Crosslinked polymer composition, power cable insulation and power cable

    公开(公告)号:US10221300B2

    公开(公告)日:2019-03-05

    申请号:US15105238

    申请日:2014-08-19

    Applicant: BOREALIS AG

    Abstract: The present invention relates to a crosslinked polymer composition, which is obtained by crosslinking a polymer composition, which polymer composition has a melt flow rate (MFR) of at least 1.7 and comprises a polyolefin, peroxide and sulphur containing antioxidant, characterized by that the crosslinked polymer composition has an Oxidation Induction Time, determined according to ASTM-D3895, ISO/CD 11357 and EN 728 using a Differential Scanning Calorimeter (DSC), which Oxidation Induction Time corresponds to Z minutes, and comprises an amount of peroxide by-products which corresponds to W ppm determined according to BTM2222 using HPLC, wherein Z1≤Z≤Z2, W1≤W≤W2, and W≤p−270*Z, wherein Z1 is 0, Z2 is 60, W1 is 0 and W2 is 9500, and p is 18500; and use thereof, a power cable insulation and a power cable, useful in high voltage (HV) and extra high voltage (EHV) cable applications direct current (DC) applications.

    A NEW POLYMER COMPOSITION, POWER CABLE INSULATION AND POWER CABLE
    3.
    发明申请
    A NEW POLYMER COMPOSITION, POWER CABLE INSULATION AND POWER CABLE 审中-公开
    新型聚合物组合物,电力电缆绝缘和电力电缆

    公开(公告)号:US20160322124A1

    公开(公告)日:2016-11-03

    申请号:US15105226

    申请日:2014-08-19

    Applicant: BOREALIS AG

    Abstract: The present invention relates to a polymer composition comprising a polyolefin, peroxide and a sulphur containing antioxidant, wherein said peroxide is present in an amount which corresponds to X mmol -0-0-/kg polymer composition and said sulphur containing antioxidant is present in an amount which corresponds to Y mmol —OH/kg polymer composition, wherein Y1≦Y≦Y2, X≦45 and 0.9*Y+m≦X≦n−k*Y, wherein Y1 is 0.50 and Y2 is 10, and m is 0.8, n is 70 and k is 4.7; and wherein said polymer composition has a melt flow rate (MFR) which is at least 1.7, and said polymer composition comprises less than 0.05% by weight (wt %) 2,4-Diphenyl-4-methyl-1-pentene; a crosslinked polymer composition, and use thereof, a power cable insulation, a power cable, useful in high voltage (HV DC) and extra high voltage (EHV DC) direct current applications, and a method for reducing electrical conductivity of a crosslinked polymer composition.

    Abstract translation: 本发明涉及包含聚烯烃,过氧化物和含硫抗氧化剂的聚合物组合物,其中所述过氧化物的存在量相当于X mmol -0-0- / kg聚合物组合物,并且所述含硫抗氧化剂存在于 对应于Y mmol -OH / kg聚合物组成的量,其中Y1≤Y≤Y2,X≤45和0.9 * Y +m≤X≤n-k * Y,其中Y1为0.50,Y2为10,m为 0.8,n为70,k为4.7; 并且其中所述聚合物组合物具有至少1.7的熔体流动速率(MFR),并且所述聚合物组合物包含小于0.05重量%(重量%)的2,4-二苯基-4-甲基-1-戊烯; 交联聚合物组合物及其用途,用于高压(HV DC)和超高压(EHV DC)直流应用的电力电缆绝缘,电力电缆以及降低交联聚合物组合物的导电性的方法 。

    NEW CROSSLINKED POLYMER COMPOSITION, POWER CABLE INSULATION AND POWER CABLE
    4.
    发明申请
    NEW CROSSLINKED POLYMER COMPOSITION, POWER CABLE INSULATION AND POWER CABLE 审中-公开
    新型交联聚合物组合物,电力电缆绝缘和电力电缆

    公开(公告)号:US20160319104A1

    公开(公告)日:2016-11-03

    申请号:US15105238

    申请日:2014-08-19

    Applicant: BOREALIS AG

    CPC classification number: C08K5/375 C08K5/01 C08K5/14 H01B3/441 C08L23/02

    Abstract: The present invention relates to a crosslinked polymer composition, which is obtained by crosslinking a polymer composition, which polymer composition has a melt flow rate (MFR) of at least 1.7 and comprises a polyolefin, peroxide and sulphur containing antioxidant, characterised by that the crosslinked polymer composition has an Oxidation Induction Time, determined according to ASTM-D3895, ISO/CD 11357 and EN 728 using a Differential Scanning Calorimeter (DSC), which Oxidation Induction Time corresponds to Z minutes, and comprises an amount of peroxide by-products which corresponds to W ppm determined according to BTM2222 using HPLC, wherein Z1≦Z≦Z2, W1≦W≦W2, and W≦p−270*Z, wherein Z1 is 0 , Z2 is 60, W1 is 0 and W2 is 9500, and p is 18500; and use thereof, a power cable insulation and a power cable, useful in high voltage (HV) and extra high voltage (EHV) cable applications direct current (DC) applications.

    Abstract translation: 本发明涉及交联聚合物组合物,其通过交联聚合物组合物获得,该聚合物组合物的熔体流动速率(MFR)为至少1.7,并且包含聚烯烃,过氧化物和含硫的抗氧化剂,其特征在于,交联的 聚合物组合物具有氧化诱导时间,其使用差示扫描量热计(DSC)根据ASTM-D3895,ISO / CD 11357和EN 728测定,氧化诱导时间对应于Z分钟,并且包含一定量的过氧化物副产物, 对应于根据BTM2222使用HPLC测定的W ppm,其中Z1≤Z≤Z2,W1≤W≤W2,W≤p-270×Z,其中Z1为0,Z2为60,W1为0,W2为9500, p为18500; 及其使用,电力电缆绝缘和电力电缆,可用于高压(HV)和超高压(EHV)电缆应用直流(DC)应用。

    Polymer composition, power cable insulation and power cable

    公开(公告)号:US10347390B2

    公开(公告)日:2019-07-09

    申请号:US15105226

    申请日:2014-08-19

    Applicant: BOREALIS AG

    Abstract: The present invention relates to a polymer composition comprising a polyolefin, peroxide and a sulphur containing antioxidant, wherein said peroxide is present in an amount which corresponds to X mmol —O—O—/kg polymer composition and said sulphur containing antioxidant is present in an amount which corresponds to Y mmol —OH/kg polymer composition, wherein Y1≤Y≤Y2, X≤45 and 0.9*Y+m≤X≤n−k*Y, wherein Y1 is 0.50 and Y2 is 10, and m is 0.8, n is 70 and k is 4.7; and wherein said polymer composition has a melt flow rate (MFR) which is at least 1.7, and said polymer composition comprises less than 0.05% by weight (wt %) 2,4-Diphenyl-4-methyl-1-pentene; a crosslinked polymer composition, and use thereof, a power cable insulation, a power cable, useful in high voltage (HV DC) and extra high voltage (EHV DC) direct current applications, and a method for reducing electrical conductivity of a crosslinked polymer composition.