Abstract:
Bicomponent filaments having a slight non-linear crimp are prepared by spinning a conjugated filament from polyaurolactam and a second linear, readily crystallizable homo- or copolyamide, stretching the filament, and then subjecting it to a heat treatment.
Abstract:
PRODUCTION OF CRYSTALLINE POLYCARBONATE FILAMENTS AND FOILS BY FORMING SUCH FILAMENTS OR FOILS AND SWELLING SUCH FILAMENTS OR FOILS WITH A KETONE OR AN ESTER SWELLING AGENT, STRETCH-ORIENTING SUCH FILAMENTS OR FOILS IN THE SWOLLEN STATE
AND THEN HEAT-TREATING SUCH ORIENTED FILAMENTS OR FOILS AT A TEMPERATURE OF ABOUT BETWEEN 180 AND 260*C.
Abstract:
PROCESS FOR THE PRODUCTION OF POLYAMIDE FIBRES HAVING LINEAR STRENGTH AND KNOT STRENGTH BY STRETCHING POLYAMIDE MONOFILS AT TEMPERATURES OF 25 TO 35*C. BELOW THE TEMPERATURE LEVEL OF THE CRYSTALLITE MELTING MAXIMUM AT A RATIO OF 1:4.5 TO 1:6.5.
Abstract:
FILAMENTARY AND FOIL MATERIAL FROM HIGH MOLECULAR WEIGHT LINEAR POLYCARBONATE HAVING A MOLECULAR WEIGHT FROM 95,000-150,000 AND A CRYSTALLINE CONTENT OF AT LEAST 18% PRODUCED BY SHAPING A SOLUTION OF THE POLYCARBONATE IN AN ORGANIC SOLVENT INTO LINEAR FORM AND STRETCHING THE LINEAR FROM SHAPED MATERIAL AT A DRAW RATIO OF AT LEAST 4:1 BY DISCRETE POINT STRETCHING AT A TEMPERATURE ABOVE THE CRYSTALLIZATION TEMPERATURE LIMIT AND BELOW THE CRYSTALLITE MELTING POINT THEREOF.