公开(公告)号:US10695819B2
公开(公告)日:2020-06-30
申请号:US16025884
申请日:2018-07-02
Applicant: CITIC Dicastal CO., LTD.
Inventor: Haiping Chang , Lijuan Zhang , Shiwen Xu , Xuepu Yin , Hongwei Zhou , Zhixue Wang , Rui Li , Jin Zhang , Dawei Xu
Abstract: The present disclosure discloses a method for forming a rim of a cast-spun aluminum alloy hub, that is, a special spinning composite machining method for forming a structure that the spokes and the inner wheel flange of the hub are cast and the middle of the rim is spun. The method can prevent the performance, strength and as-cast structure of the inner wheel flange from being destroyed, effectively improve the impact resistance of the cast-spun hub at the inner wheel flange, prevent the inner wheel flange of the cast-spun hub from cracking during radial impact and improve the performance of the spun structure of the rim, is beneficial to thinning the rim and realizes light weight of the rim.
-
公开(公告)号:US10384311B2
公开(公告)日:2019-08-20
申请号:US15688906
申请日:2017-08-29
Applicant: CITIC Dicastal CO., LTD.
Inventor: Haiping Chang , Zhixue Wang , Shiyou Gao , Jin Zhang , Rui Li , Dawei Xu , Donghui Zhang
IPC: B23K26/352 , B23K26/34 , C23C24/10 , C23C4/04 , C23C16/48
Abstract: A spinning roller surface laser reinforced processing forming method is provided. A spinning roller is normalized after forging, the normalizing temperature is controlled to 860-880 DEG C., and the heat preservation time is 40-60 minutes; the spinning roller forging blank is roughly processed to reserve a tolerance allowance of 0.5 mm on the designated working face; the spinning roller and workpiece contact surface reinforcing layer is made of Ni625+WC2, in which WC is more than 22%; a reinforcing layer having the thickness of 0.8 mm is clad with laser on the working face of the spinning roller, and the preheating temperature is controlled to 250-400 DEG C. before welding; the spinning roller laser clad reinforcing layer is rolled; and the rolled spinning roller is put into a thermal treatment furnace for thermal treatment, and quenching and tempering treatment, re-crystallization and residual stress elimination are performed.
-
公开(公告)号:US20190283107A1
公开(公告)日:2019-09-19
申请号:US16025884
申请日:2018-07-02
Applicant: CITIC Dicastal CO., LTD.
Inventor: Haiping Chang , Lijuan Zhang , Shiwen Xu , Xuepu Yin , Hongwei Zhou , Zhixue Wang , Rui Li , Jin Zhang , Dawei Xu
Abstract: The present disclosure discloses a method for forming a rim of a cast-spun aluminum alloy hub, that is, a special spinning composite machining method for forming a structure that the spokes and the inner wheel flange of the hub are cast and the middle of the rim is spun. The method can prevent the performance, strength and as-cast structure of the inner wheel flange from being destroyed, effectively improve the impact resistance of the cast-spun hub at the inner wheel flange, prevent the inner wheel flange of the cast-spun hub from cracking during radial impact and improve the performance of the spun structure of the rim, is beneficial to thinning the rim and realizes light weight of the rim.
-
公开(公告)号:US20180333802A1
公开(公告)日:2018-11-22
申请号:US15688906
申请日:2017-08-29
Applicant: CITIC Dicastal CO., LTD
Inventor: Haiping Chang , Zhixue Wang , Shiyou Gao , Jin Zhang , Rui Li , Dawei Xu , Donghui Zhang
IPC: B23K26/00
CPC classification number: B23K26/352 , B23K26/34 , C23C4/04 , C23C16/483 , C23C24/103
Abstract: A spinning roller surface laser reinforced processing forming method is provided. A spinning roller is normalized after forging, the normalizing temperature is controlled to 860-880 DEG C., and the heat preservation time is 40-60 minutes; the spinning roller forging blank is roughly processed to reserve a tolerance allowance of 0.5 mm on the designated working face; the spinning roller and workpiece contact surface reinforcing layer is made of Ni625+WC2, in which WC is more than 22%; a reinforcing layer having the thickness of 0.8 mm is clad with laser on the working face of the spinning roller, and the preheating temperature is controlled to 250-400 DEG C. before welding; the spinning roller laser clad reinforcing layer is rolled; and the rolled spinning roller is put into a thermal treatment furnace for thermal treatment, and quenching and tempering treatment, re-crystallization and residual stress elimination are performed.
-
-
-