylene diol, isophthalic acid and terephthalic acid, and polyalkylene terephthalate reinforcing fiber. The composition may be used to form an article, alone or with other thermoplastic material, at lower processing temperature, with higher melt flowability. The article formed is characterized with lower warpage and improved mechanical properties. The article may be useful for automotive, electrical, household, construction, and industrial applications. A method of preparing such thermoplastic polyester is also disclosed.
Abstract:
A thermoplastic polyurethane having a glass transition temperature of the soft phase of not more than −25° C. measured using DMA and a heating rate of 2K/min at 1 Hz under torsion based on DIN EN ISO 6721: 2016; maximum G″ can be obtained by a process at least including the reaction of a polyol composition including a polypropylene glycol, wherein the proportion of the secondary terminal OH groups based on the total number of terminal OH groups of the polypropylene glycol is in the range of more than 90%, with a polyisocyanate to obtain a polyol composition including a prepolymer and the reaction of the polyol composition including the prepolymer with a polyisocyanate composition including at least one polyisocyanate and at least one chain extender having a molecular weight
Abstract:
The present invention relates to a polybutylene terephthalate composition, comprising as component (A) polybutylene terephthalate (PBT) resin, as component (B) polyester copolymer with melting point from 105° C. to 185° C., as component (C) vinyl-based polymer, and optionally as component (D) glass bubbles. The present invention also relates to a composite of plastic/metal hybrid, which comprises metal article and the polybutylene terephthalate composition of the present invention which is joined to and integrated with the metal article.
Abstract:
The present invention relates to a polybutylene terephthalate composition, comprising as component (A) polybutylene terephthalate (PBT) resin, as component (B) polyester copolymer with melting point from 105° C. to 185° C., as component (C) vinyl-based polymer, and optionally as component (D) glass bubbles. The present invention also relates to a composite of plastic/metal hybrid, which comprises metal article and the polybutylene terephthalate composition of the present invention which is joined to and integrated with the metal article.